    I have a bunch of welds to do that need back purge gas only while actually welding. So I figured now's the time to setup my LX225 with an electrical connector to run an auxiliary gas solenoid. I thought about it a bit. There is no serious problem with any sort of plan, since the relay that runs the existing solenoid is rated for 5A/250VAC and the solenoid consumes about 100ma. But then I had to run 240VAC to the aux solenoid, or setup a 240VAC coil relay in the welder, obviously drill out a hole for a connector, mount all that up, etc, etc, then get on to plumbing in a solenoid valve.

    It all seemed like a lot of work, and then it occured to me that I could do it all up at the regulator. All I'm using is a 3 way spring return single pilot valve. Sounds complicated, but this is simply a valve which sends it's input out one port or another depending on whether it sees pressure on a control port. (Actually, this was an old pilot solenoid valve that was kicking around, but I disabled that by blocking off the solenoid ports. It just so happened to be easy to set up for air operation.) The "normally shut" output port is plugged, and the "normally open" port goes into the back purge flowmeter. The input comes from the manifold after the main pressure regulator. The control signal comes off from after the torch flow control.

    When you press the pedal and the torch gas solenoid opens, the pressure after it's flow control drops to practically zero. This turns the the valve to the "normally open" position, allowing gas to flow through the purge flow control. When you stop and the gas solenoid closes, some pressure builds up after the flow meter (~15 psi?) which directs it's input into the "normally shut" port, which is blocked off.

    When I want to get a continuous flow through the back purge, I simply remove the control line from the valve and plug it. When I don't need the back purge, I wind the flow control all the way in.

    I'm sure I'm not the first to do this, but I haven't seen it out there. At least I don't think I have.

    Click image for larger version. 

Name:	2012-09-26 18.38.29.jpg 
Views:	788 
Size:	50.3 KB 
ID:	8089
    Sorry about the crappy cell phone pictures. It's a little tight back there. Oh, the brass flow control on the left is the torch one, and the silver Everlast one is the back purge.
    Click image for larger version. 

Name:	2012-09-26 18.38.08.jpg 
Views:	875 
Size:	79.5 KB 
ID:	8088

    (PS - by "normally open" I mean normally connected to the input port. Unfortunately the opposite of an electrical switch!)
    Last edited by Paul Moir; 09-28-2012 at 03:51 AM.

  2. #2

    Default

    Here's my simple solution. Click image for larger version. 

Name:	IMG_1197.jpg 
Views:	815 
Size:	130.7 KB 
ID:	8094 works well.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Paul Moir View Post
    I'm sure I'm not the first to do this, but I haven't seen it out there. At least I don't think I have.
    Nice setup. I bet it really saves on gas, when the back purge area is not very gas tight. Especially if you have to start and stop a lot to position or move around.
    Long arc, short arc, heliarc and in-the-dark!

  4. #4
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    Zoama - that's exactly what I had before. The valve is an addition to automatically turn it on when I key the torch. Even with a valve at the end, you end up wasting a lot of gas: crack open the valve, blow off the pressure in the line, get ready to weld, weld, turn off the valve. It doesn't help that I'm paying the small bottle tax.

    Rambozo - The task is to weld a bunch of pins to some sheet metal. I'm using a gas lens to hold the pins and purge the porcupine side, and then fuse down the back side (leaving a bit of rod sticking up for material to work with). But there are lots of times I find I want to purge the back side, but wouldn't bother because of the waste of gas & put up with dealing with popcorn. No more popcorn for me!
    Last edited by Paul Moir; 09-28-2012 at 04:59 AM.

  5. #5

    Default

    Quote Originally Posted by zoama585 View Post
    Here's my simple solution. Click image for larger version. 

Name:	IMG_1197.jpg 
Views:	815 
Size:	130.7 KB 
ID:	8094 works well.
    He just wondering a little about this setup. Are the fittings 1/4 npt or 1/8 npt. Also did you buy a tee for high pressure rating or is that not needed?
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by scootarida1 View Post
    He just wondering a little about this setup. Are the fittings 1/4 npt or 1/8 npt. Also did you buy a tee for high pressure rating or is that not needed?
    That tee is 1/4"NPT and since it's after the regulator the pressure is low (under 100 psi).
    Long arc, short arc, heliarc and in-the-dark!

