  1. Question Split 3/32" filler rod into two ~0.046" rods?

    I have some excess 3/32 aluminum and steel filler rods and wanted to ask you gurus if any 'ol' shop trick exists that makes it easy to split a 3/32" thick filler rod in half so you get 2 ~0.046" thick rods? (Thereby, resulting in 2 thinner filler rods)?

    The filler rods that are thinner than 1/16 make it much easier for me to weld on thin walled tube, so just trying to make use of what I have..
    Last edited by Welderooni; 07-27-2013 at 10:46 AM.

  2. #2
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    The easiest way might be to find a guy with MIG filler wire and trade him your 3/32" for it, then chuck the .023 into a drill and combine two lengths into .046. But by the time you find that guy, or figure out a reliable way to cut 3/32, a roll of .023 from the Home Deep/Lowes/LWS/Harbor Freight might look pretty good.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  3. #3

    Default

    Yeah, I don't think you are going to find a reliable way to split 3/32 filler.

    I'd keep the 3/32 on teh shelf for a larger project and go buy smaller rods or a roll of wire.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  4. #4
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    2 pounds of .023 from Welding City is $10, free shipping. Considering the ROTEI (return on time and effort invested) that may be the smarter move.

    http://www.weldingcity.com/filler-me...3-0.6mm-wires/
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  5. Default

    The situation is I have a lot of surplus 3/32 and the time, but not a lot of extra $ to spend. So, I don't mind building a rod splitter if it works well. How would you guys go about building a tool that perfectly splits a 3/32 rod in half?

  6. #6

    Default

    Quote Originally Posted by Welderooni View Post
    The situation is I have a lot of surplus 3/32 and the time, but not a lot of extra $ to spend. So, I don't mind building a rod splitter if it works well. How would you guys go about building a tool that perfectly splits a 3/32 rod in half?
    I just don't see it happening. Your best bet would be to purchase .040 or .045 mig wire in aluminum and steel.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. #7
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    I wonder if rolling it would be easier than ripping it. Even so, it would still be less of a PITA to just sell your 3/32 and buy what you need. Or find somebody to trade with.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  8. #8
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    OK, no cash but willingness to try, got it.

    Step 1: At least try posting on CL or welding web or somewhere: have 3/32, want to swap for 1/16th TIG wire or .045 MIG. Welderooni, what's your location? It's not in your signature.

    What about: pounding the 3/32 on a vise or anvil to flatten it out a bit, then get after it with a monster set of tin snips to cut it in half? My hands hurt enough as it is, can't imagine doing this myself. One concern to this idea if it's at all even possible would be inclusions or embedding extra junk in the process of hammering.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  9. #9
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    You would pull it through a drawing die to reduce the diameter and increase the length. That was how it was made in the first place. The aluminum won't be too hard, but the steel will take some serious force. Just not very practical to do, unless you already have, or have access to the setup for that.
    Long arc, short arc, heliarc and in-the-dark!

  10. #10

    Default

    There is a solution,,,it's called money,,,get some and buy the proper dia rod,,,splitting filler rod,,,thats the best laugh I have had in some time..
    i,m not sure what an hour of your time is worth...but one hour of mine will buy a lot of proper dia rod.
    Some of those lies people tell about me, are true

  11. #11

    Default

    I sometimes split mine about 1.5'
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  12. Default

    Maybe a long shot, but it's what I would try.

    Hang one end of the filler rod from an appropriate support.
    Attach weights onto the other end thereby stretching and slimming.

    If it works, let us know.

    rivets

  13. #13

    Default

    Quote Originally Posted by Rivets View Post
    Maybe a long shot, but it's what I would try.

    Hang one end of the filler rod from an appropriate support.
    Attach weights onto the other end thereby stretching and slimming.

    If it works, let us know.

    rivets
    That's an interesting idea. I suspect Murphy of law fame would step in, find a slight weak spot in the rod and stretch that point alone until that point broke ....

  14. Default

    Quote Originally Posted by Mr120 View Post
    That's an interesting idea. I suspect Murphy of law fame would step in, find a slight weak spot in the rod and stretch that point alone until that point broke ....
    Could very well be.

    But by then the filler rod might be slimmed down to acceptable dimensions.
    Albeit with two pointy ends.

    rivets

  15. #15
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    I don't see this happening even with a lot of engineering, talent, luck, and a little magic. The only thing that even came to mind when I first read this (besides a chuckle) was slip rolls, a power bead roller, or a press brake (all would smash the rod really flat....but what do you do with it then?). If you could rig a stretching arrangement using a drill motor to twist the wire while you pulled it tight, that may decrease the diameter a little, but there's no way you're getting 2 smaller pieces of rod from one larger diameter rod. I'm not even sure how much you'd shrink the diameter regardless of how hard you try.

    What about some sort of small tool that would allow you to pull and spin the rod through using a standard drill motor while a small tool bit shaved the diameter down? Sorry for encouraging this sort of thinking, but I have to admit that I have a few (stupid) crazy ideas myself....Like a completely wireless MIG welder that uses radio freq. for a signal? Not impressed? How about my weather machine that makes it rain ONLY at night time, say 3 or 4 nights a week so we'd never be short on water, but we'd never have to deal with rain ever again during the daytime! NO? The only other current project I'm working on is the goggles that allow you to see through (only attractive) women's clothing, regardless of how many layers they have on. Yeah, that last one's a dumb idea....I mean WHO would want goggles with that feature anyways?
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  16. #16
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by youngnstudly View Post
    Like a completely wireless MIG welder that uses radio freq. for a signal?
    Ala Tesla?


    Quote Originally Posted by youngnstudly View Post
    The only other current project I'm working on is the goggles that allow you to see through (only attractive) women's clothing, regardless of how many layers they have on. Yeah, that last one's a dumb idea....I mean WHO would want goggles with that feature anyways?
    I think those have already been invented, don't you remember the ads in the back of comic books for the x-ray vision goggles?
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  17. #17
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Quote Originally Posted by youngnstudly View Post
    I don't see this happening even with a lot of engineering, talent, luck, and a little magic.
    Agreed, we should stop talking about it. It's a government psychology test to see how far into the ground we'll drive it
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  18. #18
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Quote Originally Posted by redbeard View Post
    Ala Tesla?




    I think those have already been invented, don't you remember the ads in the back of comic books for the x-ray vision goggles?
    I think someone dropped the ball on actually bringing that idea to life! Either that or the irate mothers of the 1950's all wrote into the x-ray vision goggle factory and threatened a lawsuit if they didn't seize production! Times were simple then and ideas like this simply weren't excepted with wide open arms in those days. Plus my new updated version would allow you to only see through the attractive women's clothing. I call them the "No-Ugo Selective Vision Pretty Woman X-Ray Goggles"....SHHHHHH! Don't tell anyone!

    This is what I was kinda picturing in my head when I typed my last post, except the part being bored here would have the cutting bit revolving around the welding rod and the cutting bit in the video would be the cut down rod. Seems perfectly logical to produce this type of machine to save $10 on welding rod, right? Plus it would be portable! Who doesn't like portable equipment that serves such an important purpose? Actually I'd take part in producing something like this just based on the fact I have no life and enjoy a challenge.

    http://www.youtube.com/watch?v=BHhVzJw920M
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  19. #19

    Default

    Quote Originally Posted by youngnstudly View Post
    I think someone dropped the ball on actually bringing that idea to life! Either that or the irate mothers of the 1950's all wrote into the x-ray vision goggle factory and threatened a lawsuit if they didn't seize production! Times were simple then and ideas like this simply weren't excepted with wide open arms in those days. Plus my new updated version would allow you to only see through the attractive women's clothing. I call them the "No-Ugo Selective Vision Pretty Woman X-Ray Goggles"....SHHHHHH! Don't tell anyone!

    This is what I was kinda picturing in my head when I typed my last post, except the part being bored here would have the cutting bit revolving around the welding rod and the cutting bit in the video would be the cut down rod. Seems perfectly logical to produce this type of machine to save $10 on welding rod, right? Plus it would be portable! Who doesn't like portable equipment that serves such an important purpose? Actually I'd take part in producing something like this just based on the fact I have no life and enjoy a challenge.

    http://www.youtube.com/watch?v=BHhVzJw920M
    Add a portable forge so that you can take the shavings, melt them down and create one or more rods from those. Waste not want not.

  20. #20

    Default

    Find someone that is an experienced sword swallower AND has a gap between their front teeth.
    Have then swallow the rods, then hold their jaw shut, grab the end of the rod with vise grips and give it a pull.
    If it doesn't give you the proper size, look around for a different front tooth gap width and try again.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

Similar Threads

  1. Understanding "Arc Force" and how to set for different rods
    By aland in forum Stick Welding (SMAW)
    Replies: 20
    Last Post: 01-27-2018, 04:00 AM
  2. Replies: 11
    Last Post: 10-30-2012, 06:43 PM
  3. Alcotec 1/8" x 36" R4043 Filler Rod 10 Pound Boxes
    By cbmkr in forum Buy, Sale or Trade
    Replies: 0
    Last Post: 10-29-2012, 06:00 PM
  4. Replies: 2
    Last Post: 08-27-2012, 03:21 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •