S-6 Mig wires differ
		
		
				
					
					
				
				
		
			
				
					I was welding and ran out of wire got a roll of Lincoln S-6 Mig wire .035 from Princess Auto put it in spool gun and it welds different then the S-6 Unibraze wire it will not spray weld. The Lincoln wire dose not flow as nice as the Unibraze. The setting are the same but it sure dose not weld as nice more splatter then ever. Then tried a old roll of Princess Auto S-6 wire and it is different again better then Lincoln's wire but not as good as Unibraze S-6.
				
			 
			
		 
			
				
			
				
			
			