Welding a bead on plate with 1/4" will take quite a bit of heat to get good penetration. Perhaps you are welding without enough heat and your resulting slow travel speed is causing the larger amount of etching due to hanging around too long. Also, be mindful that everytime you dip your filler, it takes energy to melt the filler. Not really of concern when welding 1/4" plate with 3/32 filler, but if you weld thin materials with relatively large diameter filler, it can be hard to manage. 
If you have some thinner (~1/8") material, I'd give that a try first for practice.
Do you have your ground clamp directly on the material?
Not sure that any of my comments really have anything to due with the amount of etching you are getting...
				
			 
			
		 
			
			
			
				
					Last edited by sportbike; 09-23-2011 at 05:03 PM.
				
				
					Reason: typo/spelling
				
			
			
			
				
			
			