    Here are some bollards I made for this job I finished last Thursday. These bollards are made from 6" schedule 40 pipe, and welded onto a 1/2" 8"x8" plate with 4 5/8" holes. They were anchored inside protecting a cooler and a piece of electrical equipment. I welded these with my power arc 140st.








    They were painted safety yellow, and had covers placed over them.

    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  2. #2

    Default

    These were outside bollards made from 6" schedule 40 pipe. They are 7' long and 3' deep in concrete. The 7' of pipe is also filled with concrete. I hate concrete, and now I hate concrete even more!



    This is a lift so they can unload their trucks.




    These were also painted safety yellow. The parking lot is on a slope, and that's what is making the bollards look bad. The bollards are level, but they would look better if they leaned with the lift.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  3. #3
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Are the tops just open with concrete in them or are you going to cap them? I ask because I'm curious if welding caps on a concrete filled pipe has the same issues as welding a cylinder shut, pressure and whatnot.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  4. Default

    Quote Originally Posted by Trip59 View Post
    Are the tops just open with concrete in them or are you going to cap them? I ask because I'm curious if welding caps on a concrete filled pipe has the same issues as welding a cylinder shut, pressure and whatnot.
    i see a couple of cans of spray in the background. you would get better coverage using rustoleum safety yellow and a brush or roller. i wouldn't even prime them unless they had to be delivered primed and then painted by others.

    filling the tubes with concrete is a pain, i agree. if you are going to do more of this type of work be aware of the notation CFT on prints involving structures made of steel tube, sq or round. it is a common procedure these days. CFT = concrete filled tube.

    not picking on your stuff guy, it's just that you are one of the few doing real work.

    just a suggestion good luck.
    Last edited by fdcmiami; 10-15-2012 at 09:27 PM.

  5. #5
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    What kind of paint is Rustoleum safety now, still a real enamel or some new formulation? We used to use that stuff by the gallon on lifts and shop areas when I was a pro wrench, always brushed it right on degreased steel, worked great, covered good and was tough as hell once you let it fully cure.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  6. Default

    don't want to hijack this thread. here's a link to the rusto.

    http://www.rustoleum.com/CBGProduct.asp?pid=130

    i don't think there's anything better off of the shelf. spray, brush or roll.

    i am suprised that the two bollards that went into the ground were not painted beforehand. also, regarding the concrete in the tube, since you can have shrinkage it is a good idea to come back and check and possibly throw some quick setting something or other in there to make the top of the tube proud if you are not going to cap it. i see this all the time with rail installers and quickset. they don't come back and deal with the shrinkage, water collects and before long if your posts are steel they rust out from sitting water.

  7. #7

    Default

    How did you cut the two caps (freehand/CNC/Plasma/O/A)? Not sure why but we always paint them red.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  8. #8
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    If you want a super smooth finish, give this stuff a try. It will make a rough casting look polished. I've painted a number of machines and equipment with it, and I don't think there is any solvent that attacks it, once cured and it's tough on impacts and abrasion, too.

    http://www.prattandlambert.com/produ...d_mastic_epoxy
    Long arc, short arc, heliarc and in-the-dark!

  9. #9

    Default

    Sounds like POR-15 Stuff is great, OK colors. The silver is a pain in the tail, it gets black streaks in it unless you stir and spray fast..

    Pratt&Lambert something you can pickup local?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  10. #10

    Default

    The pipes are full of concrete, I had to add a little more concrete to round off the tops. The inside ones have weld on caps, but also have the nice plastic covers.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  11. #11

    Default

    Quote Originally Posted by fdcmiami View Post
    don't want to hijack this thread. here's a link to the rusto.

    http://www.rustoleum.com/CBGProduct.asp?pid=130

    i don't think there's anything better off of the shelf. spray, brush or roll.

    i am suprised that the two bollards that went into the ground were not painted beforehand. also, regarding the concrete in the tube, since you can have shrinkage it is a good idea to come back and check and possibly throw some quick setting something or other in there to make the top of the tube proud if you are not going to cap it. i see this all the time with rail installers and quickset. they don't come back and deal with the shrinkage, water collects and before long if your posts are steel they rust out from sitting water.
    That is the paint that I used to finish out the bollards. I sprayed it with a paint gun. The paint mixes with acetone and sprays very good, especially for someone who is not a good painter.

    The pipes could not be pre-painted. They wanted them set in the concrete and then painted. It was done according to their specifications not mine. I would have at least put a good coat of primer before setting them in concrete. I guess they felt that it did not matter since the inside of the pipe was filled with concrete.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  12. #12

    Default

    Quote Originally Posted by everlastsupport View Post
    How did you cut the two caps (freehand/CNC/Plasma/O/A)? Not sure why but we always paint them red.
    They had to have a dome cap on top. They told me that after I thought I had finished them!
    http://www.kingmetals.com/Catalog/It...temNumber=6136
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  13. #13
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    ...They told me that after I thought I had finished them!...
    Sounds like this job had a lot of that.
    Long arc, short arc, heliarc and in-the-dark!

  14. #14

    Default

    I built this door frame from 8" channel from the local steel supply.


    I should have built it from this stuff... It was a learning experience...
    http://www.primebldg.com/product/channel-iron/
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  15. Default

    Quote Originally Posted by Rambozo View Post
    If you want a super smooth finish, give this stuff a try. It will make a rough casting look polished. I've painted a number of machines and equipment with it, and I don't think there is any solvent that attacks it, once cured and it's tough on impacts and abrasion, too.

    http://www.prattandlambert.com/produ...d_mastic_epoxy
    I'm going to have to try that.

Similar Threads

  1. seanmurphy265 Project 3 Almost Summer contest - Condenser Rack
    By SeanMurphy265 in forum Heavy Equipment and Commercial Projects
    Replies: 19
    Last Post: 10-10-2012, 03:55 AM
  2. SeanMurphy265 Project 2 Almost Summer Contest - Tube Bender
    By SeanMurphy265 in forum Other Custom Fabrications
    Replies: 5
    Last Post: 08-24-2012, 05:05 PM
  3. SeanMurphy265 Project #4 Smoker!
    By SeanMurphy265 in forum Other Custom Fabrications
    Replies: 68
    Last Post: 01-23-2012, 12:16 PM
  4. Project#3 SeanMurphy265 Latch repair
    By SeanMurphy265 in forum Welding Repairs
    Replies: 2
    Last Post: 07-14-2011, 02:26 AM
  5. Project 2 SeanMurphy265, Welding Cart do-over
    By SeanMurphy265 in forum Hobyist Projects
    Replies: 6
    Last Post: 06-18-2011, 08:28 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •