    What consumables would I replace if I wanted to make very thin, fine cuts on thin steel with my 40AMP/50AMP torch?

  2. #2
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Default

    Assuming you have the S45 torch. There are tips with smaller orifices available, Standard is .8 or .9 mm.
    I have seen them down to .6, smaller orifice, finer kerf but less power capabilities.
    If you looking for smoother cuts, try using a “new” tip, raising the air pressure slightly (confines the plasma stream). Or using less current.
    Travel speed and consistency (steadiness) has a big effect on how smooth the cuts are.
    Mark might have some suggestions also.
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

  3. #3

    Default

    The current tips DO offer about as fine as cut as practical.

  4. Default

    Actually I am not wanting to cut with it. I am doing some art work and I found that I could make some very interesting surface "etching" with the current nozzle. However, on thin metal, the margin between etching and cuttng is very slim with the current nozzle. So, I want something a bit more delicate. And yes, I have the S45. I checked with my local welding shop and they wanted to know what brand the S45 torch was. What is it? And, where might I buy these tiny nozzles?

  5. #5

    Default

    Trafimetusa.com or google for trafimet S45 consumables. You will have to weeds though a number of sites. But they are out there.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  6. #6

    Default

    Its hard on cons, but to etch, just don't use the ground clamp and the torch will not cut.

  7. Default .6mm nozzles and higher amps?

    Without the ground clamp the torch does not do what I am calling etching.

    Anyway, I ordered some .6mm nozzles. I am told that they are rated at 5 to 15 amps. What will happen if I go over the rated amps? Will I break something???

  8. #8

    Default

    Where did you order them from?

    Keep in mind, the units minimum amps is 20.
    What it will do is blow the bottom out of the consumable, or at least widen the hole.

  9. Default .6 nozzles

    Since I have no idea what I am doing,, I probably got too small of nozzles. I will turn it down to 20 and hope that is not too much more than 15 amps. As long as it does not screw up my torch it will not get too upset if it burns the hole in the .6 nozzles. Oh well they were only $14 with shipping on Ebay. That is the only place I could find them.

  10. #10

    Default

    As Ray mentions, consistency is all important. This cut was done with a constant feed, no wavering and it turned out pretty nice.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	plasma 4 002.jpg 
Views:	941 
Size:	82.2 KB 
ID:	1010  
    Everlast PP256
    Everlast Imig 200
    Everlast Power Ultra 205
    P&H 400 amp A.C.
    Miller 230 amp with Onan power

Similar Threads

  1. 2011 Power Plasma 60 cuts with P80 torch
    By zoama in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 04-23-2016, 12:54 AM
  2. Power Pro 205s fine tuning
    By Tigfreak in forum General Welder Questions
    Replies: 15
    Last Post: 11-17-2015, 07:53 PM
  3. Clean-Up after Jig Saw cuts
    By Tensas in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 10-30-2013, 02:08 PM
  4. Everlast PA160-STH fine output control demonstration / review
    By joshuab in forum Customer Testimonials
    Replies: 0
    Last Post: 08-02-2013, 07:54 PM
  5. Making a wooden propeller....
    By CGCINC in forum Personal Projects (no welder required)
    Replies: 5
    Last Post: 02-22-2013, 05:36 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •