Thread: Why is E6010 not recommended on the 225LX?

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default Why is E6010 not recommended on the 225LX?

    I'm totally ignorant when it comes to stick. The very first weld I laid down around 15 years ago used about half of one electrode and I haven't struck one since. So this might be obvious with those who know, but why is E6010 electrodes not recommended with the 225LX? I don't think I see any other Everlast welders that exclude that specific rod.

    Obviously I can get through life, no problem, without every burning an E6010. But I am curious!

  2. #2

    Default

    I'm guessing its related to the fact that E6010s run a couple volts higher when its being burned. Maybe someone else can chime in on this.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  3. #3

    Default

    Quote Originally Posted by Paul Moir View Post
    I'm totally ignorant when it comes to stick. The very first weld I laid down around 15 years ago used about half of one electrode and I haven't struck one since. So this might be obvious with those who know, but why is E6010 electrodes not recommended with the 225LX? I don't think I see any other Everlast welders that exclude that specific rod.

    Obviously I can get through life, no problem, without every burning an E6010. But I am curious!
    I'm curious as well ... in my early days of welding before I got mig machines and tig unit I used a lot of 6010 and found it worked pretty well on steel that was ... well ... not so clean ... you know a little surface rust etc. I was using my old Miller Thunderbolt and cranked it up a bit ... interesting that it's discouraged for use with the 225LX.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  4. #4

    Default

    6010 does not run well with inverter welders. It has to have some type of adjustable or adaptive arc force so it can weld 6010. I've tried running 6010 with inverters that do not have adaptive arc force, and it will drive you mad! The arc will not stay lit!
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  5. #5

    Default

    I could just run 5p 6010s on my hobart stickmate. you had to hold a tight arc cause it would go out as soon as you long arced it. my thermal arc inverter will run 6010s all day though. I can long arc it all i want and it will stay lit.

    I believe that the welders that aren't designed for 6010s can't put out the set amperage with enough voltage to keep the rod going.

    I shot a video showing the amp draw of my thermal arc inverter with different rods. the first 2 rods were 3/32 7018 and a 1/8 6010 5p rod. both were set at 90 amps, but the 6010 drew more input power because it runs at a higher voltage. Ill have to shot a video showing output voltage and output current sometime.

    bty, for the safety people, I dont use 1/8 inch or bigger rods with that welder and the 20 amp plug. I use the 50 amp plug for everything except light duty stuff.

    http://www.youtube.com/watch?v=MASbAGPPiSA
    Last edited by welderdude; 05-15-2012 at 07:40 PM. Reason: added info/spelling
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

  6. #6

    Default

    Has there been any issues using 6013 electrodes with inverter welders?
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  7. #7

    Default

    Quote Originally Posted by Winky View Post
    Has there been any issues using 6013 electrodes with inverter welders?
    6013 runs good, I have ran it on the Power Arc 200, PT 200dx, Power Arc 140st. I have not ran it on my 225lx.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  8. #8

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    6013 runs good, I have ran it on the Power Arc 200, PT 200dx, Power Arc 140st. I have not ran it on my 225lx.
    Thanks ... good to know ... of all the SMAW electrodes ... that's the one I've used the most. I have a good supply of them but they're a little old ... I may need to replace what I have.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  9. #9

    Default

    I only run two rods for the most part 7018 (heavy stuff) and 7014 (thin stuff). I have sealed cans of 6013 and 6011 that I have had for a year.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  10. Default

    It has to do with the voltage. 6010s need a few more volts to stay running smooth and with ease. I have a power are 200 that has its own port for 6010 and they still dont run the best. Now ive ran them with a transformer and they run much better it seems. If you try to run them with your machine turn the arc force all the way up because as i understand that has the most voltage output.
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  11. #11

    Default

    I use metal coat hangers for welding rod lol
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  12. #12

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    I use metal coat hangers for welding rod lol
    What do you use for hanging your coat??? Welding rod??? Hahahahahaha
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  13. Default

    Agreed with 7018 most of the time. Also 6010s. Mojority of the rods I use is 7018 becuase they work for thick not to bad for thinner.
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  14. #14

    Default

    Quote Originally Posted by bobwills View Post
    It has to do with the voltage. 6010s need a few more volts to stay running smooth and with ease. I have a power are 200 that has its own port for 6010 and they still dont run the best. Now ive ran them with a transformer and they run much better it seems. If you try to run them with your machine turn the arc force all the way up because as i understand that has the most voltage output.
    That makes sense my old dinosaur Thunderbolt is a transformer unit … come to think of it one of the reasons I don’t use that machine much anymore is because it draws a whole lot of power and I can sure see it when the bill comes.
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

  15. #15

    Default

    Bob, It seems that your and my experience may differ here. The PA 200's run them excellently. Inverters, even Millers require different techniques to run them though, and many transformer guys have trouble doing so. Ask a guy to weld with a 6010 on a transformer who has only run inverters and you'll find similar remarks. I've also had multiple pros in the industry remark on the arc quality with the 6010 and the PA200.

  16. Default

    They do run a little different between the too. I dont use them all that much. At first I seem to have a bit trouble with them going out but after I run one or two I seem to get the hang of it and they run good. Sometimes I have great luck with them sometimes not so much. I just havnt got used to them yet. Do you all use the 6010 5p (red) or 5p+
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  17. #17

    Default

    Any given welder, (Yes, even transformers) you will find that some welders perform differently with different brands. One of our customers recommends the ESAB atom arcs for the PA 200s. I use both the 5P and even the 5P+ from Lincoln.

  18. #18

    Default

    Quote Originally Posted by undercut View Post
    How long can keep rods?
    I would guess years, if they are stored properly. A number of of the low hydrogen rods can be reconditioned by baking the moisture out in a oven. DaveO posted a great chart that he found a number of months ago on reconditioning. Also, some rods (like the 6011, I think) can get too dry in storage and will run terribly until they get some moisture.

    Cheers
    Mike
    Power Pro 256

  19. #19
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by posixPilot View Post
    I would guess years, if they are stored properly. A number of of the low hydrogen rods can be reconditioned by baking the moisture out in a oven. DaveO posted a great chart that he found a number of months ago on reconditioning. Also, some rods (like the 6011, I think) can get too dry in storage and will run terribly until they get some moisture.

    Cheers
    Mike
    I'll need to search around for that chart. Thanks for the heads-up!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  20. #20

    Default

    Quote Originally Posted by undercut View Post
    I'll need to search around for that chart. Thanks for the heads-up!
    Here's the thread:

    http://www.everlastgenerators.com/fo...ead.php?t=2868

    Cheers
    Mike
    Power Pro 256

Similar Threads

  1. Just got my 225LX
    By El guapo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 15
    Last Post: 02-17-2013, 04:56 PM
  2. Anyone run cellulosic E6010 electrodes in TIG 210Ext?
    By Martine in forum Stick Welding (SMAW)
    Replies: 22
    Last Post: 12-09-2012, 10:19 PM
  3. Recommended Settings?
    By Buggy Chief in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 04-23-2012, 03:22 PM
  4. My new 225lx
    By dyethor in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 02-24-2012, 08:00 AM
  5. 225LX can't seem to get it to tig..
    By Hayapower in forum TIG Welding (GTAW/GTAW-P)
    Replies: 19
    Last Post: 12-10-2011, 01:57 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •