Laser Welders

Operations
RedSabre 550
Need To Know:
  • Optical Pump:GW
  • Unique Air Cooled Fiber Laser Technology
  • 550 Watt
  • Ergonomic Gun
  • 240V 1 Phase 
  • 1080 nm Wave length
  • 10m Cable
  • Weld/Clean/Cut
  • 62 lbs. base unit 
  • Compact size
  • Class 4 laser
  • Maximum Weld Mild/Stainless Steel:1.5 (Single Pass)
  • Maximum Weld Aluminum: 1.0mm  (Single Pass)

Quick Specs View >>
Input
Output
$3,900.00 Buy Now
RedSabre 750
Need To Know:
  • Optical Pump:GW
  • Unique Air Cooled Fiber Laser Technology
  • 750 Watt
  • Ergonomic Gun
  • 240V 1 Phase 
  • 1080 nm Wave length
  • 10m Cable
  • Weld/Clean/Cut
  • 62 lbs. base unit 
  • Compact size
  • Class 4 laser
  • Maximum Weld Mild/Stainless Steel: 2.0mm (Single Pass)
  • Maximum Weld Aluminum: 1.5mm (Single Pass)

Quick Specs View >>
Input
Output
$4,200.00 Buy Now
RedSabre 1250
Need To Know:
  • Optical Pump:GW
  • Unique Air Cooled Fiber Laser Technology
  • 1250 Watt
  • Ergonomic Gun
  • 240V 1 Phase 
  • 1080 nm Wave length
  • 10m Cable
  • Weld/Clean/Cut
  • 66 lbs. base unit 
  • Compact size
  • Class 4 laser
  • Maximum Weld Mild/Stainless Steel: 1/8" (3.5mm)
  • Maximum Weld Aluminum: 3/32" (2.5mm)
  • Maximum Cut Mild/Stainless Steel: 5/32" (4mm)
  • Maximum Cut Aluminum: 7/64 " (3mm)

Quick Specs View >>
Input
Output
$8,999.00You Save - $1,000.00
$7,999.00 Buy Now
RedSabre 1500
Need To Know:
  • Optical Pump: RLASER
  • Unique Air Cooled Fiber Laser Technology
  • 1500 Watt
  • SUP33T Laser Gun
  • 240V 1 Phase 
  • 1070 nm Wave length
  • 10m Cable
  • Weld/Clean/Cut
  • Separate wire feeder included
  • 116 lbs. base unit 
  • 30 lbs. Wire Feeder
  • Compact size
  • Class 4 laser
  • Weld Steel up to .160"
  • Weld Aluminum up to .140"
  • Cut Steel up to .200"
  • Cut Aluminum up to .160"
  • Maximum Weld Mild/Stainless Steel: 5/32" (4mm)
  • Maximum Weld Aluminum: 1/8" (3.5mm)
  • Maximum Cut Mild/Stainless Steel: 3/16" (5mm)
  • Maximum Cut Aluminum: 5/32" (4mm)

Quick Specs View >>
Input
Output
$12,774.00You Save - $2,775.00
$9,999.00 Buy Now
RedSabre 1500X
Need To Know:
  • Optical Pump: GW
  • New Water-Cooled/ Refridgeration Fiber Laser Technology
  • 1500 Watt
  • Ergonomic Gun
  • 240V 1 Phase
  • 1070 nm Wave length
  • 10m cable
  • Weld/Clean/Cut
  • Separate wire feeder included
  • 295 lbs. Base unit weight
  • 30 lbs. Feeder attachment weight
  • Compact size
  • Class 4 laser
  • Gap Fill (Root) w/o Wire: 1.0mm/.040" 

    Gap Fill (Root) Single Wire Feeder 1.6mm/.062"(≤1/16")

    Gap Fill (Root) Double Wire Feeder 2.0mm/ .080" (≤ 5/64")

    Single Side Weld Steel/S.S. Max:  4.0mm/ .16" (≤ 5/32")

    Single Side Weld Aluminum Max: 3.5mm/ .14" (≤9/64 ")

    Single Side Weld Copper Max: 2.0mm/ .080" (≤ 5/64")

    Cut Thickness Steel Max: 5.0mm/ .19"  (≤ 3/16")

    Cut Thickness Aluminum Max: 4.0mm/ .16" (≤5/32")


Quick Specs View >>
Input
Output
$9,999.00 Buy Now
RedSabre 2000
Need To Know:
  • Optical Pump: RLASER
  • Unique Air Cooled Fiber Laser Technology
  • 2000 Watt
  • SUP21T Laser Gun
  • 240V 1 phase
  • 1070 nm Wave length
  • 10m
  • Weld/Clean/Cut
  • Separate wire feeder included
  • 127 lbs. Base unit weight
  • 30 lbs. Feeder attachment weight
  • Compact size
  • Class 4 laser
  • Weld Steel up to .240"
  • Weld Aluminum up to .180"
  • Cut Steel up to .240"
  • Cut Aluminum up to .200"
  • Maximum Weld Mild/Stainless Steel: 1/4" (6mm)
  • Maximum Weld Aluminum: 11/64" (4.5mm)
  • Maximum Cut Mild/Stainless Steel: 1/4" (6mm)
  • Maximum Cut Aluminum: 3/16" (5mm)

 


Quick Specs View >>
Input
Output
$15,999.00You Save - $3,600.00
$12,399.00 Buy Now
RedSabre 2000X
Need To Know:
  • Optical Pump: GW
  • New Refrigeration-Cooled Fiber Laser Technology
  • 2000 Watt
  • SUP23T Laser Gun
  • 240V 1 Phase
  • 1070 nm Wave length
  • 10m cable
  • Weld/Clean/Cut
  • Separate wire feeder included
  • 295 lbs. Base unit weight
  • 30 lbs. Feeder attachment weight
  • Compact size
  • Class 4 laser
  • Weld Steel up to .240"
  • Weld Aluminum up to .180"
  • Cut Steel up to .240"
  • Cut Aluminum up to .200"
  • Maximum Weld Mild/Stainless Steel: 1/4" (6mm)
  • Maximum Weld Aluminum: 11/64" (4.5mm)
  • Maximum Cut Mild/Stainless Steel: 1/4" (6mm)
  • Maximum Cut Aluminum: 3/16" (5mm)

Quick Specs View >>
Input
Output
$13,999.00You Save - $1,900.00
$12,099.00 Buy Now
RedSabre 3000X (3Ph 208V/220V/240V/480V)
Need To Know:
  • Optical Pump: GW
  • New Refrigeration-Cooled Fiber Laser Technology
  • 3000 Watt
  • SUP23T Laser Gun
  • 240V/480V 3 Phase
  • 1070 nm Wave length
  • 10m cable
  • Weld/Clean/Cut
  • Separate wire feeder included
  • 333 lbs. Base unit weight
  • 30 lbs. Feeder attachment weight
  • Compact size
  • Class 4 laser
  • Weld Steel up to .280"
  • Weld Aluminum up to .250"
  • Cut Steel up to .280"
  • Cut Aluminum up to .260"
  • Maximum Weld Mild/Stainless Steel: 5/16" (8mm)
  • Maximum Weld Aluminum: 1/4" (6.5mm)
  • Maximum Cut Mild/Stainless Steel: 5/16" (8mm)
  • Maximum Cut Aluminum: 9/32" (7mm)

Quick Specs View >>
Input
Output
$23,999.00You Save - $5,500.00
$18,499.00 Buy Now
RedSabre 3001X (1Ph 220V/240V)
Need To Know:
  • Optical Pump: GW
  • New Refrigeration-Cooled Fiber Laser Technology
  • 3000 Watt
  • SUP23T Laser Gun
  • 240V 1 Phase
  • 1070 nm Wave length
  • 10m cable
  • Weld/Clean/Cut
  • Separate wire feeder included
  • 333 lbs. Base unit weight
  • 30 lbs. Feeder attachment weight
  • Compact size
  • Class 4 laser
  • Weld Steel up to .28"(8.0mm)
  • Weld Aluminum up to .22" (6.5mm)
  • Cut Steel up to .28" (7.0mm)
  • Cut Aluminum up to .25" (6.5mm)
  • Maximum Weld Mild/Stainless Steel: 5/16" (8mm)
  • Maximum Weld Aluminum: 1/4" (6.5mm)
  • Maximum Cut Mild/Stainless Steel: 5/16" (8mm)
  • Maximum Cut Aluminum: 9/32" (7mm)

Quick Specs View >>
Input
Output
$22,999.00You Save - $5,000.00
$17,999.00 Buy Now
Typhoon 230
Need To Know:
  • 230 Amp AC/DC Pulse TIG, 200 Amp AC/DC Stick. 
  • Large 5.1" Hi Definition LCD color screen.
  • Independent Amperage adjustment for EP and EN half cycles (Independent Amplitude).
  • Split wave form control for AC.
  • 2 Amp DC and 3 Amp AC Start.
  • Up to 400 Hz AC frequency.
  • DC pulse wave form shaping.
  • Standard and Adv. AC pulse
  • Standard AC Pulse Freq. 400 Hz
  • Adv. AC Pulse 10 Hz
  • DC Pulse Frequency 999.9 Hz
  • 5 AC wave forms.
  • Advanced Power Set Mode for easy setup.
  • No pop-up screens.  Easy to navigate.
  • All main settings visible at a glance.
  • Fan and Cooler Control Technology.
  • 70% Duty Cycle at max output.
  • Dual Voltage 120/240V, auto sensing.

Quick Specs View >>
Input
  • 120/240
  • 1 phase
Output
  • AC/DC
  • CC
$3,750.00You Save - $1,500.00
$2,250.00 Buy Now
GTAW/SMAW
Input:

120/240V

Min Output:

DC 3A; AC 5A

Max Output:

70%

Duty Cycle:

70% @ Max 120/240V

Price: $2,250.00
Best Features:

5 Wave Form Controls for AC

AC Amplitude Control

Split Wave Form Control

DC Pulse Wave form shaping

High Duty Cycle

5.1 HD (720) TFT Screen

RedSabre 6000 (240/480 3 phase)
Need To Know:
  • Optical Pump: GW
  • Water-Cooled Fiber Laser Technology
  • 6000 Watt
  • Ergonomic Gun
  • 240V/480V 3 Phase
  • 1080 nm Wave length
  • 10m cable
  • Weld/Clean
  • Separate wire feeder included
  • 396 lbs. Base unit weight
  • 30 lbs. Wire Feeder attachment weight
  • Dual Wire Feeder Optional
  • Class 4 laser
  • Weld Steel up to .47"(12.0mm)
  • Weld Aluminum up to .315" (8mm)
  • Maximum Weld Mild/Stainless Steel: 5/16" (8mm)
  • Maximum Weld Aluminum: 1/4" (6.5mm)
  • Wire Diameter from .030"-.062" 

Quick Specs View >>
Input
Output
$49,999.00 Buy Now