Thread: For Ken White....

  1. #1

    Default For Ken White....

    Here's what I got with the machine on 120v. oh and all i had was 1/4 steel. amps at 45. air at 65psi.
    the welding was all pedal. with 3/32 lant. pure argon. 5 cup.

    220v cut
    Click image for larger version. 

Name:	220v.jpg 
Views:	370 
Size:	139.2 KB 
ID:	5939

    120v cut
    Click image for larger version. 

Name:	120v.jpg 
Views:	337 
Size:	142.2 KB 
ID:	5940

    120v w/filler
    Click image for larger version. 

Name:	120v rod.jpg 
Views:	341 
Size:	139.4 KB 
ID:	5941

    120v fused
    Click image for larger version. 

Name:	120v fused.jpg 
Views:	356 
Size:	130.1 KB 
ID:	5942

    The machine didn't hiccup at all. hope this helps.
    PowerUltra 205
    Lincoln Weldpak
    hopefuly will have a benchtop lathe.

    I live with fear everyday, but SHE lets me play on the weekends...

  2. #2

    Default

    Wow that cut looks really nice. What kind of machine are you using??? Didn't think I wanted a plasma cutter but now you are making me look.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  3. #3

    Default

    Quote Originally Posted by Brian Ski View Post
    Wow that cut looks really nice. What kind of machine are you using??? Didn't think I wanted a plasma cutter but now you are making me look.
    PowerUltra 205
    PowerUltra 205
    Lincoln Weldpak
    hopefuly will have a benchtop lathe.

    I live with fear everyday, but SHE lets me play on the weekends...

  4. #4

    Default

    Quote Originally Posted by Brian Ski View Post
    Wow that cut looks really nice. What kind of machine are you using??? Didn't think I wanted a plasma cutter but now you are making me look.
    Your gonna mess around and start spending all your money! lol
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  5. #5

    Default

    Quote Originally Posted by CGCINC View Post
    Your gonna mess around and start spending all your money! lol
    All my money??? What money???

    Just did more digging. A plasma cutter brings in a whole new world of learning. With a whole new world of consumables. Does it ever end??? Still looking at a 200dx. But the combo Power Pro 205 looks really nice. That is a ways out of my league. To see someone cut through steel like that. Not sure what else would cut aluminum that nice without a shear.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  6. #6

    Default

    sydneysdad, thank you very much. Did you drag cut or hold the cut about 1/16" -> 1/8" above the metal? Your PU205P definitely cuts better than mine on 120V. Thanks again,

    Ken
    __________________________
    Everlast Power I-MIG 200
    Everlast PowerUltra 205P
    Everlast SM 200-N
    Thermal Dynamics Cutmaster 42

  7. #7

    Default

    That is some pretty nice cut quality on both the 220 and 120V cuts.

    If Ken gets his figured out, I think I know what my next machine purchase will be...
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  8. #8

    Default

    Quote Originally Posted by kenwhite View Post
    sydneysdad, thank you very much. Did you drag cut or hold the cut about 1/16" -> 1/8" above the metal? Your PU205P definitely cuts better than mine on 120V. Thanks again,

    Ken
    I dragged it on the wire guard thingy thing? what ever its called.. lol which is about 1/8 from the surface.
    PowerUltra 205
    Lincoln Weldpak
    hopefuly will have a benchtop lathe.

    I live with fear everyday, but SHE lets me play on the weekends...