I did a little repair work for my church Monday. I welded a piece of stainless on our hot plate (buffet table), that holds the glass. I can't say that I have ever welded any stainless. It blacked up on me pretty good, and after I got the hang of it I put down an ok bead. I was using 2% thorated tungsten and 3/32 rods. I know I needed thinner rods. No one keeps any stainless rods in stock, I bought 3 pieces at a local machine shop. The guy asked me what alloy I was welding on. I told him I had no clue, and I was just supporting a piece of plexi glass. My questions are
What do I need to do so the metal will not black up?
Do I need different rods for different stainless?
Is there a good middle of the road stainless?
What tungsten should I use?
Is there a certain way I should hold the torch?
By the way I was using my handy dandy Power Arc 140 ST


 
					
					 
							