How about this one? I used 3/32 gap but one side opened up to almost a 1/8th and the other side closed up on me to a tight 3/32 gap. I used 3/32 ER70S-6 with 3/32 tungsten. Amp settings was 85 on the right side then turned it down to 80 when using my left hand. Because I figured the pipe was already pretty hot. Argon set at 10 L/min whatever that is equal to in cfh (my welder came with this funky gauge for the gas). Anyway I will try another later and get a better fitup. Let me know what you all think. The last pic is how they were looking before now so you can see my excitement.
I am just excited to see the root all the way in finally :-)
Click image for larger version. 

Name:	uploadfromtaptalk1367020753263.jpg 
Views:	1837 
Size:	57.0 KB 
ID:	9952
Click image for larger version. 

Name:	uploadfromtaptalk1367020773956.jpg 
Views:	1360 
Size:	55.3 KB 
ID:	9953
Click image for larger version. 

Name:	uploadfromtaptalk1367020794022.jpg 
Views:	4988 
Size:	71.7 KB 
ID:	9954
Click image for larger version. 

Name:	uploadfromtaptalk1367020807829.jpg 
Views:	1757 
Size:	49.2 KB 
ID:	9955