    Well, let me start off by saying I got a killer deal on some MIG wire a about 4 years ago. I bought a Miller 250, lease size bottle, and a near new 550lb spool of wire for $1000. Sold the welder for $1000 and kept the wire/bottle.

    I have made a slight dent in the wire, but I feel it will probably last me another 10 years unless I use it ALOT more than I do. It has a dessicant bag in the bottom of it, and a plastic hood on the top the wire feeds out of, but by no means is it 'sealed'. Would the dessicant bag be enough? I haven't noticed any corrosion on it yet (I have had it for 4 years like I said above). Should I get another bag of dessicant to put in the barrel, or just leave it as-is?
    http://www.facebook.com/CBRMetalworks

    '96 Tacoma V6 on 37's, full custom, built for racin!
    Yamaha Rhino w/ 800 Rotax built for racin!
    Miller 251 MIG
    Everlast Powerplasma 60C with CNC plasma table

    Looking for sponsors for KOH 2013 race!
    Racin' Tacoma Build Thread

  2. #2

    Default

    Quote Originally Posted by Tacoma747 View Post
    Well, let me start off by saying I got a killer deal on some MIG wire a about 4 years ago. I bought a Miller 250, lease size bottle, and a near new 550lb spool of wire for $1000. Sold the welder for $1000 and kept the wire/bottle.

    I have made a slight dent in the wire, but I feel it will probably last me another 10 years unless I use it ALOT more than I do. It has a dessicant bag in the bottom of it, and a plastic hood on the top the wire feeds out of, but by no means is it 'sealed'. Would the dessicant bag be enough? I haven't noticed any corrosion on it yet (I have had it for 4 years like I said above). Should I get another bag of dessicant to put in the barrel, or just leave it as-is?
    Never seen a 550lb spool.... hows that setup work ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3

    Default

    Put it in a plastic bag, vaccum it then fill it with argon,,,should to do the trick..there maybe other ways that some one could tell us about...
    Some of those lies people tell about me, are true

  4. #4

    Default

    put in a air dry box in plastic bags and cover with fresh step crystals cat litter its 95 percent dissintent will keep it dry Click image for larger version. 

Name:	51dkXQgZmFL._SL500_AA300_.jpg 
Views:	666 
Size:	16.7 KB 
ID:	6926. when ready to use just blow off with air gun
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  5. #5

    Default

    Is it in a drum? I don't think I have ever seen a 550lb spool of welding wire. Seen it in drums, just not a huge spool.
    Last edited by sportbike; 05-31-2012 at 12:50 PM.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  6. #6

    Default

    most standard wire drums are 400 pounds there mostly uses in automation welding plants .
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    At a trade show I saw an ESAB system with 550 and 900 pound drums for feeding welding robots. They even had a little machine to butt weld the ends of the wires together and grind them smooth so they could transition from one drum to the next without the robot ever stopping. It looked something like a bandsaw blade welder.
    Long arc, short arc, heliarc and in-the-dark!

  8. #8

    Default

    Quote Originally Posted by Rambozo View Post
    At a trade show I saw an ESAB system with 550 and 900 pound drums for feeding welding robots. They even had a little machine to butt weld the ends of the wires together and grind them smooth so they could transition from one drum to the next without the robot ever stopping. It looked something like a bandsaw blade welder.
    Do the drums rotate ? If they don't it seems like twist would be a problem before the drive rollers.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  9. #9

    Default

    work like this
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  10. #10
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    work like this
    Wow. No spool in the center. Wonder how they can make it so that the wire doesn't develop a twist as it is pulled out ... ?
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  11. #11
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Quote Originally Posted by undercut View Post
    Wow. No spool in the center. Wonder how they can make it so that the wire doesn't develop a twist as it is pulled out ... ?
    ...or get snarled when one strand of coil gets wrapped up inside another. I can't even keep extension cords straight.

    Tacoma, you sure scored on that welder deal (bought for a grand, then sold for a grand and kept the wire and the bottle.) Are you in fabrication? What size wire is it? You could keep quite a few welders going, if there was a good way to re-wrap wire onto spools!
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  12. #12

    Default

    Quote Originally Posted by Tacoma747 View Post
    Well, let me start off by saying I got a killer deal on some MIG wire a about 4 years ago. I bought a Miller 250, lease size bottle, and a near new 550lb spool of wire for $1000. Sold the welder for $1000 and kept the wire/bottle.

    I have made a slight dent in the wire, but I feel it will probably last me another 10 years unless I use it ALOT more than I do. It has a dessicant bag in the bottom of it, and a plastic hood on the top the wire feeds out of, but by no means is it 'sealed'. Would the dessicant bag be enough? I haven't noticed any corrosion on it yet (I have had it for 4 years like I said above). Should I get another bag of dessicant to put in the barrel, or just leave it as-is?
    NC??? How is your humidity??? Guessing on the lower side??? If you haven't had a problem already, I don't foresee much changing. What kind of wire is it??? I have some E70S6 and it is copper coated steel so it does not rust. Is yours the same??? Another couple bags of desiccant would help but only if the container is sealed.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  13. #13

    Default

    Tocoma were you live is about the same for humidity since i am under a mile from the Colorado river, July and Sept its like 70 or more for humidity were i am at . only thing i really keep sealed good and dissident is my aluminum wire since moisture is hard on it
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  14. #14

    Default

    It's copper coated, so rust is not an issue, I was thinking more of just corrosion, no, I haven't had a problem yet, I just don't want to get to the bottom of the drum (no, it's not a spool) and have 200lbs of wire that I can't use. I will probably just put another bag of dessicant in the drum and call it good. Guess I can check the dessicant in the other bag and see if it has changed color. It is stored in a basement, temperature stays ~60-75 depending on time of year.

    I just did a quick search, mine looks identical to this (which is a good deal if someone is nearby!): http://www.ebay.com/itm/550LBS-STEEL...983#vi-content

    The hood is the same idea as this, although mine is clear: http://www.lincolnelectric.com/en-us...age-hoods.aspx
    http://www.facebook.com/CBRMetalworks

    '96 Tacoma V6 on 37's, full custom, built for racin!
    Yamaha Rhino w/ 800 Rotax built for racin!
    Miller 251 MIG
    Everlast Powerplasma 60C with CNC plasma table

    Looking for sponsors for KOH 2013 race!
    Racin' Tacoma Build Thread

  15. #15

    Default

    I don't think you should have any issues the way you're storing it now. I have a couple 40lb rolls that are stored in the box, on the shelf, for years, and have not had any issue. S/F.....Ken M
    Lincoln Power MIG 300
    Everlast 160STH
    Miller 225 Thunderbolt (sold it)
    Lincoln Squarewave 175 TIG(traded it for)
    Miller DEL 200 welder/genset
    Thermal Dynamics 1250XL plasma cutter
    Miller XMT300

Similar Threads

  1. Hot Storage
    By RP62 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 05-11-2012, 01:57 AM
  2. Replies: 26
    Last Post: 02-22-2012, 11:25 AM
  3. 67 cuda long term project
    By 67cudafb in forum Hobyist Projects
    Replies: 17
    Last Post: 02-20-2012, 12:10 PM
  4. Welder Storage????
    By Gtig in forum General Welder Questions
    Replies: 1
    Last Post: 06-11-2011, 06:48 PM
  5. Motorized scooter out of storage
    By Mikeymetal in forum Personal Projects (no welder required)
    Replies: 4
    Last Post: 04-30-2011, 12:14 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •