Share
Results 1 to 8 of 8

Thread: NOOB Tig Welder in need of questions answered

  1. Default NOOB Tig Welder in need of questions answered

    hello guys im very new to tig welding but have done alot of other kinda of welding. ive been welding/fabbing for about 2-3 years on my own stuff and other peoples stuff.

    Ok so i ordered my power pro 205 tig and just got it hooked up lastnight (had to install new box in garage) and im using what came with the setup very small #4 cup and i only have rare earth 3/32 so i know this isnt the best combo but im waiting on my bigger cuts to come in sooo anyways i started on mild steel 1/8th inch thick seemed to weld pretty good so went to stainless 1/4 flange i had laying around welded ok need bigger lens for better coverage then went to aluminum. heres my deal i watched a vid from weldingtipsandtricks.com on setting up so he has his leads hooked up torch hooked to - and ground hooked to + and hes welding aluminum and steel hooked this way mine wont weld aluminum this way it will just eat tungstens i have to switch the leads around to get it to weld is this normal??? jody was saying going from steel to aluminum all he had to change was dc to ac and make sure the hz and balance are set right then weld away.

    Sorry guys my forum writing sucks ive been told its hard to read cuz i put it all together.

    thanks Eric

  2. #2

    Default

    You just flip the switch for ac on your machine... no need to swap leads.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3

    Default

    Yep switch to AC for aluminum and make sure your balance is around 20-30 if the material is clean. To much balance will destroy electrodes quickly. Depending on what weld joint, adjust the AC frequency accordingly. For a flat butt joint my frequency is around 70-100
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  4. #4
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Welcome to the forum, Eric! If you don't mind me asking, what's your location?

    Just curious- when you went from stainless to aluminum, did you alter settings and switches on your control panel *and* swap the leads?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  5. Default

    im in iowa

    Ya i went from dc to ac the problem was i had the balance set to 65% and i went down to 30 now and it works great now thanks guys

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    The Everlast balance control is backwards from Miller, so if you see Miller settings, just use the opposite. Switching leads has the same effect as that for AC, as you figured out.
    Long arc, short arc, heliarc and in-the-dark!

  7. #7

    Default

    Doesn't Miller actually use settings that technically do not make sense in terms of the balance?
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

  8. #8
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by zedron View Post
    Doesn't Miller actually use settings that technically do not make sense in terms of the balance?
    Not really, both companies do a percentage adjustment, but one is % positive and one is % negative. It's AC so it's just a coin toss on which one you use. You can use positive and call it cleaning or negative and call it penetration. The old Syncrowaves used to have a knob that went from max cleaning to max penetration. It was just numbered 1-10 and wasn't a true percentage because the balanced position was number 3. The actual percent is a much better way, and either pos or neg just a function of brand preference.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. tig noob in need of some help
    By steve1989 in forum General Welding Questions
    Replies: 10
    Last Post: 12-31-2013, 02:15 AM
  2. Noob in need of help
    By Chuck_jkl in forum Introduce Yourself
    Replies: 10
    Last Post: 01-24-2013, 02:17 AM
  3. Mig Welder Questions
    By SeanMurphy265 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 0
    Last Post: 05-26-2011, 01:18 PM
  4. Welder spec questions
    By sportbike in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 03-05-2011, 02:53 AM
  5. Welder poec questions
    By sportbike in forum TIG Welding (GTAW/GTAW-P)
    Replies: 0
    Last Post: 03-03-2011, 04:08 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •