Thread: Concrete planter

  1. #1

    Default Concrete planter

    Pool season again and since I'm the "pool boy" at our Villas, I decided I wanted some plants to make it more homey....

    I found the huge Elephant Ear tree at a local store but couldn't find a planter big enough or heavy enough to not tip over so I made one out of concrete.
    Bought the tree on a Sunday and the pool opened the following Saturday so I had less than a week to make the forms, pour the concrete and hope it would dry fast enough to hold together moving it from my shop to the pool.
    I used 4.5 bags of concrete @ 80lbs.....2 bottles of Charcoal tinting and some Malamine shelving I had sitting around.
    I had a little chipping pulling the forms and moving it but it turned out fine.
















    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default











    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  3. #3

    Default

    It turned out really nice. Did you need to do anything to the form to make it easier for you to remove the form after it all dried?

  4. #4

    Default

    That turned out nice. You can use a rubbing rock or concrete brick to smooth the exterior and fill the small holes if you'd like. Why no drain hole ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by zoama585 View Post
    Why no drain hole ?
    Look closer.
    Long arc, short arc, heliarc and in-the-dark!

  6. #6

    Default

    Quote Originally Posted by Rambozo View Post
    Look closer.
    I didn't notice the little ones.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. #7
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Beautiful work, there. Looks great!
    '13 Everlast 255EXT
    '07 Everlast Super200P

  8. #8

    Default

    Looks fantastic! I've been tempted to try some concrete tabletops, and I was envisioning a setup very similar to the mold you've build. Is there any sort of steel reinforcement in your planter? Or is the concrete fiber-reinforced in some way? I'd think that without some wire mesh or something embedded in the concrete around the circumference, it might be prone to cracking at the corners.
    Everlast PowerArc 140ST

  9. #9

    Default

    Quote Originally Posted by MuttonHawg View Post
    Looks fantastic! I've been tempted to try some concrete tabletops, and I was envisioning a setup very similar to the mold you've build. Is there any sort of steel reinforcement in your planter? Or is the concrete fiber-reinforced in some way? I'd think that without some wire mesh or something embedded in the concrete around the circumference, it might be prone to cracking at the corners.
    Fiber mesh doesn't add to the cured strength, it's only there to prevent shrinkage cracks while curing. Wire only helps when it's under tension, otherwise it just keeps a piece from falling away once cracked.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  10. #10

    Default

    Quote Originally Posted by zoama585 View Post
    Fiber mesh doesn't add to the cured strength, it's only there to prevent shrinkage cracks while curing. Wire only helps when it's under tension, otherwise it just keeps a piece from falling away once cracked.
    I didn't necessarily state it well, but that was actually my point - the corners seem like they would be the points that would crack, and without wire, if/when they do crack, the sides would fall outwards from the soil pressure.
    Everlast PowerArc 140ST

  11. #11

    Default

    Quote Originally Posted by Mr120 View Post
    It turned out really nice. Did you need to do anything to the form to make it easier for you to remove the form after it all dried?
    The Malamine is smooth so it will pull away clean, this is what they use when making table tops. I sealed the plywood and rubbed wheel bearing grease on it about 10 mins. before I poured the concrete, lol. I was in a hurry to get it going. I drilled five 7/16" drain holes in the bottom.

    As far as smoothing it out... After I got it in place and planted, it doesn't look too bad so I'm just gonna leave it alone. Character, right!?
    I didn't use any reinforcement, just used the high strength fiber concrete. Pulling the forms off 24 hours after the pour caused a few problems and I busted a corner down low while transporting it and loosing control of the dolly and it slammed down. Concrete is tough and if you can take your time it usually looks great, just gotta make sure to vibrate the concrete or form or at least use a hammer and repeatedly tap the form to settle the concrete.


    Here's my waterfall I made
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  12. #12
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by MuttonHawg View Post
    Looks fantastic! I've been tempted to try some concrete tabletops, and I was envisioning a setup very similar to the mold you've build.
    Here is step by step of a table top. I know a few people have made table saw tops this way, too.

    Long arc, short arc, heliarc and in-the-dark!

  13. #13

    Default

    Quote Originally Posted by MuttonHawg View Post
    I didn't necessarily state it well, but that was actually my point - the corners seem like they would be the points that would crack, and without wire, if/when they do crack, the sides would fall outwards from the soil pressure.
    There are high strength countertop mixes avilable in bags that would be perfect for your use without the need for wire. Just keep it at least 2" thick and let it cure fully before handling it. Concrete takes 28 days to reach full strength.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. Concrete Plug and Fence Post Pulling Lever
    By fyidiy in forum Other Custom Fabrications
    Replies: 2
    Last Post: 04-29-2017, 10:11 PM
  2. Robust garage floor concrete patch with welded rebar.
    By fyidiy in forum Other Custom Fabrications
    Replies: 4
    Last Post: 10-13-2016, 01:59 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •