I have some excess 3/32 aluminum and steel filler rods and wanted to ask you gurus if any 'ol' shop trick exists that makes it easy to split a 3/32" thick filler rod in half so you get 2 ~0.046" thick rods? (Thereby, resulting in 2 thinner filler rods)?![]()
The filler rods that are thinner than 1/16 make it much easier for me to weld on thin walled tube, so just trying to make use of what I have..


							
						
 
				
				
				
					
  Reply With Quote


 Actually I'd take part in producing something like this just based on the fact I have no life and enjoy a challenge.
			