    These are mine. I only changed HF start duration (D02, was ~2.0) and DC start amps (D04, was ~30). Everything else is factory default.

    D01= N/A {00.5)
    D02= HF Arc start duration (.5-5 seconds) {5.0}
    D03= HF Arc start frequency (10-100Hz) {50}
    D04= HF Arc start amps DC (10-100 amps) {10}
    D05= HF Arc start amps AC (15-100 amps) {40}
    D06= N/A {1.5}
    D07= Lift start current DC and AC (10-100 amps) {15}
    D08= Torch trigger or amp control 4T function by type torch (00 = 4T 01 = 4T Normal) {00}
    D09= Voltage Reduction Device for MMA/stick (00 = VRD off 01 = VRD on) {00}
    D10= Pulse mode Standard or Advanced. AC is added to DC in Advanced mode (00 = Standard 01 = Advanced) {01}
    210EXT (2013 USA)

  2. #2

    Default

    It's times like this I'm happy that my machine only has a polarity switch and a knob to set max amps. Keep practicing and you won't need the machine's help to prevent craters.

  3. Default

    Quote Originally Posted by RichardH View Post
    These are mine. I only changed HF start duration (D02, was ~2.0) and DC start amps (D04, was ~30). Everything else is factory default.

    D01= N/A {00.5)
    D02= HF Arc start duration (.5-5 seconds) {5.0}
    D03= HF Arc start frequency (10-100Hz) {50}
    D04= HF Arc start amps DC (10-100 amps) {10}
    D05= HF Arc start amps AC (15-100 amps) {40}
    D06= N/A {1.5}
    D07= Lift start current DC and AC (10-100 amps) {15}
    D08= Torch trigger or amp control 4T function by type torch (00 = 4T 01 = 4T Normal) {00}
    D09= Voltage Reduction Device for MMA/stick (00 = VRD off 01 = VRD on) {00}
    D10= Pulse mode Standard or Advanced. AC is added to DC in Advanced mode (00 = Standard 01 = Advanced) {01}
    RichardH, Thank you for posting that for me.

Similar Threads

  1. 210ext
    By aclundwall in forum Pre-sales, Sales and Shipping questions
    Replies: 1
    Last Post: 02-17-2014, 05:15 AM
  2. new 210ext owner
    By weirtech in forum Introduce Yourself
    Replies: 9
    Last Post: 04-06-2013, 02:14 PM
  3. 210ext
    By piopio in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 02-12-2013, 08:48 PM
  4. More with the 210EXT
    By Rambozo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 10-03-2012, 08:44 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •