  1. Default 2013 PowerPro 205S

    I received my new 2013 PowerPro 205S today. I wish an online manual existed; the enclosed operating instructions leave a lot to be desired.

    I was elated that the TIG torch is not the hefty air-cooled WP-26. It is a model SR-26 with a 13-foot cable. It is a straight handle, like the Everlast WP26F15, except the neck is rigid.

    I am disappointed that the plasma torch is not a Trafimet S-45, as advertised and shown on the PP205 product page. It is a generic copy of a Trafimet, with no CE marking (European Conformity) and no model number, imprinted on the handle. I have to assume it's a 40-amp rated torch (the S-45 is rated at 40amp, 60% duty cycle; not 50amp) I discussed this with Oleg. Where's my Trafimet, Oleg??? Some Trafimet clones will not work with genuine Trafimet consumables. I have no idea if this one will.

    The dimensions are: 9.25 in wide, 22 in long, 17.25 in tall, These are the outside dimensions of black plastic, on ends of case. The power cord entrance and air inlet, including a 90-degree bend, add 1.5 inches. Sitting on the top of a Northern Tool (Metalman) welding cart, item # 16472, it exceeds the front edge by 2 inches, just barely resting on the edge.

    I tested the Trafimet-clone plasma torch at 20amps on 1mm thick sheet metal and it cut fine.

    I have not tested the TIG torch. I have a CKFL130 torch, with a Safe-Loc SL2-35G DINSE connector and it would not work! I could get it to insert all the way, but it would not turn to lock. I compared all the measurements of the Everlast DINSE connectors and, except for the CK connector being longer (which still inserted fully) the only difference was the keyway on the Safe-Loc was 1mm taller than the Everlast keyways. I ground off 1mm off the height of the Safe-Loc and it worked; problem solved. I don't know if this was a machining error on CK's part, but the connector would not work in either the positive or negative inputs.

    The unit came with a molded NEMA 6-50P connector, with a 7'8" cord. That's good, if you have your welder that close to your power outlet, but bad if you need a longer cord.

    That's all for now; hope this helps!
    Last edited by bluetec; 03-08-2013 at 01:08 AM.

  2. #2

    Default

    bluetec


    New manual for PP205S and PP256S will be uploaded later today ! Our s45 working just fine with genuine Trafimet consumables.
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  3. #3

    Default

    I believe this torch that you have with the current unit is actually heavier built internally. I have had them apart and compared. The S-45 that is sent out is heavier built and will handle the amperage better. And we have tested this company's cons and they actually outlast the trafimet...

  4. Default

    Thank you, Oleg and Mark, for the quick reply and information. The online manual is thorough and complete, but does not cover replacement of the power cord. I would like to replace the supplied cord with a 15-foot, 2-guage, 2-wire/with ground, welding cord, with a NEMA 6-50P connector. Is this possible, with the wire connections, inside the unit?

  5. #5

    Default

    Quote Originally Posted by bluetec View Post
    Thank you, Oleg and Mark, for the quick reply and information. The online manual is thorough and complete, but does not cover replacement of the power cord. I would like to replace the supplied cord with a 15-foot, 2-guage, 2-wire/with ground, welding cord, with a NEMA 6-50P connector. Is this possible, with the wire connections, inside the unit?
    That's intentional. Do not replace the cord. You can add an extension, properly sized of course, but the wire diameter and size is designed for the powe switch terminals and the input current. We will not warranty any damage caused by monkeying around with the cord and plug. We've had people try to replace the cord for a "heavier" wire to suit their electrician's demands (uninformed about the NEC) because they thought a heavier wire should be on it, and have broken things in the process. We've gone through the trouble of having adding a plug for the customer so this wouldn't be an issue.

  6. Default compressor size

    Quote Originally Posted by performance View Post
    That's intentional. Do not replace the cord. You can add an extension, properly sized of course, but the wire diameter and size is designed for the powe switch terminals and the input current. We will not warranty any damage caused by monkeying around with the cord and plug. We've had people try to replace the cord for a "heavier" wire to suit their electrician's demands (uninformed about the NEC) because they thought a heavier wire should be on it, and have broken things in the process. We've gone through the trouble of having adding a plug for the customer so this wouldn't be an issue.
    Hello, what size compressor do you need for the 205S plasma cutter? Thank You.

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by fitter View Post
    Hello, what size compressor do you need for the 205S plasma cutter? Thank You.
    Since that is a 50A I would say you can use the spec for the PP50 since it's not in the PP205S manual.
    3.5-4 cfm minimum @ 90 psi with a 30-60 gallon reserve. And of course make sure you have a good air dryer installed.
    Rule of thumb is if while using, you see your tank pressure fall below the cut-in point, you need more air. The actual size also depends on what other air consumers you are using, too.
    Long arc, short arc, heliarc and in-the-dark!

  8. #8

    Default

    Spec should be 5 cfm for regular operation.

  9. #9
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by performance View Post
    Spec should be 5 cfm for regular operation.
    Time to update the new manual.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. my PowerPro 256S (2013)
    By halojumper in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 23
    Last Post: 02-27-2015, 11:24 PM
  2. Powerpro 205s HF start does not work
    By 2005sxt24 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 12-31-2014, 01:32 PM
  3. 2013 Summer Time Contest. June 21- October 1 2013
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 54
    Last Post: 04-12-2014, 02:42 AM
  4. new powerpro 205s plasma torch connection
    By ricks69l78 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 08-18-2013, 07:59 PM
  5. Thanks Oleg, for the 2013 PowerPro 256s
    By Big Paulie in forum Customer Testimonials
    Replies: 5
    Last Post: 04-30-2013, 10:50 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •