    Got my Power-i-Mig 250 test it out using standard setting of the MTS250S but tried the stitch weld see what it would do.
    Setting:
    Stitch Weld - Lowest
    Spot Weld - number 2 the first weld and number 3 second the weld
    Arc Force - 6
    Volts - 22.1
    Amps - 254

    Click image for larger version. 

Name:	First test on Power i Mig 250 S-6.jpg 
Views:	545 
Size:	139.5 KB 
ID:	11449Click image for larger version. 

Name:	Second  test on Power i Mig 250 S-6.jpg 
Views:	2801 
Size:	137.8 KB 
ID:	11450
    Last edited by Kempy; 12-20-2013 at 10:27 PM. Reason: ADD
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  2. Default

    Is this the iMig 250 or the iMig 250P? Spot weld on a filet?

  3. #3
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Quote Originally Posted by John71a View Post
    Is this the iMig 250 or the iMig 250P? Spot weld on a filet?
    iMig 250 with spot and stitch welding.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  4. #4

    Default

    I know this thread is old.
    Have you used/mastered these settings/functions in the last year? Do you have any new pics or any other insight on the iMig 250?

Similar Threads

  1. Power Pro 256 power on issue
    By wheelrdealer in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 02-27-2019, 02:47 AM
  2. Power Tig 250EX Power Cord Connections
    By Chris411968 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 01-31-2010, 06:58 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •