    Default Confessions of a TIG Noob

    The universe smiled on me at the last Everlast contest, and holy cow I won- who'da thunk it. I always enter this kind of thing totally expecting to never win, but here I am the proud owner of a 210 EXT. I'm mortified to admit it took me til today to just bloody make the time to weld with it. I should preface this by saying I've never even *held* a TIG torch before today, as the photo will show, but let me tell you I am completely jazzed. Can't get over it- the machine is just amazing. I'm totally psyched with this machine and the possibilities it is opening up. Thanks again, Everlast!

    If you're thinking about a TIG machine but on the fence or intimidated by it, give it a go!

    I realize these welds are nothing to write home about (but I may anyway). Mild steel, 2% lanthanated 3/32" tungsten, about 110 amps (I was experimenting), 7 LPM argon.

    Click image for larger version. 

Name:	DSCF0453.jpg 
Views:	349 
Size:	145.9 KB 
ID:	8618
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Congrats, and welcome to the world of TIG. Doesn't look bad for a first go. One thing, TIG is not tolerant of rust, mill scale, dirt, etc. like MIG and stick, so grind your metal clean and things will go a lot better for you.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Good start... clean the mill scale off before tig welding. Time to update your sig with the new machine.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    @Now@ I understand about mill scale and how clean surfaces must be. I got after it with a cup brush but clearly that wasn't enough, and explains why the edges of the puddle were sparkling.

    Stoked for TIG, now, and very in touch with Undercut's "break it so i can weld it back together" tagline!
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  5. #5

    Default

    Just keep on practicing on mild steel you will get more comfortable at mild steel and then try some stainless its real close to welding mild steel. Aluminum will be a lot of fun and with the different settings on the 210EXT and low amps on AC it opens up a lot of Aluminum welding applications.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  6. #6
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Will do, definitely, Monday I'm off to visit scrap yards to find practice pieces. The steel supplier closest to me lets their drops go for cheap but they're a drive to get to.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  7. #7

    Default

    Drops will be easier to clean up in most cases and give nice straight line for the butts and all. Has a little more cost, but better to start out with. And a stainless steel brush with a BIG A on it.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  8. #8
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    True, and I'll be more likely to find a large-ish plate for a welding table surface. In my mind's eye I envision finding the perfect piece of clean plate for a welding table at a scrap yard, which realisitically falls into the "Yeah, right, like that'll ever happen" category of expectations.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  9. #9

    Default

    I still have the very first piece of material I TIG welded. I figured it would be a nice keepsake one day when I get older and it really is. I have it easily view able in the garage where I can see it all the time. My first TIG experience was on 3/16 aluminium plate and most of my general "practice" was on some assortment of aluminium.
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

  10. #10

    Default

    Quote Originally Posted by DaveO View Post
    Will do, definitely, Monday I'm off to visit scrap yards to find practice pieces. The steel supplier closest to me lets their drops go for cheap but they're a drive to get to.
    I went to a local fab shop and told them I'm teaching myself to tig weld and would like to buy some scrap to practice on. The guy took me to a plastic barrel full of scrap aluminum and gave me all I wanted for free. I've been back two more times since and they tell me to take what I want every time.
    This is some of what I have left. Click image for larger version. 

Name:	IMG_1238.jpg 
Views:	323 
Size:	150.4 KB 
ID:	8629
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  11. #11
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    That's very generous of them. There's not a lot of fab shops in my immediate area, I'll have to look in the right places, I guess see if I can make that kind of connection. Do you ever bring them a box of Krispy Kremes, or something?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  12. #12

    Default

    Quote Originally Posted by DaveO View Post
    That's very generous of them. There's not a lot of fab shops in my immediate area, I'll have to look in the right places, I guess see if I can make that kind of connection. Do you ever bring them a box of Krispy Kremes, or something?
    I just happened to stop in there one day a few years back needing a piece of aluminum to make a computer case panel from. The guy got the piece I needed, sheared it to size and said the price was $4, I gave him $10. I went back a couple more times over the next two years to buy similar pieces and the guy would give me a low price every time... then we started the scrap aluminum thing. They're just nice people.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. tig noob in need of some help
    By steve1989 in forum General Welding Questions
    Replies: 10
    Last Post: 12-31-2013, 01:15 AM
  2. Noob in need of help
    By Chuck_jkl in forum Introduce Yourself
    Replies: 10
    Last Post: 01-24-2013, 01:17 AM
  3. noob
    By bubbas55 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 11-08-2012, 12:23 AM
  4. Noob to Tig
    By Ram48 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 04-06-2011, 03:46 AM
  5. Noob from CT
    By Bikenstitchz in forum Introduce Yourself
    Replies: 3
    Last Post: 03-26-2011, 02:13 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •