Share
Page 2 of 2 FirstFirst 12
Results 21 to 29 of 29

Thread: Everlast Cooler and Weldcraft CS310

  1. #21

    Default

    Blue line is not rated for that much pressure....different material too if it's the one I am thinking about. Don't swap.

  2. #22
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by performance View Post
    Blue line is not rated for that much pressure....different material too if it's the one I am thinking about. Don't swap.
    Sorry, I'm used to older Weldcraft torches and hoses, and they use the same part number for the water feed hose and the argon hose. I guess these are different. Do you advise him to replace the argon hose to insure there is no contamination? Do you have a procedure for him to get it all cleaned out? I know where I used to work if that happened we would be required to toss that hose.
    Long arc, short arc, heliarc and in-the-dark!

  3. #23

    Default

    Well, if he is not at work, he can do as he pleases. It will depend upon what kind and how much coolant he has used. The manual is pretty clear with procedures how to determine and check. I am not sure he read all the information provided. No, we don't have any procedure, nor should we. If it is only water, then there shouldn' t be any issues once dried out. If it was the water cooler type antifreeze with water, then I suggest flushing it with more water since water was the carrier, then drying it thoroughly.

    I doubt there will be any serious long term issues if it is flushed and dried completely...unless he is building the new spaceX rocket.

  4. Default

    I ran straight coolant through it. You are correct, I saw the picture and saw a blue line and I ASSUMED incorrectly.

    "ARGON GAS LINE SHOULD BE TAGGED AS “Ar”. IF NOT, TAKE DRY, COM-PRESSED AIR AND GENTLY BLOW THROUGH THE LINES TO DISCOVER WHICH LINE EXHAUSTS THROUGH THE TORCH OR THROUGH THE RE-TURN LINE. ON SOME TORCHES, THE WATER LINES ARE COLOR CODED: BLUE FOR COOL WATER SUPPLY AND RED FOR HOT WATER RETURN. COOLER FITTINGS SHOULD BE COLOR CODED BLUE AND RED AS WELL."

    I think the above instructions are a little ambiguous. In my case, there was no tag marked "Ar" and I had a blue line, which above states that, "On some torches, the water lines are color coded: Blue for cool water supply". I did not go through the compressed air steps because I had a blue line. I am surprised this doesn't happen more often, all three hoses have the exact same connector, I would think I'm not the only one who looked at the diagram in the manual and thought, hey, I have a blue line, that must be the output because the fitting on the cooler is blue.

    It might be helpful to place something in bold with an asterisk letting the user know that just because their torch might have a blue line, that doesn't mean it should be plugged into the blue cooler connector, just in case there are people out there that don't have the means to blow compressed air through it. Just my $0.02.

    Anyway, it all seems to be working, I haven't tried to weld anything with it yet so I don't know how much of a contamination issue I'm going to have. How does one run water through the hoses to flush them out if the cooler already has coolant in it? Empty the cooler, fill it with water and mix up the hoses again to rinse out the gas line? What's the procedure for emptying the cooler, flip it upside down and drain it through the filler hole?

    Thanks again for the help.

  5. #25
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    I agree it would be nice if they wouldn't use the exact same connector for the water as for the argon, but I understand that from a cost prospective they only want to stock one type of part.

    For my 2ยข if it was me, I would just cobble up some kind of connection to a garden hose or even just hold it up to a tap with your hand. Run water through it until it comes out clear. Then do something similar with air at low pressure to dry it out. If you have moisture in the hose, and try to weld aluminum, you will know in a big hurry if you didn't get it dry enough.
    Long arc, short arc, heliarc and in-the-dark!

  6. #26
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    I made that mistake once now I blow thru each line and listen for the one that I can hear air coming out of the torch end then I know that is the gas line. I put water thru for awhile and then put methanol (alcohol) to take out the water then blow air to dry up the alcohol and that was fast after a minute or so I could not smell the alcohol did a test weld and all was fine. Good luck Kumaichi.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  7. #27

    Default

    here is a look at my setup

    Click image for larger version. 

Name:	IMG_1243.jpg 
Views:	423 
Size:	147.1 KB 
ID:	12382Click image for larger version. 

Name:	IMG_1244.jpg 
Views:	428 
Size:	140.6 KB 
ID:	12383Click image for larger version. 

Name:	IMG_1243.jpg 
Views:	423 
Size:	147.1 KB 
ID:	12382Click image for larger version. 

Name:	IMG_1244.jpg 
Views:	428 
Size:	140.6 KB 
ID:	12383Click image for larger version. 

Name:	photo 3-3.jpg 
Views:	429 
Size:	118.1 KB 
ID:	12384

    video of my tig machine:
    https://www.youtube.com/watch?v=aUu4...ne4q3WXoSu9MTQ

    here is a link to the adapters
    https://www.arc-zone.com/index.php?m...yword=everlast


    r/
    Jon
    Last edited by dzljon; 09-21-2014 at 04:28 PM.
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

  8. Default

    Thanks Jon, you have the exact setup I'm putting together

  9. #29

    Default

    Quote Originally Posted by kumaichi View Post
    Thanks Jon, you have the exact setup I'm putting together
    No problem brother!
    Machines: EVERLAST Power Tig 210EXT w/ water cooler and 25' CS310 weldcraft torch
    LONGEVITY 250EX Tig
    MILLER 211 mig w/spool gun
    EVERLAST Power Plasma 80s mounted on my Torchmate 2x2 cnc table
    SMITHY 1324 mill/lathe
    60 gal. 7.5 hp air compressor


    MY YOUTUBE CHANNEL: https://www.youtube.com/user/dzljon/videos

Similar Threads

  1. Everlast 250EX and water cooler question...
    By Lucky in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 04-04-2015, 12:06 AM
  2. Tig cooler cooler power source - "warning"
    By Odyknuck in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 12-17-2012, 09:37 PM
  3. Weldcraft 300 aircooled, anyone use it?
    By EchoSixMike in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 05-29-2012, 04:55 PM
  4. Replies: 14
    Last Post: 02-02-2012, 12:28 PM
  5. Cooler
    By dave s in forum Pre-sales, Sales and Shipping questions
    Replies: 0
    Last Post: 12-12-2011, 01:49 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •