New to TIG welding but not new to MIG or Stick. I'm welding carbon steel thin sheet metal body panels up to 2" square tubing so nothing really heavy. My question is with the ground on the DC port in the front what does my lead inside the welder need to be on, the + or the - terminal above the wire feeder?