Does anyone know or have a link that gives general combination's of collet body/gas lens and cup size by a given tungsten diameter and/or amperage?
Trying to get an order together to cover the WP9 and WP26 torches.
Thanks in advance!
Does anyone know or have a link that gives general combination's of collet body/gas lens and cup size by a given tungsten diameter and/or amperage?
Trying to get an order together to cover the WP9 and WP26 torches.
Thanks in advance!
Rengaw,
The manual has a little bit of that in there in regard to amps and tungsten size. However, cup size is related to application, more than amperage.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
Here is a useful starting point:
"Guide for Shield Gas Flows, Current Settings, and Cup Selection"
http://www.ckworldwide.com/tech-3.pdf
Last edited by jakeru; 03-11-2011 at 04:45 AM.
'13 Everlast 255EXT
'07 Everlast Super200P
Hello,
Ive been using weldcraft rare earth tungsten. Ive mostly worked on stainless with it. They have been working fine for me. Problem is I am not an expert and not absolutley sure everything that is suppose to be ideal. It doesnt seam to bead up on me or anything. The tip does round out a bit after some good current through it. Anybody who knows what they are doing used these?
Frank
I have a 250 EX welder and several other machines and equipment to allow for small scale manufacturing and prototyping of inventions
I am located in Oregon about 20 minutes west of Portland
Check out http://www.weldcraft.com/pdfs/WP9ENG.pdf and http://www.weldcraft.com/pdfs/WP26ENG.pdf there is a nifty chart that show the proper parts combination.