  7. #7

    Default

    Quote Originally Posted by scootarida1 View Post
    He just wondering a little about this setup. Are the fittings 1/4 npt or 1/8 npt. Also did you buy a tee for high pressure rating or is that not needed?
    It's as Rambozo said. If you make one of these be careful not to overtighten the fitting going into the regulator, too much force could crack it.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  8. Default

    Quote Originally Posted by zoama585 View Post
    Here's my simple solution. Click image for larger version. 

Name:	IMG_1197.jpg 
Views:	815 
Size:	130.7 KB 
ID:	8094 works well.
    Hey where did you get those little regulators on the left from ? I need to back purge and this would be a quick way for me to get a set up.

  9. #9

    Default

    Quote Originally Posted by Vinhtec View Post
    Hey where did you get those little regulators on the left from ? I need to back purge and this would be a quick way for me to get a set up.
    It's the standard regulator/flow meter that comes with the welder Click image for larger version. 

Name:	324_1[1].jpg 
Views:	614 
Size:	35.6 KB 
ID:	8219 plus a tee, a 1/4" npt close nipple and the flow meter from another everlast regulator.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  10. Default

    Quote Originally Posted by zoama585 View Post
    It's the standard regulator/flow meter that comes with the welder Click image for larger version. 

Name:	324_1[1].jpg 
Views:	614 
Size:	35.6 KB 
ID:	8219 plus a tee, a 1/4" npt close nipple and the flow meter from another everlast regulator.
    Ohhh that was a dumb question for me to ask. I see now Ill try to make something like that too !

  11. #11

    Default

    Quote Originally Posted by Vinhtec View Post
    Ohhh that was a dumb question for me to ask. I see now Ill try to make something like that too !
    There's no such thing as a dumb question... ask me anything.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  12. Default

    Zoama Thanks man your a cool guy forums need more of you ! I cant wait to get my machine back and weld more !!!!!!

  13. #13

    Smile

    There's no such thing as a dumb question... ask me anything.
    Ok, here goes
    On one picture of the guage, it shows female threads, then another picture, it shows male threads?
    I know male threads are what goes into the tanks.

  14. #14
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Markcuda View Post
    Ok, here goes
    On one picture of the guage, it shows female threads, then another picture, it shows male threads?
    I know male threads are what goes into the tanks.
    The Everlast Flowmeters are male so they screw into the female Tee, then use a close nipple to screw the Tee into the regulator. Different makers use a mix of male and female so you might need a slightly different setup. You might also want different length nipples to make it easier to screw things together or to have them point the same direction. There are fittings for whatever you need.


    Click image for larger version. 

Name:	Pic.JPG 
Views:	1164 
Size:	135.3 KB 
ID:	9008
    Long arc, short arc, heliarc and in-the-dark!

  15. #15

    Default

    Quote Originally Posted by Markcuda View Post
    Ok, here goes
    On one picture of the guage, it shows female threads, then another picture, it shows male threads?
    I know male threads are what goes into the tanks.
    I just noticed that I grabbed the wrong pic. All the regulators that come with everlast welders are male into the tank. I just used two standard regulators plus a tee to make a purge setup.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  16. #16

    Cool

    All the regulators that come with everlast welders are male into the tank.
    Ok great, I was worried a tad bit

  17. #17

    Default

    Now everlast needs to sell just the flow meter parts if they don't already...
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

Similar Threads

  1. Easy on the eyes theme barter?
    By zeus_r6 in forum Forum related Questions
    Replies: 4
    Last Post: 06-05-2013, 11:23 PM
  2. To Purge or not to Purge
    By Rectified in forum General Welding Questions
    Replies: 7
    Last Post: 03-23-2013, 02:59 AM
  3. easy quick bending fork
    By Winky in forum Hobyist Projects
    Replies: 0
    Last Post: 11-28-2012, 05:06 PM
  4. Dual Flow Regulator for Purge ?
    By zoama in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 05-30-2012, 09:38 PM
  5. Using a gas Y for Tig purge line
    By worntorn in forum TIG Welding (GTAW/GTAW-P)
    Replies: 12
    Last Post: 03-19-2011, 12:02 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •