Share
Results 1 to 6 of 6

Thread: Temporary plasma cutter from TIG?

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Temporary plasma cutter from TIG?

    Is it possible to do any short-term plasma cutting with a TIG setup?

    i.e. could I theoretically get a plasma torch, some air, and use my TIG machine to do some plasma cutting?

    What are the actual machine requirements for the processes? Amp, voltage, etc.
    .
    Eide
    PowerTig 225 LX

  2. #2

    Default

    I have not done this myself but read that you can cut thin metal with a tig torch. You would not use compressed air like a plasma and the cuts are not as clean. I am not sure if the everlast machine will allow you to run a tig only machine for plasma but I don't think it will. Other machines will not work like this. I would love to see more information if it is possible with the Everlast units.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  3. #3

    Default

    I do not think that is possible or advisable. Although it is possible to MELT THROUGH thin metal with any welding process this is not the proper use of a machine and bespeaks a gross lack of respect for the equipment. Mark and Mike could answer your question about how the machine works but probably faster to just wiki "plasma cutter". I know the process of ionization has to do with the movement of the air and the particular kind of metal used in the electrode... halfnium i think it is called....
    Everlast PP256
    Everlast Imig 205
    HF 90 am inverter tig
    Scopes, Scanners, Meters

  4. #4

    Default

    No,
    Don't try it.
    Even though tig and plasma share roots together, it won't do it

  5. #5

    Default

    why couldnt you move the tungsten back inside the cup, the the amp up to 200 or so and bump the argon out to 50 - 60 or so? I think it was just on Jodys site that I saw a video of him setting it up that way
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

  6. #6

    Default

    This talks about doing the tig cutting in thin sheet from Jody's site.

    http://www.weldingtipsandtricks.com/...tig-torch.html
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

Similar Threads

  1. Plasma cutter or combo?
    By Fallon in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 11-27-2014, 12:50 PM
  2. Replies: 15
    Last Post: 08-02-2012, 01:30 PM
  3. Power Plasma 50 plasma cutter....
    By CGCINC in forum Customer Testimonials
    Replies: 4
    Last Post: 07-20-2012, 12:58 PM
  4. PU205P Plasma Cutter
    By Tritium in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 04-11-2012, 11:13 PM
  5. Super cut 50 plasma cutter
    By maddog in forum Everlast Plasma Cutters (PAC)
    Replies: 29
    Last Post: 02-21-2010, 11:28 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •