Share
Results 1 to 4 of 4

Thread: Getting a high pitched buzz and little or no arc

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default Getting a high pitched buzz and little or no arc

    225 lx, been using the torch button but just broke out the foot pedal to try and fill in holes from plasma cutting.

    Anyway, it was working fine until it started the buzzing. Looking at the amp read-out, it said 14 amps. I thought it was the foot pedal so I switched back to the torch button. Got the same buzz. Got it working again but shut it down to ask here what might be the cause. I've had this problem on and off for a while.


    Thanks,
    Charlie


    P.S.
    Did you ever get the low profile foot pedal?
    Last edited by jtybt; 02-24-2011 at 04:32 AM.
    Charlie

    Everlast 225 LX
    Everlast PP 50

    HF 130 TIG/90 ARC
    HF 90 fluxcore

    ATX MIG (don't ask)

  2. #2

    Default

    Hey,
    Give us a call when you can. We'll see what we can do. Sounds like a point gap adjustment.

  3. Default

    Sorry for the delay, Mark. I guess I had my 'email notification' turned off.

    Tried to call just now but you were unavailable.

    I suspected a solenoid/gap problem as I hear/don't hear the solenoid. Is there a diagram and gap specs? ...225 LX

    Also getting intermittent spark/arc on the PP 50.
    Charlie

    Everlast 225 LX
    Everlast PP 50

    HF 130 TIG/90 ARC
    HF 90 fluxcore

    ATX MIG (don't ask)

  4. #4

    Default

    This might be a switch problem on the torch.

Similar Threads

  1. Pro 256 no HF (high frequency) start
    By jch13 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 07-01-2015, 11:24 PM
  2. I-Mig 205 wire speed not high enough?
    By camboscams in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 4
    Last Post: 01-21-2014, 02:41 PM
  3. High pitched beep coming from machine
    By Jef_Replogle in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 6
    Last Post: 03-13-2012, 05:41 AM
  4. PP256 goes high and low with output
    By BlownBlueZ06 in forum Everlast Plasma Cutters (PAC)
    Replies: 15
    Last Post: 01-29-2012, 05:04 AM
  5. No High Friq
    By WAYNESWORLD in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 01-03-2010, 12:03 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •