  1. Default Cleaning dirty aluminum

    I'm gonna try tig repairing an old pair of shrubbery clippers. The cast aluminum anvil portion broke.
    My question is: Should I use my dedicated SS brush to clean this piece or will that just contaminate my brush?
    I realize I could buy a new clipper for less trouble and possibly less money but hey..... i have a tig welder and Im gonna use it😜
    שלום

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    First scrub it with some cleaner and a scrub brush to get all the plant material off, then give a once over with your SS brush and an acetone wipe. Depending on the alloy, it might be no problem or virtually unweldable.
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    Thanks Ram Ill take pics
    שלום

  4. Default

    Well, no pics, sorry... it was a total failure. I don't know if it was because of contamination, alloy, technique or all 3.
    Lighting up on this thing produced all kinds of red colored lightning that looked like Northern lights.
    The only time I could get any kind of focused arc was when it attached to the filler rod. No puddle, just small explosions.
    I guess its time for a new shrubbery clipper.....unless I fabricate a whole new part. Was it on this forum someone said "Why buy a new part for $10 when I can make it for $100"?
    שלום

  5. Default

    Could it have been Magnesium maybe?

  6. Default

    I dunno, Blaster . Just a cheap clipper I bought from Big Lots a long time ago.... Probably $5 brand new.
    שלום

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Blaster View Post
    Could it have been Magnesium maybe?
    More likely pot metal, if it was mag the arc would be stable.
    Long arc, short arc, heliarc and in-the-dark!

  8. #8

    Default

    Probably pot metal. I did have a heck of a time welding a security barrier arm. Turned out it was magnesium. Unstable and worse (visual) than aluminum when it would melt.

    Ended up patching it up with slits and hose clamps until the new one arrived.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. AC balance & cleaning
    By broberts5 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 01-15-2014, 10:34 PM
  2. AC cleaning gone?
    By Infidel in forum TIG Welding (GTAW/GTAW-P)
    Replies: 16
    Last Post: 09-14-2012, 12:38 AM
  3. Cleaning of the welder itself
    By Jules The Great in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 04-20-2012, 07:19 PM
  4. Spring Cleaning...
    By wruehl in forum Personal Projects (no welder required)
    Replies: 13
    Last Post: 04-28-2011, 11:18 PM
  5. Cleaning - How much is needed.
    By sschefer in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 12-21-2010, 04:27 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •