    Default

    Thanks for the pic.
    Joe
    CH 110 mig/flux
    Looking to step up to Everlast tig

  2. Default

    no problem!

  3. Default

    Quote Originally Posted by performance View Post
    Originally it wasn't put there. I know, because I wrote it. Apparently in some changes in the site, some templates got changed. The web guys are constantly making changes, and it is hard to keep up with when they do or undo something and screw up a page.

    ...but on the other hand, I have had several call me up and say they wish they had bought the separate units.
    Your post that is quoted above is from March 2011. I ordered in October 2010 and remember "Fabrication, Industrial, and Motorsports" were CLEARLY listed then too, but it looks like I should have gotten a 250EX from what you're saying. If the PP256 is not truly intended for those environments then why on Oct 12, 2011 is it STILL listed that way. I feel like I got punched in the nuts! I'm thinking about a mig setup which is why I'm here but.. I don't know.
    Last edited by mrprism; 10-12-2011 at 05:36 AM. Reason: terminology

  4. Default

    Hey ASE_MasterTech, How do you like your Longevity 256PI? How does it compare to the PP256? Do you have any input on other Longevity products? I have an automotive fab and production shop and just want to be guided to the right mig welder choice. I currently only have a 120V mig so anything pretty thick needs to be Tig welded which costs me time. Red and Blue are awesome, but I think they are a bit overpriced. I have an opportunity to get a good deal on an Everlast but don't want to make the wrong choice in welder again. Input welcome.
    Last edited by mrprism; 10-12-2011 at 07:35 AM. Reason: spelling

  5. #25

    Default

    If I had a shop, I would go with the 250EX. A dedicated heavier duty cycle machine. A little lighter in weight (not a big deal). Takes up more space, but no hose and torch swapping between welding and cutting. You can save a lot of money with us, but the bigger price bang on our products come with some trade offs too.

    I have use the PP256, nothing wrong with it, but I like a dedicated TIG and higher duty.

    As far as the competition, I would check everyones forums to see when we announced our PP256 units and how long before other announced something like it with a 256 in the name and the IGBT drivers. You will find who the leader and innovator is. You will also find only a couple even offer a product like we designed.

    It all really comes down to you and your needs. I am sure people that have used our units will chime in and you will hear but are good. I just know what I like.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  6. #26

    Default

    Quote Originally Posted by mrprism View Post
    Your post that is quoted above is from March 2011. I ordered in October 2010 and remember "Fabrication, Industrial, and Motorsports" were CLEARLY listed then too, but it looks like I should have gotten a 250EX from what you're saying. If the PP256 is not truly intended for those environments then why on Oct 12, 2011 is it STILL listed that way. I feel like I got punched in the nuts! I'm thinking about a mig setup which is why I'm here but.. I don't know.
    Mrprism,

    A few things in reply:
    1) The 256 certainly welds nearly as good as any other product we sell. I'd give it a 90% on cutting (my personal belief).
    2) The remark made about "industrial" and "fabrication" is related to a production setting. It does not mean it can't serve in an industrial setting, but its design is intended to be used for repair and fabrication for things like you'd find in a small design or repair shop. A typical example of appropriate "industrial use" in my mind would be where they needed to take the unit through a factory to make a steam valve repair or a fix conveyor or a food table.
    3) Using your welder in any of these settings will not void the warranty. The unit is covered regardless of use, except for abuse (or dropping or running it in water)
    4) 35% has traditionally been a homeowner, small shop duty cycle. Until recently this was the standard until Miller's Marketing got in the way of good sense. Now they will tell you it is a
    "light industrial" duty cycle. Well since they are bigger than we are, who can argue? But if you pick up a text book or go back a few years in their literature, it'll tell you 60% is the gold standard for industrial use. Any thing less should be considered homeowner, hobby, or small shop duty.
    5) There's a lot packed into the same box as the 250EX, more parts, and more items and some sharing the same circuits, other not. Conventional wisdom will tell you that the more parts you have stuffed in the same space, and more parts in general decreases reliability. That is the major rub where we have tried to clarify the units application. A commercial facility expects nothing less than the most reliable product... and the 256, while not a BAD product doesn't reach the level of reliability of our other products because of the extra parts in side....Also most commercial facilities will not have a use for a machine that does double duty like this. They will have separate products. Again, the reason we have pointed out many times the application of this unit favors portable repair is that it does not require the carrying around of 2 units. This is a favorable item for portable repair, where operational efficiency isn't always expected. Changing the lines and hoses back and forth in a heavy industrial production setting ISN"T going to cut it for most companies.

    With that said, we do have people using them in places from factories to oil derricks on the sea.

    As far as our MIGs, I'll put my MIG up with any comparable MIG on the market. You'll find precious little complaints or service issues with these units. They will weld circles around any transformer welder of the same size class on the market of any company. And they will double duty as a stick welder. This isn't a "added" component feature as with the 256, and is accomplished with the existing circuitry. Add to it the inductance/arc force control, and the unit is the best on the market. We use heavier gear drive feeders, with all metal components as well. Spatter is almost non existent. Don't forget we actually use a name brand torch with our units, instead of a "copy" version. Beware of cheaply made MIG torches.
    Last edited by performance; 10-12-2011 at 02:43 PM.

  7. #27

    Default

    @ performance (Mark),
    What do you think of this hose setup for the PP256... there are no leaks and changing process only takes a few seconds.

    Click image for larger version. 

Name:	IMG_1155 - Copy.jpg 
Views:	452 
Size:	144.9 KB 
ID:	3616Click image for larger version. 

Name:	IMG_1156 - Copy.jpg 
Views:	475 
Size:	142.7 KB 
ID:	3617

    I'm not a sensitive person so make no effort to spare my feelings if you don't like the hose setup.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  8. #28

    Default

    As I have told others, that's not what I consider ideal.
    The problem is that the coupling and uncoupling of the lines leads to condensation in the mouths of the fittings, introducing moisture to the system. A static situation where valves are used is the best.

    It does not solve the changing out torch issue.

  9. #29

    Default

    Quote Originally Posted by performance View Post
    As I have told others, that's not what I consider ideal.
    The problem is that the coupling and uncoupling of the lines leads to condensation in the mouths of the fittings, introducing moisture to the system. A static situation where valves are used is the best.

    It does not solve the changing out torch issue.
    I see where it could get a little condensation under some circumstances but so far I haven't noticed anything. I'm never in a hurry since welding is just a hobby for me, but if I were in a hurry I believe I could change torches and hoses in about 40 seconds.
    Thanks for the opinion. I like to hear what others think, good bad or indifferent especially from professionals.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  10. #30

    Default

    well this basically made my mind up. i was on the fence over these two, thanks to everyone
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  11. #31

    Default

    Quote Originally Posted by jerky View Post
    well this basically made my mind up. i was on the fence over these two, thanks to everyone
    Which did you choose and why ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  12. #32

    Default

    Wow this seemed to ruffle a few feathers. I have been searching all over the web trying to decide on what size and brand of tig welder to buy and everybody has an opinon about red,blue.yellow or green. They all seem to agree stay away from combo tig plasma as they seem to have the most problem.

  13. #33

    Default

    think ill just go with the 250. i dont really need a plasma, it just would have been nice. what i dont need is more problems. the more stuff in one box, the more can go wrong, so for me, clear choice now.
    Journeyman welder
    250EX
    Power plasma 60
    horizontal band saw
    Miller digital elite 'wicked' lid

  14. #34
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    With the cost of the Everlast plasma cutters I would just opt to purchase a single unit over the multi function unit. I would agree with performance that when you get too many parts in an area that things just tend to be more unreliable.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  15. Default

    Quote Originally Posted by performance View Post
    The remark made about "industrial" and "fabrication" is related to a production setting. It does not mean it can't serve in an industrial setting, but its design is intended to be used for repair and fabrication for things like you'd find in a small design or repair shop.

    Changing the lines and hoses back and forth in a heavy industrial production setting ISN"T going to cut it for most companies.
    Ok I see what your getting at. Industrial and fabrication as far as something like a production line. I agree, I wouldn't think a company would have 15 or 20 PP256's in that type of setting, as you state, changing the lines and such would kill efficiency and production. PLUS you're welding all day long day after day. That requires a much higher duty cycle. I thought you were saying the 256 was strictly a hobbyist machine and had no real business in a professional shop. I have a small shop where we'll be welding one or maybe two projects at a time, and the welder is used at least 15 to 20 hours in a week. I have never had the machine quit because of a duty issue and its handy to be able to plasma some stuff when you need to. After you clarified your remarks and I thought about what you're getting at, I understand what you mean. I thought you were saying the machine didn't belong in a shop like mine when in fact, its a perfect fit. We don't weld constantly, we only need plasma once in a while, the projects we have are smaller in scale, (Alum manifold mods, turbo down pipes, suspension control arms, Caltrac bars etc.) and it supplements another small welder. I guess the terms "industrial" and "fabrication" are all relative in nature. I would consider us an automotive industrial small custom fab shop, but we're no Griffin Radiator or Hooker Headers either. All in all I don't know why I got so excited, once my issues were sorted out the 256 has been a great machine so far. I just thought you ment it wasn't intended for what we are using it for when in reality its a great fit.

    Alan

  16. Default

    Quote Originally Posted by zoama585 View Post
    I like to hear what others think, good bad or indifferent especially from professionals.
    The way you have the argon flowing through the water trap it is possible to pick up moisture in that bowl. I've heard of other guys making a manifold with ball valves which will work fine. The way I have my 256 set up is the cats ### IMHO. I bought a Miniature Diverting 3-Port PVC Ball Valve from McMaster-Carr. Part number 4757K57 for the valve with 1/4" barbed fittings and part number 4757K58 for the valve with 3/8" barbed fittings. Get the size that matches your welders hose size. I'll take a picture of mine tomorrow and post. It literally takes as long as a torch change to go from welding to cutting WITH ZERO MOISTURE! I may make a video displaying how fast one can from one mode to the next with this setup.

    Alan

  17. #37

    Default

    Having to switch gas supplies is like many things we all have a different way.
    Here is mine having a forum to show thing is a great help to see what other's have done and select the one you like.
    I find my project book gets larger from what I have seen posted and thats a good thing.

    have fun
    Tom
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	Welding cart (4).jpg 
Views:	339 
Size:	138.8 KB 
ID:	3629  

    Everlast PM256
    Millermatic 180
    Hypertherm PowerMax 65 with machine torch
    Longevity Force Cut 80I
    DIY CNC table for plasma/routing
    13" metal lathe
    Small Mill
    ect, ect.

  18. #38

    Default

    The ball valve method is much better choice. And never run the Argon through the trap. Also the 1/4 NTP connectors can corrode and even leak if tweaked a little (they wear over time), so I would avoid them.

    Also always turn off the tank when done. One leak can be $40-$80 the next day.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  19. #39

    Default

    Quote Originally Posted by mrprism View Post
    The way you have the argon flowing through the water trap it is possible to pick up moisture in that bowl. I've heard of other guys making a manifold with ball valves which will work fine. The way I have my 256 set up is the cats ### IMHO. I bought a Miniature Diverting 3-Port PVC Ball Valve from McMaster-Carr. Part number 4757K57 for the valve with 1/4" barbed fittings and part number 4757K58 for the valve with 3/8" barbed fittings. Get the size that matches your welders hose size. I'll take a picture of mine tomorrow and post. It literally takes as long as a torch change to go from welding to cutting WITH ZERO MOISTURE! I may make a video displaying how fast one can from one mode to the next with this setup.

    Alan
    Quote Originally Posted by everlastsupport View Post
    The ball valve method is much better choice. And never run the Argon through the trap. Also the 1/4 NTP connectors can corrode and even leak if tweaked a little (they wear over time), so I would avoid them.

    Also always turn off the tank when done. One leak can be $40-$80 the next day.
    Look at those pics again guys... no argon goes through the air regulator. The argon hose plugs straight into the welder. I get no moisture whatsoever, have no leaks and it works perfectly.
    For me this setup was the simplest and made the most sense. I maintain my air fittings just like the rest of my equipment.

    Click image for larger version. 

Name:	IMG_1155 - Copy.jpg 
Views:	422 
Size:	144.9 KB 
ID:	3630Click image for larger version. 

Name:	IMG_1156 - Copy.jpg 
Views:	409 
Size:	142.7 KB 
ID:	3631
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  20. Default

    Quote Originally Posted by zoama585 View Post
    Look at those pics again guys... no argon goes through the air regulator. The argon hose plugs straight into the welder.
    My mistake, I thought the argon was flowing through the trap for some reason. That looks like a good setup. Moisture would be almost non existent as only whats trapped in the small piece of hose would be an issue, and that sure would be very very minimal. As long as it does the job for you is all that counts.

    Alan

Similar Threads

  1. Pt250ex foot perception acting up.
    By srhprerunner in forum TIG Welding (GTAW/GTAW-P)
    Replies: 15
    Last Post: 04-21-2012, 05:07 AM
  2. pp256 tig help
    By jede76 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 24
    Last Post: 12-16-2011, 09:49 PM
  3. PT250EX - only getting HF arc
    By dgarnier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 10-08-2011, 10:40 AM
  4. Pp256
    By scorp765 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 05-19-2011, 12:20 AM
  5. TG AC pp256 need help.
    By Racecar in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 03-15-2011, 05:11 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •