Thread: Wire Spool Binding

  1. #1

    Default Wire Spool Binding

    Ok I hope this makes since. I have an I-MIG 200 and lately I've been having issues with the wire spool binding on the shaft that it turns on. It still turns and welds fine but it makes this terrible noise like a tupperware burp (farting). I'm using a 10 pound spool of wire. I put a little oil on it with my finger and it stopped for about a day but now it's doing it again. Am I the only one having this issue? I don't like how the spool rides on the washer rather than the shaft. Is there some sort of adapter I could get to increase the size of the shaft hahaha? No but really. I hope you get what I'm talking about. I'm sure this binding will eventually cause a problem with the wire feed motor so I want to take care of the problem ASAP.
    Alvarez Metal Works
    Syracuse/DeWitt, NY
    www.alvarezmetalworks.com
    www.upstate4x4.com

    *** PowerTIG 210 EXT *** PowerPlasma 50 *** I-MIG 200 ***

  2. #2

    Default

    I just looked at a IMIG200, no spool in it of course at the moment (4043 and spool gun).

    Make sure the wingnut is not too tight. I will add a spool later (when I open up everything) and see what I find. I know the wire feeder rollers pull the wire and turn the spool, the back does not turns. The spool just rides on it. We have ran many 10lbs spool in them and no noise. So something is up.

    Can you tell if the sound is from the roller area or the backshaft that holds the spool. Maybe some wax on the inside of the washers edge, but you might have the wingnut too tight.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #3

    Default

    Remove the wire from the machine and check the plastic spool for cracks at the edge of the hub. If it's cracked the wire can pull down into the side of the spool as it rotates causing it to bind. Click image for larger version. 

Name:	spool.jpg 
Views:	422 
Size:	20.5 KB 
ID:	9455
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4

    Default

    I'll check the spool again for damage later today when I get home. The binding is on the outer edge where the spool comes in contact with the outside washer. That's where I put the oil and the noise stopped for the day. I like the adapter option allot. I don't like the current design. I'd rather have the welder not accept the smaller spools of wire (I have no need for them) than to keep this current setup. I might be alone in the thought though. The wing nut isn't too tight. If I loosen the wing nut the spool won't sit properly.
    Alvarez Metal Works
    Syracuse/DeWitt, NY
    www.alvarezmetalworks.com
    www.upstate4x4.com

    *** PowerTIG 210 EXT *** PowerPlasma 50 *** I-MIG 200 ***

  5. #5

    Default

    Quote Originally Posted by everlastsupport View Post
    the back does not turns. The spool just rides on it.
    Should the front outside washer turn? Mine doesn't.
    Alvarez Metal Works
    Syracuse/DeWitt, NY
    www.alvarezmetalworks.com
    www.upstate4x4.com

    *** PowerTIG 210 EXT *** PowerPlasma 50 *** I-MIG 200 ***

  6. #6

    Default

    Quote Originally Posted by Rafael View Post
    Should the front outside washer turn? Mine doesn't.
    No, it's keyed on the shaft.

    Yea, check for burrs on the spool too. Do you have any wax? Candles? You can see if they helps. Be careful with any sprays, or take it off, spray and put back on so nothing gets on the wire. Make sure no cracks like mentioned (check on the inside too, could be there).

    They do get bounced around in shipping and 10-12lbs all on top of each other. Also make sure the end of the wire is not sticking out and making the noise.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7

    Default

    If you have the wire spool too tight it will make those noises. It probably feels as if it is struggling to weld, when you loosen the nut it will weld 10x smoother.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  8. #8

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    If you have the wire spool too tight it will make those noises. It probably feels as if it is struggling to weld, when you loosen the nut it will weld 10x smoother.
    That's still my thought.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  9. #9
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    If you have the wire spool too tight it will make those noises. It probably feels as if it is struggling to weld, when you loosen the nut it will weld 10x smoother.
    That's what I was thinking too. If you loop the loose (stinger end) of the wire into the spool housing so the spool doesn't unravel, can you spin the spool on the shaft easily by hand? Any strange noises while doing this (with the machine off)? Does the keyed washer have a sharp burr on the edge leftover from the stamping process? As Mike suggested, look at the "dead end" of the wire on the spool to see if it's sticking out too far and dragging on the inside of the machine as it spins.

    Other than that, I can't think of anything else in that area that would cause problems.
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  10. #10

    Default

    Don't see anything that could be causing it. I even loosened the nut to the point where it's barely holding the spool up. I just rubbed some more oil on the washer with my finger and I'll wait until this spool is gone. If it does it with the new spool I'll let you know.
    Alvarez Metal Works
    Syracuse/DeWitt, NY
    www.alvarezmetalworks.com
    www.upstate4x4.com

    *** PowerTIG 210 EXT *** PowerPlasma 50 *** I-MIG 200 ***

  11. #11

    Default

    The way I was taught to adjust the wire spool tension is to angle the gun and hold it against a slick surface (against the welder). Pull the trigger and the wire should curl. If the wire pushes on the gun and does not curl then you have too much tension. You want the spool to spin with ease, but you don't want the spool to spin freely. In other words when you let off the trigger the spool stops and does NOT continue to spin.

    Also how do you have wing nut, spring, and washer in place? I put on the spool with the plate that goes in the center and align. Put the spring on the shaft it will go against the metal plate. Put the washer against the (outside) spring, and tighten the wing against the washer. I've played with it but this works the best.

    What is the brand name wire?
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  12. #12

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    The way I was taught to adjust the wire spool tension is to angle the gun and hold it against a slick surface (against the welder). Pull the trigger and the wire should curl. If the wire pushes on the gun and does not curl then you have too much tension. You want the spool to spin with ease, but you don't want the spool to spin freely. In other words when you let off the trigger the spool stops and does NOT continue to spin.
    That's the way to adjust the drive roller tension Click image for larger version. 

Name:	IMG_1234 - Copy.jpg 
Views:	572 
Size:	140.2 KB 
ID:	9500 The spool tension should only be tight enough to prevent backlash when you release the trigger.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  13. #13

    Default

    Could it be something as simple as having the spool on backwards,,the wire should feed in from the bottom of the spool...spool tension on a new 10 lb spool should be almost non existent as if turns slowly when it is new..
    Some of those lies people tell about me, are true

  14. #14

    Default

    So here is an update. I didn't change a thing just let the spool of wire run out and swapped put in a new spool. No more noise. I think it may have had something to do with old sticker gunk on the spool. I went with a MUCH CHEAPER MIG wire from www.usaweld.com this time and love it. Two spools for the price I was paying for one Hobart spool.
    Alvarez Metal Works
    Syracuse/DeWitt, NY
    www.alvarezmetalworks.com
    www.upstate4x4.com

    *** PowerTIG 210 EXT *** PowerPlasma 50 *** I-MIG 200 ***

  15. #15

    Default

    Maybe the spool was not wound well? The one that made the noise. Or at the end of it unwound. Either what glad it is all worked out.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. wire speed of spool gun sm100n and sm3035n????
    By Doc Pete in forum General Welding Questions
    Replies: 3
    Last Post: 04-03-2016, 11:44 PM
  2. Wire speed not working on spool gun for 251si
    By seaarc24 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 0
    Last Post: 11-03-2015, 09:01 PM
  3. How to load Mig wire spool???
    By Dr. Fell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 6
    Last Post: 08-11-2012, 02:47 PM
  4. Replies: 26
    Last Post: 02-22-2012, 11:25 AM
  5. Spool Spool / Roll Adaptor for Power IMIg250P, DYI
    By Ray in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 3
    Last Post: 08-10-2010, 07:46 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •