    Default Wall art , first real tig project.

    Here are a couple of shots of my first metal scroll art project.
    It is for the new sun room My wife wanted one and I said I can do that why buy one.
    It was a fun project and allowed me to buy a scroll attachment for the HF compact bender, earn a few brownie points and tell my wife "see honey all those tools and machines really are for the both of us." Pretty good investment I think.

    I used my Everlast 250 ex set to 185 or so amps 3/32, 2% thoriated. tungsten,
    for the fusion welds. I only had to re-grind the tungsten a few time during the project, now for me that's real progress and a point of pride

    Click image for larger version. 

Name:	sun room 006.jpg 
Views:	699 
Size:	92.1 KB 
ID:	3887

    Click image for larger version. 

Name:	sun room 003.jpg 
Views:	693 
Size:	59.1 KB 
ID:	3888
    Last edited by Ram48; 11-04-2011 at 02:23 PM. Reason: Growing up in the 60s still has its drawbacks
    Everlast I mig 205
    Everlast 200 amp spool gun
    Everlast 250 ex
    H. F. 12x36 lathe
    Grizzly Mill
    10,000 lb two post lift
    Box and Pan Brake
    Bead roller
    jet 5x7 horizontal band saw
    Wilton 14 inch vertical band saw
    Mitec 50 A plasma cutter.
    tool grinder
    20 ton press and press brake
    more power and hand tools then I can list here
    Dodge Neon that runs 10.23 @143 mph in the quater
    70 Chevelle convert
    It took 62 years But I finally have my dream Garage

  2. #2

    Default

    Looks pretty cool. Hopefully your wife likes it and will allow you to buy more toys :-)
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  3. Default

    That looks nice... it's always nice when ones wife sees the value of ones tools.
    How did you bend the strips of metal?.. they look so uniform.

    Ahhh! I've been jipped!

    My 250EX TIG didn't come with any voltage control facility what so ever.

    Joking aside, where did you get the 18.5 volts from?

    Wait, I thought arc force was for stick mode only. Is that what you were using?
    Last edited by parkour; 11-04-2011 at 02:23 AM.

  4. #4

    Default

    Cool looking work, it appears you have some artistic talent we didn't know about.
    Some of those lies people tell about me, are true

  5. #5
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Thanks for the tips on getting the wife's approval for new toy... er I mean tools. (where is the strikethrough on this forum anyway?)

    That is some seriously nice craftsmanship there, great job.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  6. #6

    Default

    Quote Originally Posted by parkour View Post
    That looks nice... it's always nice when ones wife sees the value of ones tools.
    How did you bend the strips of metal?.. they look so uniform.

    I used a scroll attachment for my Harbor freight compact rod bender. I had the bender and the scroll attachment was $39 with coupon.

    Ahhh! I've been jipped!

    My 250EX TIG didn't come with any voltage control facility what so ever.

    Joking aside, where did you get the 18.5 volts from?

    Wait, I thought arc force was for stick mode only. Is that what you were using?
    Um this what happens when you breath welding fumes all day, oor it could be I am just old lol
    I gave the mig voltage setting I used for attaching the "M" to the scroll work.


    Quote Originally Posted by geezer View Post
    Cool looking work, it appears you have some artistic talent we didn't know about.
    Thanks Geezer I did not know about that either lol
    Everlast I mig 205
    Everlast 200 amp spool gun
    Everlast 250 ex
    H. F. 12x36 lathe
    Grizzly Mill
    10,000 lb two post lift
    Box and Pan Brake
    Bead roller
    jet 5x7 horizontal band saw
    Wilton 14 inch vertical band saw
    Mitec 50 A plasma cutter.
    tool grinder
    20 ton press and press brake
    more power and hand tools then I can list here
    Dodge Neon that runs 10.23 @143 mph in the quater
    70 Chevelle convert
    It took 62 years But I finally have my dream Garage

  7. #7

    Default

    Quote Originally Posted by redbeard View Post
    (where is the strikethrough on this forum anyway?)
    [s]strikethrough[/s] vB code in not enabled on this forum.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  8. #8

    Default finished

    Here are a couple of the finished wall art.
    My wife loves it and asked if I could make candle holders to match. I said sure bit I will need to get a ring roller for the project. If you need it get it she said.
    I think I may have hit upon a plan for future purchases lol. What can I make for her that would require a stomp shear?
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	sun room 008.jpg 
Views:	527 
Size:	125.7 KB 
ID:	3920   Click image for larger version. 

Name:	sun room 007.jpg 
Views:	499 
Size:	125.8 KB 
ID:	3921  
    Everlast I mig 205
    Everlast 200 amp spool gun
    Everlast 250 ex
    H. F. 12x36 lathe
    Grizzly Mill
    10,000 lb two post lift
    Box and Pan Brake
    Bead roller
    jet 5x7 horizontal band saw
    Wilton 14 inch vertical band saw
    Mitec 50 A plasma cutter.
    tool grinder
    20 ton press and press brake
    more power and hand tools then I can list here
    Dodge Neon that runs 10.23 @143 mph in the quater
    70 Chevelle convert
    It took 62 years But I finally have my dream Garage

  9. #9
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by Ram48 View Post
    What can I make for her that would require a stomp shear?
    Well it might be a bit too utilitarian, but a set of metal shelves ought to get you a box-and-pan brake as well.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  10. #10

    Default

    Quote Originally Posted by redbeard View Post
    Well it might be a bit too utilitarian, but a set of metal shelves ought to get you a box-and-pan brake as well.
    Already have a box and pan brake lol Im 62 and been doin this for a while
    Look at my partial list of toys below
    Everlast I mig 205
    Everlast 200 amp spool gun
    Everlast 250 ex
    H. F. 12x36 lathe
    Grizzly Mill
    10,000 lb two post lift
    Box and Pan Brake
    Bead roller
    jet 5x7 horizontal band saw
    Wilton 14 inch vertical band saw
    Mitec 50 A plasma cutter.
    tool grinder
    20 ton press and press brake
    more power and hand tools then I can list here
    Dodge Neon that runs 10.23 @143 mph in the quater
    70 Chevelle convert
    It took 62 years But I finally have my dream Garage

  11. #11

    Default

    Looks like you are about to enter the world of Eisenkraft, either buy it or build it,http://www.youtube.com/watch?v=F6ra2KaNhkY
    Some of those lies people tell about me, are true

  12. #12

    Default

    Quote Originally Posted by geezer View Post
    Looks like you are about to enter the world of Eisenkraft, either buy it or build it,http://www.youtube.com/watch?v=F6ra2KaNhkY
    Great stuff but its my guess they are not priced for the hobbyist. I am more interested in motorsports fabrication then ornamental iron work but want to be able to perform as many metalworking disciplines as possible. Like most on here I just love to make things
    Everlast I mig 205
    Everlast 200 amp spool gun
    Everlast 250 ex
    H. F. 12x36 lathe
    Grizzly Mill
    10,000 lb two post lift
    Box and Pan Brake
    Bead roller
    jet 5x7 horizontal band saw
    Wilton 14 inch vertical band saw
    Mitec 50 A plasma cutter.
    tool grinder
    20 ton press and press brake
    more power and hand tools then I can list here
    Dodge Neon that runs 10.23 @143 mph in the quater
    70 Chevelle convert
    It took 62 years But I finally have my dream Garage

  13. #13
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Quote Originally Posted by Ram48 View Post


    Already have a box and pan brake lol Im 62 and been doin this for a while
    Look at my partial list of toys below
    Oops, that list is so long I must have just glossed right over it.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  14. #14

    Default candle holders

    Well I scored so many brownie points with the wall art I figured Id go for broke and made a set of candle holders to match. Man It worked, I just need to figure out what I want to do with them, the points not the candle holders.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	sun room 012.jpg 
Views:	491 
Size:	126.5 KB 
ID:	3990   Click image for larger version. 

Name:	sun room 009.jpg 
Views:	492 
Size:	108.0 KB 
ID:	3991   Click image for larger version. 

Name:	sun room 010.jpg 
Views:	497 
Size:	99.9 KB 
ID:	3992   Click image for larger version. 

Name:	sun room 011.jpg 
Views:	498 
Size:	124.0 KB 
ID:	3993  
    Everlast I mig 205
    Everlast 200 amp spool gun
    Everlast 250 ex
    H. F. 12x36 lathe
    Grizzly Mill
    10,000 lb two post lift
    Box and Pan Brake
    Bead roller
    jet 5x7 horizontal band saw
    Wilton 14 inch vertical band saw
    Mitec 50 A plasma cutter.
    tool grinder
    20 ton press and press brake
    more power and hand tools then I can list here
    Dodge Neon that runs 10.23 @143 mph in the quater
    70 Chevelle convert
    It took 62 years But I finally have my dream Garage

  15. #15

    Default

    Quote Originally Posted by Ram48 View Post
    Well I scored so many brownie points with the wall art I figured Id go for broke and made a set of candle holders to match. Man It worked, I just need to figure out what I want to do with them, the points not the candle holders.
    Collect those points as soon as possible, otherwise they might do away. Or maybe double them by mentioning Christmas is coming.

    It all came out quite nice. Not gonna show my wife...
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  16. #16

    Default

    Looks great ... gives me an idea for a plant holder to go on the wall outside our front door. NICE JOB!
    Powertig 200DX
    Lincoln 180c
    Hobart Handler 125
    Miller Thunderbolt
    and a bunch of other tools

Similar Threads

  1. First "real" TIG welding project coming up.
    By 225 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 12-27-2012, 07:48 PM
  2. Replies: 29
    Last Post: 09-01-2012, 05:23 PM
  3. Project 2 from welderdude: custom tv wall mount.
    By welderdude in forum Other Custom Fabrications
    Replies: 9
    Last Post: 02-25-2012, 05:45 PM
  4. my first real project
    By shawn in forum Off Road Fabrication
    Replies: 18
    Last Post: 10-09-2011, 04:28 PM
  5. Electric Wall Heater Repair
    By jakeru in forum Welding Repairs
    Replies: 3
    Last Post: 03-07-2011, 05:13 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •