I have a PowerPro 256 and I need a much smaller tig torch because I'm welding up something with lots of nooks and crannies.
I need to use up to 125amps AC on aluminum.
It can be air cooled.
I think the torch I'm using now is the EV18 which came with the welder.
I think they should change the way they list the torches to a spreadsheet comparing all of them..the long list with no pics is hard to read and makes it difficult to shop.
BTW the welder is coming up on 5 years and has been worth every penny. What a deal!!!
So my questions would be:
Is the EV17 much smaller than the EV18? There dont seem to be pics on the everlast site.
Could I get away with an even smaller series like the EV9 at 125amps (way over its rating), if I watch how much it heats up carefully?
Is there some kind of used option on ebay that would save me money so I could try it out and resell it if I dont like it?
Or some other brand of common used torch I could adapt?
Thanks for any help!
Heres what I'm welding, its an intake for the old chryslers:
The one in the pic was using the PowerPro256..not too great but its functional!! Thats why I want a smaller torch, the EV18 is just huge to get between the runners.
![]()


							
						
				
				
				
					
  Reply With Quote

				