 I Need Advise On Welding Aluminum With A Spool Gun
 I Need Advise On Welding Aluminum With A Spool Gun
		Last edited by zoama; 06-29-2014 at 05:02 PM.
Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
 
 
		Zoama
i just got mine working with a lot of help from Yofish the biggest thing form was that I had the tip out to far it is in now about 1/4" recessed or inside the face of the cup that made a big difference. The second was wire speed was to fast. I slowed the wire down it is at about 210 ipm. but all guns and machines are different I have the same gun as Yofish so it made it easer to get the settings closer.
My settings are on the MTS250S:
100% argon @ 25 CFM or 15 LPM
Wire speed at 210 IPM shown on the machine or #3 on the gun
Voltage that worked well for me was 20.0V to 20.5V
Wire size .047 Grade 4043
Mig (Wave Form Control) not Arc force set at 2
Aluminum was 6061T6 .132 thick and the flat piece was .188 thick.
Pics on (http://forums.everlastgenerators.com...ted-to-MTS250S) number 42 are the above settings.
Yofish or other aluminum Spoolgun welders will give you a better idea of the setting with your machine, I do have a i-Mig250 but I have not put my second 30A gun on it yet it needs to rewire.
Everlast PowerTig 325EXT (Canada)
Everlast Power I Mig 250 (Canada)
Everlast PowerPlasma 80S (Canada)
Everlast PowerCool W300 (Canada)
Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
Miller Dynasty 400 wireless(Canada)
Millermatic 252 plus 30A Spoolgun(Canada)
 New Member
					
					
						New Member
					
					
                                        
					
						
							
								 
							
						
					
					
						 
 
		My advice? Too much wire. Set arc force to zero. Rinse, repeat until spatter disappears.
EDIT: Also, it helps weld appearance to mechanically remove the mill surface with SS wire wheel or abrasives. Less stuff will 'bubble up'. Welding 5000 series plate with 5000 wire will produce smut, there is just no way around it. A more radical gun angle helps some as does a little more Ar. Blueshield also helps but who wants to pay for it?
Last edited by Yofish; 06-30-2014 at 04:03 PM.
 
 
		Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw
 New Member
					
					
						New Member
					
					
                                        
					
						
							
								 
							
						
					
					
						 
 
		Links to my welding projects > : Spray Arc with the 250p : Coldsaw Stand : Welding Cart : Heavy Duty Rolling Shelf : Taller Bandsaw
2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw