    ]I got my power plasma 50 last week and thought I would give my first impression of it.
    It arrived well packaged I unpacked it and went to install the water filter and found a minor glitch. I couldn't install it with the supplied hardware. I went to the Hardware store and bought 2 spacers which allowed the installation of the Bracket. See attached pictures Click image for larger version. 

Name:	253.JPG 
Views:	497 
Size:	58.5 KB 
ID:	4239[ATTACH=CONFIG]4240[/ATTACH I then went to install the filter to the bracket and found the mouting screws were too long. A dremmel with a cutoff wheel quickly fixed this. I next installed my power plug.
    Now that I got the filter installed Time To play. I set the input pressure on my air supply to 85psi connected the air hose and plugged the plasma cutter in.Set air pressure to 70psi and amperage to 30amps on plasma cutter. Connected ground clamp to some 1/8 steel stock and proceeded to cut through it like butter. I made numerous cuts piercing and edge cuts. I'm loving this plasma cutter. after about 15 minutes of cutting metal I turned the power off and heard an air leak inside the plasma cutter. I removed the cover and found oneof the air hoses was not pushed all the way into it's connector. The hose is clear polypropolene material and runs next to the transformer I don't know if the heat softened it or it just wasn't connected all the way from the factory. I have now installed a nylon hose on the quick connectors (it has a much higher operating temperature and pressure and only cost $5 I had to buy 10 feet). I put the cover back on the plasma cutter no leaks anymore. I'm loving my plasma cutter again. For the price I don't mind doing a couple of minor things to end up with a even better plasma cutter. At this point I would have no problem recommending this plasma cutter. I still have thicker metal to cut and see how it performs with it. The only recommendations I would make is supply 2 plastic spacers for the filter bracket, 2 shorter screws to mount the filter to it's bracket and change the internal air supply hose to nylon just to be safe.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	255.JPG 
Views:	433 
Size:	68.2 KB 
ID:	4240  
    Lincoln 180 Mig 36inch blast cabinet
    Grizzly 10x22 Lathe 12 Ton hydraulic press
    Enco Square column Mill
    Oxy Acetylene Torch
    Power Plasma 50
    Micro Tig 185

  2. #2

    Default

    The mounting bracket has been a problem for quite a while. I made one from a small piece of aluminum angle that worked well.

    The air lines also have been an issue. My solution was to use the nylon brake lines and replace the push-in fittings with compression fitting throughout the machine. No air leaks now and much less of a possibility of future leaks.

    Next time you have the machine apart you may want to check the gap on the HF points. Not sure what the setting should be for your machine.

    Photo of bracket before the air fittings were changed to compression.
    Click image for larger version. 

Name:	Welder-Plasma_04 (Large).JPG 
Views:	521 
Size:	138.3 KB 
ID:	4241

    I have a review of the PP70 somewhere if you search. Ah, found it:

    http://www.everlastgenerators.com/fo...asma-70-review
    Last edited by GWD; 12-23-2011 at 08:12 PM.
    Everlast PowerArc 300
    Everlast PowerArc 200
    Everlast PowerPlasma 70
    Hobart Handler 125 EZ
    Lincoln Tombstone AC
    Lincoln Tombstone AC/DC
    O/A outfit
    Honda 11K generator

  3. #3

    Default

    Quote Originally Posted by vettebob View Post
    ]The only recommendations I would make is supply 2 plastic spacers for the filter bracket, 2 shorter screws to mount the filter to it's bracket and change the internal air supply hose to nylon just to be safe.
    Same here on the older model SC50. I Spaced our's with a 1/4"-20 nut and two washers. Thanks for the review, as I am going to getting one soon.
    I Love Plasma and rolleye's at the costly addiction of MAPPgasoron's.

    http://brothers2woodworking.webstarts.com/

    Everlast Plasma cutter Power Plasma 50
    Everlast PowerArc 200 ~ Happily Married To That gutsy babe, git'er dun.


    Wishlist: Free consumables, Small TIG maybe Alex, when you have overstock give me ring!

Similar Threads

  1. Power Plasma 50 MVP
    By frans in forum Everlast Plasma Cutters (PAC)
    Replies: 5
    Last Post: 12-30-2013, 11:34 AM
  2. Power Plasma 50 or 60c
    By MoJo1917 in forum Everlast Plasma Cutters (PAC)
    Replies: 2
    Last Post: 11-22-2012, 11:00 PM
  3. Power Plasma 50 plasma cutter....
    By CGCINC in forum Customer Testimonials
    Replies: 4
    Last Post: 07-20-2012, 12:58 PM
  4. Power Plasma 60C
    By todmorg in forum Everlast Plasma Cutters (PAC)
    Replies: 4
    Last Post: 11-28-2011, 02:46 PM
  5. Power Plasma 50 help.
    By dean_af in forum Everlast Plasma Cutters (PAC)
    Replies: 11
    Last Post: 10-04-2011, 03:46 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •