    I need to cut several 4" circles so that 4" PVC will fit loosely in them.

    Is it possible to use a small cut off piece of the PVC and basically trace around the PVC with the plasma cutter while cutting the hole?
    Yess, I can freehand it but I would like it to look a little better than freehand and I don't want to do a lot of work after the cut.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default

    Seems like it would work, but the PVC might get a bit melty and make a mess. The offset from the torch would be pretty large too ... I think you would end up with at least a 5" hole. You might want to try a 3" pipe to make the size a bit closer.

    Cheers
    Mike
    Power Pro 256

  3. Default

    2x what posixPilot said. I think a tuna can might work pretty well also.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  4. #4

    Default

    Quote Originally Posted by CGCINC View Post
    I need to cut several 4" circles so that 4" PVC will fit loosely in them.

    Is it possible to use a small cut off piece of the PVC and basically trace around the PVC with the plasma cutter while cutting the hole?
    Yess, I can freehand it but I would like it to look a little better than freehand and I don't want to do a lot of work after the cut.
    A good chance to try your bandsaw in vertical position, and cut a disc out of wood the right diameter. Can allow for the lesser dimension due to the torch cone. Draw your plasma around that. If you put a short broom handle-like handle on it, would help get your pattern holding hand out of the way of the torch.

    ken
    UNT 520D plasma/stick/tig; Hobart Handler 140 Mig; HF 80amp stick welder; Victor O/A; 4x6 Horizontal bandsaw; Planishing hammer; & Stuff

  5. #5
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by KSmith View Post
    A good chance to try your bandsaw in vertical position, and cut a disc out of wood the right diameter. Can allow for the lesser dimension due to the torch cone. Draw your plasma around that. If you put a short broom handle-like handle on it, would help get your pattern holding hand out of the way of the torch.

    ken
    I like your idea about the broomstick. CGCINC will need to ensure all fleshy bits are well away from the cutting arc. The circle is going to be quite small. Probably won't be able to cut the circle in one go if the blade is wide but sure if you take a few swipes at it.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    I don't know about a plasma, but with a cutting torch, I've often used a piece of string or wire with a loop tied in one end to guide around a circle. Infinitely adjustable and just secure the other end to the center with a drilled hole or a tacked on post. Nothing to block your progress, one quick pass and you're done. Cheap, easy and fast circle cutter. I can't freehand anything worth a damn.
    Long arc, short arc, heliarc and in-the-dark!

  7. #7

    Default

    Quote Originally Posted by Rambozo View Post
    I don't know about a plasma, but with a cutting torch, I've often used a piece of string or wire with a loop tied in one end to guide around a circle. Infinitely adjustable and just secure the other end to the center with a drilled hole or a tacked on post. Nothing to block your progress, one quick pass and you're done. Cheap, easy and fast circle cutter. I can't freehand anything worth a damn.
    Rambozo is right, this method is simple works quite well on about everything but expanded metal.

    This is something quick and dirty I made and it worked quite well (but you need a magnet; maybe $2 at Hf and it came with two of them).

    http://www.everlastgenerators.com/fo...ghlight=magnet

    Then later bought this setup.

    http://www.everlastgenerators.com/fo...t=plasmahelper

    Waiting on Rod to chime in here with his 5HP 4 stroke plasma circle cutter. Kidding Rod
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  8. #8

    Default

    You could also make your own circle cutter with some shaft collars. Get one collar that will fit your plasma torch. Weld a piece of 3/8" round bar to the collar that fits the plasma torch. Get a 3/8" collar and weld a 1/8" piece of round stock to it so it will be your center point. The 3/8" collar will slide up and down the 3/8" round stock making it adjustable. It would probably cost you $10.00 to make, and you would have an adjustable hole cutter.

    Swagg Offroad has one that's not to pricey.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  9. Default

    You could also get something like this and add a threaded rod with a sliding anchor point to it. I find this makes any tupe of circular motion a breeze as you can loosen the outer ring and this allows turning much easier compared to a stationary stand-off
    Cheers
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	A81 Sitewheel 001.jpg 
Views:	419 
Size:	138.5 KB 
ID:	7388  
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  10. #10

    Default

    All great ideas!

    I bought a 3" coupling to try it but it was going to be too small so I ended up just free handing it.
    Works for what I'm doing right now but I like the adjustable collar idea that Seanmurphy265 had!

    Thanks everyone, you soon will see my Amazing free hand abilities!!! lol
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

Similar Threads

  1. Powerpro 164 Plasma Cutter intermittently not cutting through 0.400" thk SS.
    By gtty in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 8
    Last Post: 08-03-2014, 01:00 PM
  2. 1/2" Cutting troubles, asking for insight
    By LMironworks in forum Everlast Plasma Cutters (PAC)
    Replies: 9
    Last Post: 02-04-2014, 05:27 AM
  3. Anybody cutting 1"?
    By Jake98 in forum Everlast Plasma Cutters (PAC)
    Replies: 19
    Last Post: 05-11-2012, 05:19 PM
  4. Cutting 3"x3"x3/16" Angle
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-01-2011, 11:56 PM
  5. Oxy-Acetylene Cutting 1/2" Thick Steel Fire Barrel
    By jakeru in forum Other Custom Fabrications
    Replies: 0
    Last Post: 03-04-2011, 10:20 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •