Share
Results 1 to 15 of 15

Thread: air suppy ?

  1. Default air suppy ?

    whats the best way to plumb in the air dryer right after the fliter/reg thats on back of the powerultra205p
    iam thinking of hard plumbing from filter to air dryer and a ball valve on so i can use argon or air
    so filter valve then tee one side down to air inlet one side a valve from the gas
    someone posted a pic of theres a month back looked nice and clean he had both air and argon going though the dryer

  2. #2

    Default

    This is the way I did it on the 256 but the argon never goes through the dryer. The QC connects directly to the flowmeter line. Click image for larger version. 

Name:	IMG_1156 - Copy.jpg 
Views:	333 
Size:	142.7 KB 
ID:	10011Click image for larger version. 

Name:	IMG_1155 - Copy.jpg 
Views:	374 
Size:	144.9 KB 
ID:	10012
    I cut a cheap 10' 1/4" air hose to make this. It all works perfectly and never gave a problem.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    where does the drying go ? i might be missing it in pic

  4. Default

    Click image for larger version. 

Name:	air argon.jpg 
Views:	376 
Size:	124.7 KB 
ID:	10013
    is this a good idea ?

  5. #5

    Default

    Quote Originally Posted by travis View Post
    where does the drying go ? i might be missing it in pic
    I have a motor guard filter on my supply line. I suggest the M-60 kit or M100 kit since they come with 3 filters and side inlet/outlet http://www.automotivetoolsonline.com...it_p_9417.html
    Quote Originally Posted by travis View Post
    is this a good idea ?
    Looks ok to me but I prefer the quick couplings since there's no way to get it wrong. Whatever works and suits you will be fine.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #6

    Default

    Quote Originally Posted by travis View Post
    Click image for larger version. 

Name:	air argon.jpg 
Views:	376 
Size:	124.7 KB 
ID:	10013
    is this a good idea ?
    That looks fine. Filtering the gas will not hurt anything. Changing the filter might be a little work, gut all worth it. Moisture really does miss up the cuts and does no help welding either.

    Was there a reason you did not go with the ball valves? FYI, I had trouble with 1/4" NPT quick connects leaking years ago, and have it all clamped, I loose no gas that way, esp on the couple 150s I still have.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. Default

    that picture was taken off a post on the forum i will use ball vaulves
    would there be a best type of pipe to use or any to stay away from ....brass copper black pipe or gavlvinized ?

  8. #8
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by travis View Post
    that picture was taken off a post on the forum i will use ball vaulves
    would there be a best type of pipe to use or any to stay away from ....brass copper black pipe or gavlvinized ?
    Ok on the first two, stay away from the last two. Black pipe = rust, galvanized can shed zinc particles. You can also get a nice three way ball valve so you don't have worry about mixing things up.
    Long arc, short arc, heliarc and in-the-dark!

  9. #9

    Default

    Ideally, the added filter will come before the water trap/filter on the rear of the unit...not after.

  10. Default

    so air dryer then filter then inlet to plasma cutter ?

  11. #11

    Default

    Compressor, filter, trap, cutter. When you see water in the trap time for a new filter. Or get the ones that change from blue to pink, cheap, easy to use, disposable (or reusable).
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  12. #12

    Default

    I found a good source for three way ball valves, and the plastic one is compact, and rated to 125PSI. http://www.mcmaster.com/#three-way-ball-valves/=mmr3r2.

    Ordered one, and plan to plumb it in off the input port with one leg to a Argon Regulator, and the other through a dryer to the output of the regulator/separator. I have a couple of the smaller Motorguard disposables, and will just use barbs and clamps to avoid leaks.
    Last edited by zoama; 05-06-2013 at 01:36 PM. Reason: changed the link to the 3 way valve page
    Everlast PowerPro 256 (2013)
    Northern Hybrid 200 & ST80i
    HF 90Amp FluxCore (Don't laugh, it is what got me started)
    Lotos LT5000D Plasma
    HF 4x6 Horizontal Bandsaw
    Rikon 18" Bandsaw w/VFD
    Delta 14" Drill Press
    Robland NLX31 Euro Combo WW

  13. #13

    Default

    Quote Originally Posted by Big Paulie View Post
    I found a good source for three way ball valves, and the plastic one is compact, and rated to 125PSI. http://www.mcmaster.com/#three-way-ball-valves/=mmr3r2.

    Ordered one, and plan to plumb it in off the input port with one leg to a Argon Regulator, and the other through a dryer to the output of the regulator/separator. I have a couple of the smaller Motorguard disposables, and will just use barbs and clamps to avoid leaks.
    Here is the link to the McMaster site and specific parts (I went with the barbed version, to accomodate various tubing diameter subtle differences. I bought two, one for the Power Pro, to switch from compressed air for Plasma, to Argon for ITG, and one for my mig to switch ArCO2 over to pure Argon, for use with Aluminum TIG.

    http://www.mcmaster.com/#three-way-ball-valves/=mmsddd
    Everlast PowerPro 256 (2013)
    Northern Hybrid 200 & ST80i
    HF 90Amp FluxCore (Don't laugh, it is what got me started)
    Lotos LT5000D Plasma
    HF 4x6 Horizontal Bandsaw
    Rikon 18" Bandsaw w/VFD
    Delta 14" Drill Press
    Robland NLX31 Euro Combo WW

  14. #14

    Default

    Quote Originally Posted by everlastsupport View Post
    Compressor, filter, trap, cutter. When you see water in the trap time for a new filter. Or get the ones that change from blue to pink, cheap, easy to use, disposable (or reusable).
    Here's how I got mine setup: compressor, cheap oil/water separator with quick connects to also use on other air tools, motorguard filter, trap that came with cutter and pressure regulator then into cutter.
    If you are going to get a motorguard filter, get the M100 kit. It has 1/2" ports, where as the M60 has 1/4 or 3/8" ports.
    EverLast 140ST
    PowerPlasma 50
    No You Can't Use Them

  15. #15

    Default

    Quote Originally Posted by Gerry View Post
    Here's how I got mine setup: compressor, cheap oil/water separator with quick connects to also use on other air tools, motorguard filter, trap that came with cutter and pressure regulator then into cutter.
    If you are going to get a motorguard filter, get the M100 kit. It has 1/2" ports, where as the M60 has 1/4 or 3/8" ports.
    Yep, that's perfect. Or how I have mine and it works great, even do lite painting with it.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •