Looks really cold. I would bump up amperage next time.
Try using 1/16th for a root pass, then use the 3/32 for your cover pass, remembering to cool down with an air blower. Stainless doesn't like a lot of heat.
Hope this helps
Frank
Looks really cold. I would bump up amperage next time.
Try using 1/16th for a root pass, then use the 3/32 for your cover pass, remembering to cool down with an air blower. Stainless doesn't like a lot of heat.
Hope this helps
Frank