Here's the gearchange rear-set. I used a folding GSXR footpeg and altered the brake side middle bracket (aluminum) to work for my gear lever, or rather I made a gear lever to fit the bracket pivot. The gear lever is made to look like the original Vincent one, except it has the little lug on top for the linkage to attach to. The linkage rod& ends plus the frame bracket(the one that has a hole in centre and is tack welded) are made of SS 316, same as the frame material. It actually machines and threads very nicely.
The heel bracket is from 6061 Al. I had a black painted tin one from the GSXR stuff but it looked kinda cheap on there so I cut one out of Al. on the mill.