Share
Results 1 to 4 of 4

Thread: just getting started

  1. #1

    Default just getting started

    ordered pt250ex to rework my bowfishing rig lots of .125 aluminum.. I am ok with a MIG, but TIG is new to me. Watched Jody videos and start off with 11 gauage aluminum looks like the way to go. Then I read over here that I should start out with mild steel. Which should I start with?

    Then I was going to order some filler rod and parts. Does the filler rod have to match the tungsten size?

    How do you pick the right size tungsten and filler rod?
    sold my miller mig
    got a PT250EX
    saving up for a plasma cutter

  2. Default

    I select the tungsten dia. For the amount of amps I'm using. Anymore I just use Ceriated, (orange) for all my Tig welding, (with inverter).
    I select the filler size for the size of weld I want to make. Tungsten size has a lot to do with how big the weld will be also.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	Tungsten heat range 2.jpg 
Views:	398 
Size:	89.0 KB 
ID:	902  

  3. #3

    Default

    ok being that I haven't Tig welded in 20 years due to being paralyzed in an accident I don't think I can really give you much help other than pointing you in the direction of some good literature and hope it helps and I don't get in Trouble for pointing to to another mfg website. I got hit by an uninsured unlicensed driver in my power wheelchair some time back and a new frame would cost $1500 dollars. Well I just decided to buy a Tig welder and fix the frame myself then at least I have something I will be able to use in the future rather than to just pay for $20 in material and $1480 for someone's welds ( probably a robot ) LOL

    anyway here is a link to Millers site and their pdf Tig welding handbooks great info on everything TIG
    http://www.millerwelds.com/resources/TIGhandbook/

    hope this helps you, have fun reading LOL
    Don

    MTS 200 workhorse
    PowerTig 250EX <---sweet
    80 amp HF inverter arc welder
    Lincoln Buzzbox
    Rotobrute AC-35 Mag Drill
    Milwaukee mag drill
    HF Heavy Duty 16 Speed Bench Drill Press (Custom made Adjustable Height stand)

    I gotta find more junk to sell on EBaY ... Must Buy a Plasma Cutter and a Mig Welder


    Fullerton, Ca
    USA

  4. #4

    Default

    Quote Originally Posted by dgarnier View Post
    ordered pt250ex to rework my bowfishing rig lots of .125 aluminum.. I am ok with a MIG, but TIG is new to me. Watched Jody videos and start off with 11 gauage aluminum looks like the way to go. Then I read over here that I should start out with mild steel. Which should I start with?

    Then I was going to order some filler rod and parts. Does the filler rod have to match the tungsten size?

    How do you pick the right size tungsten and filler rod?
    I would definitely start with steel and stay on it until you are real comfortable with tig welding, then go to al..
    To start, get three 6" square pieces (coupons) of 1/4" mild steel and run beads on them until they look good. Let one cool, weld the next and so on. Scribe lines on the coupons 1/2" inch apart and try to follow the lines with your weldbeads. When all the lines are filled up go back and put nice straight beads in between.

Similar Threads

  1. Looking for advice on getting started with a 200DX
    By EmptyNester in forum TIG Welding (GTAW/GTAW-P)
    Replies: 21
    Last Post: 12-10-2012, 12:01 AM
  2. PP 205 Setup and getting started.
    By qcksnake in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 12-30-2011, 01:40 AM
  3. My wife started talking about plasma cutters last night.
    By Haywire in forum Everlast Plasma Cutters (PAC)
    Replies: 13
    Last Post: 05-15-2011, 01:20 AM
  4. Started my plasma table today.
    By A/C Guy in forum Other Custom Fabrications
    Replies: 13
    Last Post: 04-12-2011, 01:00 PM
  5. Just getting started
    By madcratebuilder in forum TIG Welding (GTAW/GTAW-P)