Share
Page 2 of 2 FirstFirst 12
Results 21 to 29 of 29

Thread: Everlast, I need a different torch. Which one to buy?

  1. #21

    Default

    I will Friday when I get off.
    Purple Fabricator 211i

  2. #22

    Default

    Quote Originally Posted by NRM View Post
    Buggy Chief and 225 will you take some pics of the included torch (WP-26???) and your new ck210/ck130 side-by-side to show the size differences? I am interested in both torches and just want to see a visual comparison to the original torch since I can’t locate them locally.
    It's hard to put them close enough together to get a good comparison. The blue handle torch on the left is water cooled and came with my PP256.
    Click image for larger version. 

Name:	IMG_1213 - Copy.jpg 
Views:	555 
Size:	145.6 KB 
ID:	6928Click image for larger version. 

Name:	IMG_1214.jpg 
Views:	510 
Size:	146.6 KB 
ID:	6929Click image for larger version. 

Name:	IMG_1215.jpg 
Views:	507 
Size:	146.5 KB 
ID:	6930Click image for larger version. 

Name:	IMG_1216.jpg 
Views:	484 
Size:	146.6 KB 
ID:	6931Click image for larger version. 

Name:	IMG_1217.jpg 
Views:	471 
Size:	145.5 KB 
ID:	6932

    I let them all hang freely about 15 inches from the the torch head to give an idea of the lead's flexibility. Same order as in the first pic.
    The CK130 is my favorite, I use it up to 150amp @ 60% duty cycle. It's rated @130amp AC/DC @ 100% duty cycle.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #23
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by zoama585 View Post
    It's hard to put them close enough together to get a good comparison. The blue handle torch on the left is water cooled and came with my PP256.

    I let them all hang freely about 15 inches from the the torch head to give an idea of the lead's flexibility. Same order as in the first pic.
    The CK130 is my favorite, I use it up to 150amp @ 60% duty cycle. It's rated @130amp AC/DC @ 100% duty cycle.
    Very kind of you to remind us that you put in your own switch on the CK130. Nice comparison and I can see why you say the lead is as limp as a wet noodle. Day and night ...
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  4. #24

    Default

    Quote Originally Posted by undercut View Post
    Very kind of you to remind us that you put in your own switch on the CK130. Nice comparison and I can see why you say the lead is as limp as a wet noodle. Day and night ...
    It was about 92 degrees in my unfinished shop when I took those pics. At 50 degrees the rubber lead torches would've had very little bend, but they get softer as they warm up in use.
    The superflex leads are the same at any temp but the 200amp lead is relatively heavy.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #25
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Agreed on the density of the 200 amp CK (Trimline 210) superflex lead. That is it's only downside, IMO. It's most noticeable if it's hanging straight down a long distance. I will just drape the lead over my shoulder or around my neck to take the weight off, if that's the case.

    On the plus side, it seems virtually indestructable. I have yet to blow it up, and I've been pretty hard on it with my 200 amp, 60% duty cycle machine. I can't say the same for the old WP-17, whose cable suffered a melt down. I seriously wonder if it might even be OK to use it with substantially more than 200 amps.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  6. #26

    Default

    My holding mine almost pencil will tell you how small it is. She is 5' 2". Very tiny hands.
    Purple Fabricator 211i

  7. #27
    Join Date
    Mar 2012
    Location
    Melbourne, Australia
    Posts
    5

    Default

    zoama585, is your CK210 a Trim-Line?
    I have seen jakeru's picture of his CK210 which also says "Trim-Line", but looking on the CK website, I can only find the 'standard' CK210.
    In Trim-Line, they list the TL26 as the 200A torch.

    After picking up a 9 series torch recently with a super / high flex cable, I don't think I ever want to go back to a 'standard' cable.

  8. Default

    Zoama thanks for taking the time to put the pics together. I was at a LWS yesterday and they had the ck210 w/valve 1 piece and it really felt big but the superflex cable was really nice. They are getting pricing for me so I will see how it compares to prices online.
    PowerPro 205
    9" South Bend Lathe
    Enco Mill/Drill
    Evolution Rage 2

  9. #29
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Quote Originally Posted by 225 View Post
    My holding mine almost pencil will tell you how small it is. She is 5' 2". Very tiny hands.
    Based on the OD of the teflon insulator being flush with the torch head, and there being a "2 series consumables" paper in the box, I'd say it looks like you got the CK130.
    '13 Everlast 255EXT
    '07 Everlast Super200P

Similar Threads

  1. where can i buy a new tig torch for my everlast power tig 200 dx-d
    By steve1989 in forum General Welding Questions
    Replies: 4
    Last Post: 12-28-2015, 12:04 AM
  2. How to I use this Everlast torch.
    By Judgeless in forum TIG Welding (GTAW/GTAW-P)
    Replies: 46
    Last Post: 06-16-2014, 12:33 AM
  3. Tig torch video from Everlast
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 1
    Last Post: 08-26-2012, 03:14 AM
  4. New Everlast Amp control torch
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 2
    Last Post: 07-12-2012, 04:13 PM
  5. Everlast Tig Torch for sale
    By acourtjester in forum Buy, Sale or Trade
    Replies: 5
    Last Post: 06-07-2011, 08:24 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •