    According to several tungsten manufactures, a diamond wheel is the only satisfactory implement to use to sharpen tungsten electrodes.
    If you get right down to it.
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

  2. #22

    Default

    There are a couple websites that sell inexpensive dremel type diamond wheels. I'll try to find the website again and post, but they had from 80 to like 320 grit diamond wheels.
    .
    Eide
    PowerTig 225 LX

  3. #23

    Default

    Alright, that didn't take as long as I thought it was going to

    http://www.widgetsupply.com/page/WS/...nd-coated-disk

    No affiliation, just a happy customer.

    Here's a dremel attachment that I designed for these bits, works pretty well:
    Click image for larger version. 

Name:	Hex Tungsten.jpg 
Views:	1002 
Size:	35.3 KB 
ID:	866
    .
    Eide
    PowerTig 225 LX

  4. #24

    Default

    Very Cool Eide! So what is the angle they are jigged to cut on the Tungsten? You wanna sell one? Either way, simple, basic, functional.

    Slick!
    PowerTig 225LX
    PowerCool W300
    PowerPlasma 60S
    Miller 140 MIG

  5. #25

    Default

    some GREAT ideas in this thread, this should be stickied!!
    300whp FWD 94 Celica
    PowerPro 205 with a hack behind the mask!

  6. #26

    Default

    i've seen ppl use alot of diffrent things for shaprening. i my self use the sanding method with a duel belt sander i picked up at lowes for 15$ no way im paying 300+ for a dedicated sharpener it's not like im doing life depending work
    Aaron

  7. #27

    Default

    I am just gonna guess the way I have always sharpened them is a big no-no after reading this thread... I just put it at like a 45degreeish angle in my bench grinder and spin it with my fingers, bad idea?
    Lincoln IdealArc 300/300 (Square one)
    Airco Dip/Stick 160

  8. #28

    Default

    Quote Originally Posted by n20civicb18 View Post
    I am just gonna guess the way I have always sharpened them is a big no-no after reading this thread... I just put it at like a 45degreeish angle in my bench grinder and spin it with my fingers, bad idea?
    I think most of us still do it that way, but the grinding stone should at least be dedicated to grinding only your tungstens.
    Gerald

    Millermatic 251
    Spectrum 300 Plasma
    Everlast PowerTig 250EX
    Everlast PowerCool W300
    Harris / Victor OA
    Craftsman 13 Speed Drill Press
    ProTools Air/Hydraulic Bender
    48" Brake, 72" Brake, 52" Stomp Shear
    Mitler Bros. 36" High Throat Bead Roller
    Compressor, Notchers, Grinders, etc.

  9. Default

    I bought my HF stuff for this today. I got a bonus Emery wheel also. I'll do a write up on my angle jig as it gets built.
    I am out trying to 'find myself'. If I should wander back while I am gone, please tell me to sit quietly and wait for myself to return.

    LOTS of scuba and vintage scuba equipment [I'm Always willing to trade or buy the stuff you think is too old to use]
    Smithy XLT Mill/lathe [It was easier to learn than I thought, I'm no pro, but I can make a bearing hanger]
    Everlast PP256

  10. #30

    Default

    Eddie, I am certai that people would be interested in these. What might you sell one for?
    When opportunity knocks, most do not recognize it, because it shows up wearing overalls and looking like work!!
    Joshua,Tacoma,Wa
    24'x48'shop-6/2010
    Hobart Handler125w/125cf 75/25-1998-Welds perfect
    Power tig250EX-w/300cf argon-2/2011-had 4053 problem, fxed and good as new
    Power Cool W300-4/2011-works great after making hoses
    Power Plasma 50-4/2011-in for repair
    Shop air

  11. Default

    Yesterday I went to Princess Auto and picked up a little "Jewelers/Jewelery drill" for $10. It has 4 collets that will accept .1mm up to 2mm.
    I think it's brilliant since I like cutting my tungsten down to 2''-3'' pieces and then grinding both ends. Having almost 30 pieces with both ends sharpened helps keep me in the welding groove when I don't have to get up and go sharpen a piece.

    I"ll post up some pics later.

  12. #32
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    I sharpen (and polish) mine on a lapidary wet diamond grinder that I already had since I grind stones for jewelry.
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  13. #33

    Default

    This is a cheap, but great way to save money. Having used high dollar sharpeners and using the cheaper way there is not much difference. For the everyday guy or gal this is a great method.

  14. #34

    Default

    This is very nice Eide! Are they for sale?

    Quote Originally Posted by eide View Post
    Alright, that didn't take as long as I thought it was going to

    http://www.widgetsupply.com/page/WS/...nd-coated-disk

    No affiliation, just a happy customer.

    Here's a dremel attachment that I designed for these bits, works pretty well:
    Click image for larger version. 

Name:	Hex Tungsten.jpg 
Views:	1002 
Size:	35.3 KB 
ID:	866
    James Swanson

    Millermatic 135
    (saving for a Power pro 256)
    Linde HDA200
    Custom water cooler and cart

  15. #35

    Default

    Quote Originally Posted by performance View Post
    Belt sanders are full of aluminum oxide...the very thing you are trying to avoid.
    The belt I use for sharpening is actually made from Silicon Carbide. Is it still a bad thing?
    James Swanson

    Millermatic 135
    (saving for a Power pro 256)
    Linde HDA200
    Custom water cooler and cart

Similar Threads

  1. $39 Harbor Freight tungsten sharpener
    By DaveBonds in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 14
    Last Post: 03-22-2014, 12:35 PM
  2. chemical tungsten sharpener
    By bubbas55 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 11-09-2012, 01:21 AM
  3. tungsten sharpener
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 34
    Last Post: 12-27-2011, 11:43 PM
  4. Plasma cutting 'table' on the cheap- way cheap.
    By qubit in forum Hobyist Projects
    Replies: 5
    Last Post: 10-24-2011, 04:10 PM
  5. DIY Tig Electrode sharpener
    By acourtjester in forum Other Custom Fabrications
    Replies: 4
    Last Post: 06-10-2011, 02:20 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •