Quote Originally Posted by performance View Post
One issue with with square nuts is that they are generally softer than even a grade 5 and have a grade 2 rating. Even though welding a nut removes some of the strength, it doesn't completely destroy the quality, and hardened nuts are welded all the time in the industry for this type application...Unless you can verify the hardness of the square nut, I wouldn't use it for welding.
My local bolt store has them in both grade 2 and grade 5, but not grade 8. However, I can get flange nuts in grade 8 if needed. It all depends on the application and the size as to what kind of fasteners you select. For some jobs 1/4"-20 grade 2 is fine, for other 4"-4 grade 8 is not enough!