Originally Posted by
Rambozo
Aluminum frame work on 110V, that is impressive. What is the max amps that it will put out on 110V? Nice to see the panel setting for max amps instead of the pot on the pedal. That should remove some peoples nitpicking on that machine.
That machine used to not have max control available when using a foot pedal. Used to just be max of the machine was max of the pedal. That in itself really isn't much of an issue though.
Mine will go to 120A in AC per the readout on the machine when using 110v (or 120V or whatever it was).
That is pretty much where I was for all of teh welding I did with it. Never got warm at all and never tried to pop the 20A breaker.
Last edited by sportbike; 12-07-2013 at 08:29 PM.