    Quote Originally Posted by zoama585 View Post
    I picked up five bags of coal slag at tsc and it's full of curved wire about 3/4" long. I've tried to sift it out but most of the wire goes through the screen. Ever seen this ?
    No clue what that is, but I'd bag it back up and take it back. TSC folks are really good about keeping their customers happy in general.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  2. #22

    Default

    I just had another look and it's not wire. It's more like black glass strands that come to a point like an icicle. Click image for larger version. 

Name:	IMG_1270.jpg 
Views:	353 
Size:	142.5 KB 
ID:	8928 zoom in for a better view.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #23

    Default

    Quote Originally Posted by zoama585 View Post
    I just had another look and it's not wire. It's more like black glass strands that come to a point like an icicle. Click image for larger version. 

Name:	IMG_1270.jpg 
Views:	353 
Size:	142.5 KB 
ID:	8928 zoom in for a better view.
    Does not look right. Maybe a bad run or something at the plant messed up. Look like a lot of work to filter it out. Will get go through the gun without eventually clogging it up?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. #24

    Default

    It clogs the pressure pot instantly. The siphon gun works ok but I have to put my finger over the nozzle and pull the trigger to clear it often.
    Last edited by zoama; 12-25-2012 at 11:29 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  5. #25
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Quote Originally Posted by zoama585 View Post
    It clogs the pressure pot instantly. The siphon gun works ok but I have to put my finger over the nozzle a pull the trigger to clear it often.
    Mine has been driving me nuts, same thing (symptom, not cause) I'll have to look closer to see if that's what's doing it. I cut one of my hoses to about 10" and just manipulate the gun around to siphon up grit, no screen in my cabinet because it kept clogging. I'd love to find a way to get it to feed proper, third gun and two different siphon tubes just love to clog.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  6. #26
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    On a siphon cabinet at an old job I always had to do the finger thing. Then I copied the air setup from the Zero Blast N Peen we had at school. It had a small aux air line right after the foot valve that went down and kept things mixed up right at the siphon tube entrance. Worked like a charm. I put in a needle valve to adjust the flow. I haven't done this to my present cab, because the air valve is on the gun, but I will, someday. It gets old unclogging the tube. And even with super dry air it seems like some things just like to pack up. I miss the foot valve, too. Gets old holding the trigger all the time. Projects, projects. the more I finish, the longer the list becomes. Reading this stuff just reminds me of more stuff I should do.
    Long arc, short arc, heliarc and in-the-dark!

  7. #27
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Thanks for the info, looks like I have two new additions to my project list, copying the air feed and building a foot valve And I desperately need an air dryer; a bead dryer would turn pink in a day though, need to dig around a bit for a better one than what I have.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  8. #28
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    People rave about those Franzinators. I haven't built one yet, but I have a new compressor installation on the list that I will probably try it on. I'm too cheap to spring for a refrigerated dryer on my nickle.
    Long arc, short arc, heliarc and in-the-dark!

  9. #29

    Default

    I think adding a ledge inside the cabinet just above the pickup would stop the material from packing around it. Click image for larger version. 

Name:	pickup.jpg 
Views:	341 
Size:	12.3 KB 
ID:	8972 I'm building a cabinet now so I'll give it a try.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

Similar Threads

  1. Replies: 59
    Last Post: 02-19-2013, 10:16 AM
  2. Replies: 12
    Last Post: 12-30-2012, 05:05 PM
  3. Replies: 7
    Last Post: 10-15-2012, 05:06 PM
  4. Replies: 18
    Last Post: 09-07-2012, 06:46 PM
  5. Replies: 12
    Last Post: 07-19-2012, 08:03 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •