Share
Results 1 to 20 of 20

Thread: Metal cutting Circular saw..... Pics

  1. #1

    Default Metal cutting Circular saw..... Pics

    A cousin of mine brought by a present the other day... a circular saw that is "supposed" to slice through 1/8" steel like butter.
    He bought two of them, one for me and one for him to cut metal siding for out buildings.
    I said, hmmmmm, Thanks, I'll give it a try and let you know. I was a little skeptical....

    WELL, I tried it today and it really does buzz right through 1/8" steel just like you were cutting wood. The cut was super smooth and the saw worked perfect! The only bad thing was the fine metal shavings that hit me in the face and arms.

    Here's the saw on Amazon.. http://www.amazon.com/Evolution-RAGE.../dp/B004QX7P1Y





    And the cut.....
    Last edited by CGCINC; 11-22-2012 at 06:32 PM.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Neat. Not a bad price for something with a 15 amp motor. Definitely wear a full face shield or at least goggles that seal off top, bottom and sides. Be careful!

    Noticed in the description:

    A blade can cut up to 165 feet of 1/4" mild steel before a replacement is required.

    How much for a replacement blade? Is it like razors where they sell the handle below cost so you continue to buy the blades?
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  3. #3

    Default

    I cut 1/4 aluminum plate on my jet cabinet saw with a Freud Diablo non-ferrous blade. The cuts are super smooth with clean edges. The blades are also available in 7 1/4", ferrous or non-ferrous for use in a regular saw.
    Last edited by zoama; 11-22-2012 at 07:11 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4

    Default

    The blades are $24 from what my cousin said. He bought these for $79.99 each locally.
    Not bad for a freebie!!


    Not sure if you can throw this blade on Any circular?!? I guess power is the factor
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  5. #5
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Power and torque. It's got a good 15A. Amazon didn't say how fast the blade is moving.

    Can't complain about the price and if it helps get nice straight cuts with no HAZ, you are laughing!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by undercut View Post
    Amazon didn't say how fast the blade is moving.
    Sure they did, 3700 RPM.

    They have a multi-purpose blade, and a special blade for steel that is a little more.
    I would make sure to only use this on a saw with a metal blade guard, not plastic.
    They might also have dome something with the cooling to make sure the fan doesn't suck chips into the motor. YMMV
    I've been looking for a reason to give one of these a try.

    BTW: I could only find non-ferrous on the Freud site. Is the ferrous one a new item?
    Long arc, short arc, heliarc and in-the-dark!

  7. #7

    Default

    Nothing new here, have done that with a circularsaw 30+ years ago, any circular saw will do the job if you have the right blade. The are abrasive blades made for metal cutting/ bricks etc, ordinary carbide tipped blades will do thin sheetmetal of all types, like metal sideing or eaves trough etc...the downside is flying chips and the noise..
    Some of those lies people tell about me, are true

  8. #8

    Default

    Quote Originally Posted by Rambozo View Post
    Sure they did, 3700 RPM.

    They have a multi-purpose blade, and a special blade for steel that is a little more.
    I would make sure to only use this on a saw with a metal blade guard, not plastic.
    They might also have dome something with the cooling to make sure the fan doesn't suck chips into the motor. YMMV
    I've been looking for a reason to give one of these a try.

    BTW: I could only find non-ferrous on the Freud site. Is the ferrous one a new item?
    I couldn't find them on their site either but everyone sells them http://www.google.com/#hl=en&sugexp=...0&bih=932&bs=1
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  9. #9

    Default

    Quote Originally Posted by Rambozo View Post
    BTW: I could only find non-ferrous on the Freud site. Is the ferrous one a new item?
    I was in Norther Tool this morning and noticed they have the Freud steel diablo blades in stock with many sizes and tooth counts at around $38.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  10. #10

    Default

    Quote Originally Posted by zoama585 View Post
    I was in Norther Tool this morning and noticed they have the Freud steel diablo blades in stock with many sizes and tooth counts at around $38.
    They also have Norton cutoff wheels in 61/2 & 7 inch dia for 3 bucks,,,if you really need to try this ..on a circular saw..
    Some of those lies people tell about me, are true

  11. #11

    Default

    I have used one for about 15 years now , It is a 7 1/4" Freud on an older Dewalt saw and has never been sharpened , It has cut thru 2" stacks of building tin and up to 3/8" flat bar with no problems. You do need to wear safety glasses that seal around your eyes and protective sleeves because the hot metal does fly around from these blades.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  12. #12
    Join Date
    Nov 2012
    Location
    Cambridge, ON. CA
    Posts
    111

    Default

    This looks very interesting! I have a 13A skilsaw laying around that could use one of these kinds of blades. Right now I'm using abrasive asphault blades to cut metal. 8" disk for a buck at PrincessAuto. I'm wondering if it's worth it to get the diablo blades instead. Seems to be a price premium but if they last longer then that might be a good deal. Any thoughts on that? Abrasive vs carbide for the hobbyist?
    PowerArc 140ST
    Victor VPT-100FC

  13. #13
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    We had a miter saw with carbide blade where I used to work that was used for aluminum. I hated it. The noise was horrendous, the hot chips landing on your arms sucked and it just didn't feel right cutting metal like that.

    I also used a circular saw with th eabrasive blade for many years before the PC came to my shop. It made for really smooth straight cuts, but it did take a while to get through 1/2 plate. It throws a lot of particulates too, every time I used it there would be a rather nasty metalic taste in my mouth that lingered for a while.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  14. #14
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    I also hate the abrasive blades, but that's all I have at the moment. I use a 14" chop saw for that. I do try to remember to wear a respirator to keep from breathing that crap. I would love a cold saw, as I've used them in the past, but the size and price keeps them away. I would like to try one of the newer 14" carbide saws that spin much slower, and claim to cut cool. I mostly cut tubing so a plasma isn't as well suited as a saw, for me. I've used a lot of carbide saws on aluminum and never had much issue, but most had some form of coolant.
    Long arc, short arc, heliarc and in-the-dark!

  15. #15

    Default

    Quote Originally Posted by Rambozo View Post
    I also hate the abrasive blades, but that's all I have at the moment. I use a 14" chop saw for that. I do try to remember to wear a respirator to keep from breathing that crap. I would love a cold saw, as I've used them in the past, but the size and price keeps them away. I would like to try one of the newer 14" carbide saws that spin much slower, and claim to cut cool. I mostly cut tubing so a plasma isn't as well suited as a saw, for me. I've used a lot of carbide saws on aluminum and never had much issue, but most had some form of coolant.
    Cutting 2'x2' 1/4" 6061 on the cabinet saw doesn't add any noticeable heat and cuts very easy.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  16. #16
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by zoama585 View Post
    Cutting 2'x2' 1/4" 6061 on the cabinet saw doesn't add any noticeable heat and cuts very easy.
    For aluminum that works great, but it's steel that I'm more interested in. That's where I use the abrasive blade, and would like to switch to something else.
    Long arc, short arc, heliarc and in-the-dark!

  17. #17
    Join Date
    Nov 2012
    Location
    Cambridge, ON. CA
    Posts
    111

    Default Abrasive vs Carbide?

    I've never had a problem with the abrasive disks aside from the mess. As long as you don't force them into the metal they won't shoot fuming chunks of firey sleet at you. They're so cheap and work so well that I find it hard to look at something else. At a place I used to work, we cut anywhere from 1/2" to 1" solid bar stock with them. Now they had a bandsaw there too but everybody preferred the disks because it was faster, surprisingly. Straighter custs on bar stock too anyways.

    Don't really need a metal cutting circular saw as much as just a blade for my miter. After some reading, I could buy a whole new saw for the price of some of those blades. I'll pass for now and stick with whats been working.

    Oh and a little tidbit for those that want a better cut: A lot of the cheaper saws have some far out runout. One way to help with this is to turn down the mandrel hardware included with your saw. I just secured the saw so it won't move and let it free wheel with the mandrel cups exposed but secured and took a sharpening stone to it. True cuts all the time now for 1/5 the price of a finishing saw. If that doesn't work look at replacing the bearings with good allball roller types.

    Cheers.
    PowerArc 140ST
    Victor VPT-100FC

  18. #18

    Default

    Quote Originally Posted by cbmkr View Post
    You do need to wear safety glasses that seal around your eyes and protective sleeves because the hot metal does fly around from these blades.
    They cut well and spew red hot swarf! These aren't grinder sparks, they are ribbons of orange hot metal. If you have any saw dust lurking in the shop's dark corners - do it outside.

  19. #19

    Default

    Quote Originally Posted by blacksmith View Post
    They cut well and spew red hot swarf! These aren't grinder sparks, they are ribbons of orange hot metal. If you have any saw dust lurking in the shop's dark corners - do it outside.
    YES... Don't cut in short sleeves!!! YEouch!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  20. #20

    Default

    or flip flops.... don't ask!
    Everlast PowerTig 200DX
    Everlast Supercut 50P
    I need a MIG.... which one to buy:
    I-Mig 160, I-Mig 200, or a MTS 160

Similar Threads

  1. Cutting Expanded Sheet Metal
    By xtreme cartz in forum Everlast Plasma Cutters (PAC)
    Replies: 55
    Last Post: 02-14-2013, 02:16 PM
  2. DIY dryer for plasma cutting and TIG welding. Dross cutting or TIG electrode fur
    By everlastsupport in forum Welding articles from Professionals (knowledge database)
    Replies: 0
    Last Post: 03-15-2012, 12:08 PM
  3. Cutting expanded metal with the PP 50
    By trickbiker in forum Everlast Plasma Cutters (PAC)
    Replies: 6
    Last Post: 01-24-2012, 08:24 AM
  4. cutting expanded metal
    By macdarren in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 12-04-2009, 03:00 AM

Posting Permissions

  • You may not post new threads