  1. Default Just Bought PowerTig 185

    Hi all,

    I'm new to welding but have been building bikes for some time (welding was done by Chassis Enginnering who are local to me). I bought a PowerTig 185 to learn how to weld on. My unit arrived in good condition, no damage from shipping. I have been using the machine a few days and it has been great. This machine is very capable and in an experienced welders hands I am sure it can make some nice beads.

    Here are some pictures in my cluttered garage...











    And these are some of the welds I have made with it.




  2. Default

    Here is an update, these are two pictures of something I welded. Three days experience.




  3. #3

    Default

    That looks great for 3 days! Tie in is good, heat lines show even torch angle. Color of weld appears to be the correct temperature. Bead with is fine, with a little underfill on the sides of the bevel toward the end on the second picture. The ends of the welds look properly filled as well.

    I have told many guys that this machine will meet almost all their needs. There is no slack in performance or weld quality on this unit. I can tell you that it is every bit as competent as any of our other TIG welding units.

  4. Default

    How much does this machine cost with a foot pedal? I am torn between this one and the PowerTig DX 200A. I mean the 200A is only $1100. If this one is $900 shipped with a foot pedal, it is almost worth it just to get all the extra options for another $200.

  5. #5

    Default

    Diabolic,
    Give me a call and we'll see what we can do on a 185.

  6. Default

    I am still waiting for everlast to recieve the foot pedals. I cant wait to get mine in, I just want to be able to grab the torch closer to the neck it would give me much better control. Hopefully the pedals will come in soon.

Similar Threads

  1. Bought a broken 99 4runner the other day
    By ncsugrad2006 in forum Personal Projects (no welder required)
    Replies: 16
    Last Post: 01-07-2013, 04:27 AM
  2. new tool i bought
    By Rodsmachineshop in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 13
    Last Post: 06-15-2012, 01:24 AM
  3. Just bought a Powerpro 205
    By valveman in forum Introduce Yourself
    Replies: 1
    Last Post: 07-01-2011, 12:44 PM
  4. bought the powermaster 256 maybe screwed up
    By 1bad05gto in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 12
    Last Post: 07-29-2010, 11:01 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •