HF Start vs. DC Lift Start Tig vs. Scratch Start
If you are left “scratching” your head about the differences in the different start methods of TIG, you are not alone. Many experienced users get the facts wrong when it comes to the 3 basic ways you can start a TIG arc.
Scratch start TIG is probably the oldest method of starting an arc. It’s not a pretty process as it involves flicking near molten tungsten across the metal until an arc starts. The Scratch start method is similar to striking a match on a box. It works well, and it allows almost any DC stick welder to be turned into a TIG welder without much work. But Scratch start has some significant draw backs as the tungsten gets hot almost instantly as the arc is struck and small bits and pieces of the tungsten break off and get stuck in the weld. This can cause structural problems later. For general work though it works pretty well. Scratch start is a good way to get started TIG welding and is used throughout the world on a daily basis. It is far from falling out of use.
Lift start is probably the most misunderstood form of starting. A lot of times it is confused with scratch start. It may look similar but is far from it. It is a relatively clean process even though it involves contact with metal. The lift start involves bringing the tungsten down quickly and lightly into contact with the metal, and then a quick lift up to “draw” the arc. What happens with lift start is the OCV of the welder cuts back to a very low voltage output when the unit senses it has made continuity with the work piece. Once lifted the unit shifts to a higher output as the tungsten leaves the surface. This creates little contamination and preserves the point on the tungsten. It is still not 100% clean. The tungsten still can get contaminated. But lift start is a much better option than scratch starting, for steel and stainless. But it is not a good option for Aluminum because of the affinity aluminum and tungsten have for each other.
The most popular and best option is the use of High Frequency start that generates a high frequency arc that is capable of ionizing the air and bridging the gap between the tungsten point and the work piece. The High Frequency start is a touch-less method and creates almost contamination unless the tungsten is over sharpened or the amperage is turned too high at the start. It is an excellent choice for welding aluminum, and really is the only acceptable choice. Unless you need to weld Aluminum, you don’t have to really have High Frequency start, but it is nice to have to weld AC or DC if you have the option.
Comments
jackryan replied on Permalink
Can CBD Oil Help Increase Libido? Wonderful article. Fascinating to read. I love to read such an excellent article. Thanks! It has made my task more and extra easy. Keep rocking.
jackryan replied on Permalink
Wonderful article. Fascinating to read. I love to read such an excellent article. Thanks! It has made my task more and extra easy. Keep rocking. panda love
adilkhatri replied on Permalink
This post is extremely radiant. I extremely like this post. It is outstanding amongst other posts that I ve read in quite a while. Much obliged for this better than average post. I truly value it! 우리카지노
adilkhatri replied on Permalink
해외토토추천 해외사이트추천 토토사이트추천 BEST OF BEST | 먹튀검증 전문업체 해외사이트추천
adilkhatri replied on Permalink
토토사이트 스포츠토토 토토픽 먹튀사이트 검증추천 최강 토토피플 안전놀이터
adilkhatri replied on Permalink
A debt of gratitude is in order for composing such a decent article, I staggered onto your blog and read a couple of post. I like your style of composing... 우리카지노
adilkhatri replied on Permalink
Dubai Curtain Shop is experienced in Curtain installation, Curtain fittings, Curtain fixing, Blinds Fitting Services in all over Dubai. Call us at 058 965 6471 Dubai curtain service
adilkhatri replied on Permalink
I am scanning for and I need to post a comment that "The substance of your post is magnificent" Great work! 토토사이트 추천
adilkhatri replied on Permalink
Gangaur Realtech is a professionally overseen association having some expertise in land administrations where coordinated administrations are given by experts to its customers looking for expanded an incentive by owning, involving or putting resources into land. 369superslot.com
adilkhatri replied on Permalink
Much obliged to you for your post, I search for such article along time, today I discover it at long last. this post give me heaps of prompt it is extremely helpful for me. Cross Institutional Study
Digital_work replied on Permalink
Fabulous post, you have denoted out some fantastic points, I likewise think this s a very wonderful website. I will visit again for more quality contents and also, recommend this site to all. Thanks. gclub
Jashmin replied on Permalink
Rolling sky and crafting and building are my favorite games for mobile
https://apkgameapps.com/adventure/crafting-and-building/
https://apkgameapps.com/arcade/rolling-sky/
adilkhatri replied on Permalink
I am scanning for and I need to post a comment that "The substance of your post is magnificent" Great work! https://www.caz79.com
adilkhatri replied on Permalink
I would recommend my profile is crucial to me, I welcome you to inspect this subject... 토토사이트 추천
adilkhatri replied on Permalink
Kundali Matching or Horoscope Matching is an auspicious process that is carried out before the wedlock takes place. From the history of the Vedas and the Puranas, it is quite clear the Marriage has been the divine ritual for every individual. In today’s world, it is still unique and one of the best memories when a couple gets married. marriage matching by name
NewAmericanStore replied on Permalink
Thank you for this great contribution, I find it very interesting and well thought out and put together. I hope to read your work in the future. Cobra Kai Jacket
adilkhatri replied on Permalink
Trying to say thanks won't simply be adequate, for the fantasti c clarity in your written work. I will immediately snatch your rss channel to remain educated of any updates. Car consignment
adilkhatri replied on Permalink
I am overpowered by your post with such a decent theme. Typically I visit your web journals and get refreshed through the data you incorporate yet the present blog would be the most obvious. Well done! 360 Innovation Tech
Digital_work replied on Permalink
This is very significant, and yet necessary towards just click this unique backlink: royal online
adilkhatri replied on Permalink
Effectively, the article is really the best point on this registry related issue. I fit in with your decisions and will energetically anticipate your next updates. สมาชิกใหม่ ฟรีเครดิต
adilkhatri replied on Permalink
Gorilla! Toto Site Safety Playground Meet the top of private Toto Safety Park verification sites There are honest major sites If you experience the essence of Safety Toto sites, you no longer need to verify other food sites. 먹튀검증사이트
adilkhatri replied on Permalink
Thankful to you for your post, I look for such article along time, today I find it finally. this post give me piles of provoke it is to a great degree supportive for me. 안전놀이터
adilkhatri replied on Permalink
Totosite Safety Playground, No.1 Recommended for eating and drinking, please try to verify and report. It is the number one in the community that provides an optimized interface. 먹튀검증
adilkhatri replied on Permalink
This post is extremely radiant. I extremely like this post. It is outstanding amongst other posts that I ve read in quite a while. Much obliged for this better than average post. I truly value it! 토토사이트
adilkhatri replied on Permalink
Are you still trying to solve this problem by yourself? Now, try it with Muktuword. Toto site eatery solution community. 토토사이트
adilkhatri replied on Permalink
This is my first time I visit here. I discovered such a significant number of engaging stuff in your blog, particularly its talk. From the huge amounts of remarks on your articles, I figure I am by all account not the only one having all the recreation here! Keep doing awesome. I have been importance to compose something like this on my site and you have given me a thought. dentist chico ca
Digital_work replied on Permalink
Keep up the good work; I read few posts on this website, including I consider that your blog is fascinating and has sets of the fantastic piece of information. Thanks for your valuable efforts. Ufabet
adilkhatri replied on Permalink
When you sign up for a website, personal information and financial damage occur a lot. In most cases, the ID is immediately suspended when inducing additional deposit or applying for currency exchange. In the event of damage, a quick smudge report prevents additional victims. 먹튀사이트
jackryan replied on Permalink
Wonderful article. Fascinating to read. I love to read such an excellent article. Thanks! It has made my task more and extra easy. Keep rocking. Leads genereren
adilkhatri replied on Permalink
Hello, I found your blog per Google bit looking for such kinda instructive prompt also your educate sees extremely noteworthy for me. ปั่นแปะออนไลน์
jackryan replied on Permalink
Wonderful article. Fascinating to read. I love to read such an excellent article. Thanks! It has made my task more and extra easy. Keep rocking. Leads genereren
adilkhatri replied on Permalink
I need you to thank for your season of this great read!!! I definately appreciate each and every piece of it and I have you bookmarked to look at new stuff of your blog an unquestionable requirement read blog! 토토사이트
adilkhatri replied on Permalink
Trying to say thanks won't simply be adequate, for the fantasti c clarity in your written work. I will quickly get your rss channel to remain educated of any updates. 안전놀이터
adilkhatri replied on Permalink
This is a social media platform called HotBox. You can share your stories, share images, videos, documents and audio files. It is a free speech social platform, speak your mind. We are also adding a new blogging tool for user profiles. Users will soon be able to publish their own articles and backlink to their sites but we are only going to allow articles with quality. List your business
adilkhatri replied on Permalink
I am another client of this site so here I saw different articles and posts posted by this site,I inquisitive more enthusiasm for some of them trust you will give more data on this points in your next articles. bihar Election 2020
adilkhatri replied on Permalink
Its most noticeably awful piece was that the product just worked discontinuously and the information was not exact. You clearly canot go up against anybody about what you have found if the data isn't right. สล็อตออนไลน์
adilkhatri replied on Permalink
This is my first time I visit here. I discovered such a significant number of engaging stuff in your blog, particularly its talk. From the huge amounts of remarks on your articles, I figure I am by all account not the only one having all the recreation here! Keep doing awesome. I have been importance to compose something like this on my site and you have given me a thought. fair credit reporting act compliant background checks
pawar91104 replied on Permalink
Amazing post !seriously you are post a very good blog harley quinn outfits
adilkhatri replied on Permalink
Its most noticeably awful piece was that the product just worked discontinuously and the information was not exact. You clearly canot go up against anybody about what you have found if the data isn't right. 발기부전
jackryan replied on Permalink
Wonderful article. Fascinating to read. I love to read such an excellent article. Thanks! It has made my task more and extra easy. Keep rocking. affärsjuridik
seomaster replied on Permalink
I like to recommend exclusively fine plus efficient information and facts, hence notice it:avtal
adilkhatri replied on Permalink
To a great degree lovely and interesting post. I was scanning for this kind of information and savored the experience of examining this one. glitter in bulk
adilkhatri replied on Permalink
Extremely pleasant and fascinating post. I was searching for this sort of data and appreciated perusing this one. Continue posting. Much obliged for sharing. USA Green Card
adilkhatri replied on Permalink
일산룸 최대규모 일산자이언트 일산카네기 추천. 일산룸
adilkhatri replied on Permalink
Its most noticeably awful piece was that the product just worked discontinuously and the information was not exact. You clearly canot go up against anybody about what you have found if the data isn't right. lsd sheets
adilkhatri replied on Permalink
The site is affectionately adjusted and spared as much as date. So it ought to be, a debt of gratitude is in order for offering this to us. 토토커뮤니티
jackryan replied on Permalink
Wonderful article. Fascinating to read. I love to read such an excellent article. Thanks! It has made my task more and extra easy. Keep rocking. Erotische massage Limburg
jackryan replied on Permalink
Wonderful article. Fascinating to read. I love to read such an excellent article. Thanks! It has made my task more and extra easy. Keep rocking. Zonnepanelen
panistefanin replied on Permalink
Dziękuję za informacje! Szukałem i nie mogłem znaleźć. Pomogłeś mi! 1 USD to CAD
adilkhatri replied on Permalink
It is perfect time to make some plans for the future and it is time to be happy. I’ve read this post and if I could I desire to suggest you few interesting things or tips. Perhaps you could write next articles referring to this article. I want to read more things about it! cash for cars
Pages