    Default 250 ex problems

    was welding on some .100 thick aluminum today and could not strick an arc without touching the materail ,then it would weld just fine and when i stopped had to touch again to get the arc started again,gas was at around 7 lpm 3/32 lanthanated tungsten,i even tried to strike arc on my ground clamp to make sure it was not a grounding issue, still same thing happened also my gas has been staying on when i am done welding almost like i have my post flow on,but i dont,then sometimes when i push on my pedal again it goes off.

  2. #2

    Default

    Quote Originally Posted by johnson697 View Post
    was welding on some .100 thick aluminum today and could not strick an arc without touching the materail ,then it would weld just fine and when i stopped had to touch again to get the arc started again,gas was at around 7 lpm 3/32 lanthanated tungsten,i even tried to strike arc on my ground clamp to make sure it was not a grounding issue, still same thing happened also my gas has been staying on when i am done welding almost like i have my post flow on,but i dont,then sometimes when i push on my pedal again it goes off.
    The switch on your foot pedal may be hanging. Make sure it rocks fully down on the switch, or it may need to be adjusted. Have you tried it with the torch switch? Are you getting any spark at all? If so, then it probably needs a point gap adjustment.

  3. #3

    Default

    point gap adjusted to .035 and i am getting spark at the tungsten but it just will not start an arc.how do you adjust the pedal?

  4. #4

    Default

    Quote Originally Posted by johnson697 View Post
    point gap adjusted to .035 and i am getting spark at the tungsten but it just will not start an arc.how do you adjust the pedal?
    What are your settings....and did you examine the pedal switch for sticking or not fully operating? You can try to widen the gap a little more. Can you lift start?

  5. #5

    Default

    what gap should i set it at?

  6. #6

    Default

    Quote Originally Posted by johnson697 View Post
    what gap should i set it at?
    .030 to .040 is fine. Does it work with the torch switch? Remove the pedal and see it is welds. If it does we can look into the foot pedal.

    Also sounds like maybe the solenoid is sticky, have you called tech support, they can walk you through the solenoid, spring sometimes is a little tight.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7

    Default

    yes talked to mark and he said the same thing with gap spread,havent tried using the torch switch.

  8. #8

    Default

    OK..set gap to .045 and still the same thing so i am gonna set them at .030 and try them again ,not comfortable trying to reset them again after i already had machine on so i am gonna wait till tommorow and try again.

  9. #9

    Default

    Ten to fifteen minutes is all you need.

  10. #10

    Default

    wow...wished i would have known that before ,just trying to be safe,hope fully the .030 works.

  11. #11

    Default

    I also have another pedal that everlast sent was a wrong pedal that has a nob on the front of pedal,anyway i could unhook wires from nob on front of pedal and use that pedal on my 250 ex?

  12. Default same problem

    I just pulled my 250ex out to do some aluminum and I am having the same problem. Did you ever get it to work, What was it?

    Thanks Jeff

  13. Default

    Do you have the switch on the control panel set for TIG (HF)? If not your in tig lift mode and it works the way you describe.

  14. Default tig hf

    I do have the switch in TIG (hf).

  15. #15
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Follow the same steps, try the torch switch, check the points.

    Make sure your preflow isn't cranked up.
    Long arc, short arc, heliarc and in-the-dark!

  16. Default

    I did try the trigger switch and checked the preflow. Same result. When I first turned it on it worked three time on the pedal and with the trigger and then it stopped again and would have to scratch start again. How do you check the points?

  17. #17
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by gree box View Post
    I did try the trigger switch and checked the preflow. Same result. When I first turned it on it worked three time on the pedal and with the trigger and then it stopped again and would have to scratch start again. How do you check the points?
    Give tech support a call and they will walk you through it. You are basically checking the gap between them with a feeler gauge. There are also some wire connections they will have you check.
    Long arc, short arc, heliarc and in-the-dark!

  18. Default update

    I talked to Ray today with tech support. He walked me threw the troubleshooting. Come to find out when I put the welder on my new cart I must have unplugged all the leads. When I hooked it back up I put the ground lead in the negative port and the tig torch in the positive port. Human error on my part. All is good now.

  19. #19

    Default

    Normally the tungsten will burn up on you. But it's always best to post pictures of the machine and welds if you can.

    Glad you are up and running again.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Seriously?! (NEW 51-P problems)
    By tdkask in forum Everlast Plasma Cutters (PAC)
    Replies: 5
    Last Post: 05-25-2016, 11:43 PM
  2. a few problems?
    By nikstiks in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 11-11-2014, 08:15 AM
  3. PP205 problems--
    By JBnID in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 0
    Last Post: 08-23-2014, 06:21 PM
  4. Plasma Problems
    By Slartybartfa in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 34
    Last Post: 07-03-2012, 02:03 AM
  5. MIG 200 tip problems
    By countrygardener in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 7
    Last Post: 11-08-2010, 08:47 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •