    New to the forum and relatively new to welding too. As a mechanical engineer, I know a bunch about specing welds and weld metallurgy and all that theory, but have only laid a few actual welds. Now I find it time to expand my hobbies into welding and am looking for a machine. Everlast jumps out as a great inexpensive option without being cheap - also, I work around the corner from the Canadian office. To that end, I need help identifying the best starter welder. Mostly I'll be welding thin to thick wall tube, some sheet, some plate. Mostly steel, some stainless.

    What I know I want: TIG and stick
    What I know I can't afford yet: AC TIG
    What I don't want: MIG, plasma cutting

    That still leaves the field wide open. My research tells me that small machines have their place, but are difficult to learn on. Big machines are expensive. Looking at the product line-up, the Power I-TIG 200 looks great, right near the middle of the smaller machines. What is the general opinion? Is this too much machine and I should look at the 140ST or the 160STH? Is it a bit weak and I should look at the PU205P (and get plasma as a bonus)? What about the SU205 - is mosfet technology an issue?

    Ideally I'd get the 200DX or PP205 but the wallet can't handle that right now...

    Best regards, ABUGGELN
    PowerArc 160STH

    "Life is tough pilgrim, it is even tougher if you're stupid” ― John Wayne

  2. #2
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Well hello there! Welcome to the forum. From what I've read, all of those products are great but they do fill different areas of the market. Will you be welding using a 220V circuit?

    I'm not sure if there is such a thing as "too much machine". LOL

    What is the thickest material do you think you will stick weld? How about with TIG?

    There are some really good people on this forum. A lot of good knowledge and helpful advice. Hope you enjoy your stay.

    Cheers!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  3. #3

    Default

    Quote Originally Posted by abuggeln View Post
    New to the forum and relatively new to welding too. As a mechanical engineer, I know a bunch about specing welds and weld metallurgy and all that theory, but have only laid a few actual welds. Now I find it time to expand my hobbies into welding and am looking for a machine. Everlast jumps out as a great inexpensive option without being cheap - also, I work around the corner from the Canadian office. To that end, I need help identifying the best starter welder. Mostly I'll be welding thin to thick wall tube, some sheet, some plate. Mostly steel, some stainless.

    What I know I want: TIG and stick
    What I know I can't afford yet: AC TIG
    What I don't want: MIG, plasma cutting

    That still leaves the field wide open. My research tells me that small machines have their place, but are difficult to learn on. Big machines are expensive. Looking at the product line-up, the Power I-TIG 200 looks great, right near the middle of the smaller machines. What is the general opinion? Is this too much machine and I should look at the 140ST or the 160STH? Is it a bit weak and I should look at the PU205P (and get plasma as a bonus)? What about the SU205 - is mosfet technology an issue?

    Ideally I'd get the 200DX or PP205 but the wallet can't handle that right now...

    Best regards, ABUGGELN
    Welcome to our little forum ... as far as machine selection goes ... I recommend you do as I did ... I pondered it for a while and decided that settling for less than I needed was not an option so I skipped the lattes and donuts and did a few odd jobs for "extra money" if there is such a thing ... for a half a year and got the Powertig 200DX ... AWESOME machine! You will not be disappointed!
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  4. Default

    Quote Originally Posted by Winky View Post
    Welcome to our little forum ... as far as machine selection goes ... I recommend you do as I did ... I pondered it for a while and decided that settling for less than I needed was not an option so I skipped the lattes and donuts and did a few odd jobs for "extra money" if there is such a thing ... for a half a year and got the Powertig 200DX ... AWESOME machine! You will not be disappointed!
    Welcome Neighbour
    You have a big advantage if you are local to the Main Office here in Burlington. This will allow you to narrow down your choices and give them a workout before deciding what is best for your needs.
    The PA 160STH is as good as it gets regardless of what make you compare it to and what i like about it is the ability to go above the magic number of 90 amps (most common setting worlwide ) while running on 110v . The smoothness of the Arc is really something else and dropping from 5 amps up to 160 will cover most situations from razor blades to 1/4",
    and this level of performance is just not found in anything even remotely close to this price range.
    I think you can tell i really like the 160sth
    the 140 St is a really cute little thing and it is great for around the house and the price is a great selling point , but it does not compare in TIG mode to the 160sth ( if the truth be known there are not many out there that do compare to this model )
    Both of these have the ability to perform on 110v and 240v.
    You mentioned the 200DX as a possibility. This is my all time favourite model in AC /DC Tig
    Cheers
    Duncan
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  5. #5
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Titan winch View Post
    ... You have a big advantage if you are local to the Main Office here in Burlington. This will allow you to narrow down your choices and give them a workout before deciding what is best for your needs. ...
    You have a HUGE advantage. Definitely take this opportunity! Good luck in making a decision on which one to buy.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  6. #6

    Default

    Thanks all for the responses! A bit more on my plans:
    I have 220 in the garage (but an unit capable of 110 would make it portable). For Stick, making jigs, trailer augmentation, general repair and assembly - nothing over 1/4". For tig, I would think that 1/8" would be my limit.

    I like your approach Winky! The DX200 is the machine I want, but I really need to learn and practice basics (and I learn slow!). Based on Titan Winch recommendation - I'm now really leaning toward the 160STH, with the opportunity to look at some of the others as well. In a few years (remember - slow learner) I'll know much more about what I really want to be able to do and can then get the proper machine and still have a portable unit.

    (After I posted my first message, I realized the introduction board isn't the best place for these questions - Sorry!)
    PowerArc 160STH

    "Life is tough pilgrim, it is even tougher if you're stupid” ― John Wayne

  7. #7

    Default

    Quote Originally Posted by abuggeln View Post
    Based on Titan Winch recommendation - I'm now really leaning toward the 160STH, with the opportunity to look at some of the others as well. In a few years (remember - slow learner) I'll know much more about what I really want to be able to do and can then get the proper machine and still have a portable unit.
    One thing I have learned is one machine/tool does not do everything really well. Different tools for different jobs. I told a buddy I wanted a TIG welder and he said for me to sell him my MIG welder... No that is staying... One won't replace the other. Welding is a big field and the more I learn, the more I realize I have to learn.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  8. #8

    Default

    ...and now I've flipped again. I really like the idea of being able to learn about the various TIG functionality the is present in the I-TIG 200, and not in the PowerARCs.
    PowerArc 160STH

    "Life is tough pilgrim, it is even tougher if you're stupid” ― John Wayne

  9. #9
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by abuggeln View Post
    ...and now I've flipped again. I really like the idea of being able to learn about the various TIG functionality the is present in the I-TIG 200, and not in the PowerARCs.
    Flippin' is OK. You haven't committed anything. The more you learn about the possibilities, the more you may find your needs changing. TIG was a very low priority for me when I was looking but then I began to think that I might get into more detailed welding. Don't forget to go to the Everlast office and look around.

    Quote Originally Posted by Brian Ski View Post
    One thing I have learned is one machine/tool does not do everything really well. Different tools for different jobs. I told a buddy I wanted a TIG welder and he said for me to sell him my MIG welder... No that is staying... One won't replace the other. Welding is a big field and the more I learn, the more I realize I have to learn.
    IMHO you did the right thing, Brian. I see TIG as being a really good complement to stick and / or MIG, not really as a replacement. I think you would have really missed having a MIG machine. Cheers.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  10. #10

    Default

    Quote Originally Posted by undercut View Post
    IMHO you did the right thing, Brian. I see TIG as being a really good complement to stick and / or MIG, not really as a replacement. I think you would have really missed having a MIG machine. Cheers.
    On the other hand I haven't fired up the ole buzz box stick welder in maybe a decade. I don't do a lot of welding but the MIG takes care of about all of it so far. At least until I got to Aluminum. I think it is a 185 amp and it has done everything I have thrown at it.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  11. #11
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by abuggeln View Post
    ...and now I've flipped again. I really like the idea of being able to learn about the various TIG functionality the is present in the I-TIG 200, and not in the PowerARCs.
    Remember, even a very basic machine can produce great TIG welds, all the way down to something like the PowerArc 140 or 160. All the bells and whistles in the world are no substitute for lots of practice.

    Long arc, short arc, heliarc and in-the-dark!

  12. #12

    Default

    Well my friend which ever way you go I'm sure you will be satified with the quality of thr Everlast products. Rambozo is right ... it's all about practice and not getting discouraged ... take your time ... get comfortable strike an arc and go.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  13. #13

    Default

    Get you a Power Arc 160 and when you get the hang of it jump up and purchase the largest AC/DC tig welder you can afford! You will still use that 160 regardless because of the size. I use my 140st all the time even though I have larger welders
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  14. #14

    Default

    As a starter machine, for practice, would the PA140ST be suitable instead of the 160STH? The main differences is no HF start and (of course) the lower amperage. If I take the approach of getting an inexpensive machine now to practice with and when I have enough experience and dollars, I can make a much more informed choice. This is sounding great.
    PowerArc 160STH

    "Life is tough pilgrim, it is even tougher if you're stupid” ― John Wayne

  15. #15
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by abuggeln View Post
    As a starter machine, for practice, would the PA140ST be suitable instead of the 160STH? The main differences is no HF start and (of course) the lower amperage. If I take the approach of getting an inexpensive machine now to practice with and when I have enough experience and dollars, I can make a much more informed choice. This is sounding great.
    160sth supports a pedal and has a gas solenoid to turn the gas on and off automatically when you weld. If you are mainly stick'ing the 140 will save you some money as you establish your needs. It's a tad smaller and lighter too. If you want to get serious about TIG, I would personally save up a bit more and go for the 160sth for the pedal support and the gas solenoid.

    Both should be great machines so I can see how tough the decision can be!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  16. #16

    Default

    So I got the 160STH.
    I went to check out the machines in person (nice to have the Canadian head office down the road!) on Thursday. We spent a lot of time discussing the options, pro, cons and possible upgrade paths. Excellent help!
    I went back on Friday to pick up the 160STH. Now to spark it up and see what I can do.

    Very exciting!
    PowerArc 160STH

    "Life is tough pilgrim, it is even tougher if you're stupid” ― John Wayne

  17. #17
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by abuggeln View Post
    So I got the 160STH.
    I went to check out the machines in person (nice to have the Canadian head office down the road!) on Thursday. We spent a lot of time discussing the options, pro, cons and possible upgrade paths. Excellent help!
    I went back on Friday to pick up the 160STH. Now to spark it up and see what I can do.

    Very exciting!
    Cool! Good for you! Now the fun stuff begins.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  18. #18

    Default

    Quote Originally Posted by abuggeln View Post
    So I got the 160STH.
    I went to check out the machines in person (nice to have the Canadian head office down the road!) on Thursday. We spent a lot of time discussing the options, pro, cons and possible upgrade paths. Excellent help!
    I went back on Friday to pick up the 160STH. Now to spark it up and see what I can do.

    Very exciting!
    If aluminum is not on your list, the 160STH is quite the complete and compact package. I use one myself, great machine. Did you meet up with Duncan and Jean?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  19. #19

    Default

    Quote Originally Posted by everlastsupport View Post
    Did you meet up with Duncan and Jean?
    In my excitement I've forgotten! - How embarrassing! What do they look like?

    Over the weekend I fired it up and started figuring things out. Perhaps not the best first project, but I have an old cast steel anvil that was previously badly gouged by a torch so I set to filling it. Went pretty well - some porosity but way better then it was!

    No tank yet so I can't try tig.
    PowerArc 160STH

    "Life is tough pilgrim, it is even tougher if you're stupid” ― John Wayne

  20. #20
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by abuggeln View Post
    In my excitement I've forgotten! - How embarrassing! What do they look like?
    I believe the following is Duncan

    Click image for larger version. 

Name:	IMG_0765.jpg 
Views:	822 
Size:	133.3 KB 
ID:	7419

    http://www.youtube.com/watch?v=ta4pN...hannel&list=UL

    Have a lot of fun with your new welder!
    Last edited by undercut; 07-23-2012 at 06:29 PM.
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

Similar Threads

  1. Hello from Oro Ontario!
    By Brent H in forum Introduce Yourself
    Replies: 0
    Last Post: 03-12-2018, 01:20 PM
  2. Robert from Ontario
    By wgnracer in forum Introduce Yourself
    Replies: 8
    Last Post: 03-03-2014, 12:34 PM
  3. Hello from Brampton Ontario
    By Dwight in forum Introduce Yourself
    Replies: 3
    Last Post: 10-14-2012, 03:52 PM
  4. Hello from SW Ontario
    By Farmer in forum Introduce Yourself
    Replies: 3
    Last Post: 07-26-2010, 05:23 AM
  5. Hello from Ontario
    By agrrob in forum Introduce Yourself
    Replies: 0
    Last Post: 04-28-2010, 02:17 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •