that's true and i make plenty; he ordered the unit on new years day, a P30; we are now talking about a P130; but i think what he's really talking about is this.
Hi- I've purchased a PA140 and am having a hard time welding with 1/8 6011 rod. I've tried all heats from 60-140A. The arc seems very unstable. I find that the only way to kep an arc going is to...





Reply With Quote