Yeah,

No sweat. The 100% Argon will make everything right.

Maybe you got lucky on the Cigweld 175 MIG unit also doing TIG with the same gas due it being a primarily CV unit.

You're going dig that 255EXT, especially when you get pretty good on aluminum.