Thread: Welding practice on Friday

  1. #1

    Default Welding practice on Friday

    Click image for larger version. 

Name:	100_4598.jpg 
Views:	576 
Size:	147.9 KB 
ID:	5969Well, here I have an uphill weld...Four passes of 7018 at 90 amps on 1/8" steel.

    Click image for larger version. 

Name:	100_4599.jpg 
Views:	573 
Size:	148.9 KB 
ID:	5967Here I have just one pass of FCAW.

    Click image for larger version. 

Name:	100_4597.jpg 
Views:	607 
Size:	148.3 KB 
ID:	5968And here I have 7 passes, yes seven passes, of 7018 at 120 amps. The weld is about 1-3/16" wide.


    This was all performed with my Everlast IMIG 200.
    Benjamin

    Owner of IMIG 200 and half owner of Power Plasma 50

    https://www.facebook.com/BenjaminRootPhotography

  2. #2
    Join Date
    Mar 2011
    Location
    The Boonies of Texas
    Posts
    420

    Default

    Mighty fine Benjamin. I need to practice a lot.

    Thurmond
    Miller Bobcat 3 Phase,
    Miller Suitcase X-Treme 12VS wire feeder for the Bobcat with M-25 300A .045" gun / Bernard 400A 5/64" wire mig gun .
    26 series gas cooled TIG torch, setup for quick connect to Bobcat.
    17 series gas cooled Tig Torch for Low Amp Solar Tig (Direct Solar Panel Powered Tig welding)
    Hobart Handler 187 Mig / Fluxcore
    EVERLAST PowerUltra 205P
    EVERLAST PowerTig 250 EXT 2013 Model

  3. #3

    Default

    Quote Originally Posted by Tritium View Post
    Mighty fine Benjamin. I need to practice a lot.

    Thurmond
    Thank you! I am in the process of getting 75/25 Ar/Co2 so that should help me out some with better wire welds.
    Benjamin

    Owner of IMIG 200 and half owner of Power Plasma 50

    https://www.facebook.com/BenjaminRootPhotography

Similar Threads

  1. TIG welding practice
    By SportPilot in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 07-05-2013, 03:09 AM
  2. practice welding question
    By Brian Ski in forum General Welding Questions
    Replies: 22
    Last Post: 05-04-2012, 10:33 PM
  3. more welding practice, PP205
    By presure2 in forum General Welding Questions
    Replies: 7
    Last Post: 10-09-2011, 07:17 PM
  4. Mig welding practice over the weekend
    By MigPlazArc in forum Hobyist Projects
    Replies: 17
    Last Post: 09-24-2011, 02:36 PM
  5. Mig welding practice over the weekend
    By MigPlazArc in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 0
    Last Post: 09-20-2011, 01:40 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •