Share
Results 1 to 19 of 19

Thread: My Welding Condo (cart)

  1. #1

    Default My Welding Condo (cart)

    This is the start of my welding cart, It will have three shelves. The bottom for storage, or maybe a drawer. the middle will hold my Mitec plasma cutter and a future W300 water cooler and the top will hold me 250ex tig and I-Mig 200, there is room for two bottles of any size I may need. I will be adding holders for my cables, peddle and filler rod.
    Pic # 1 is the basic frame layout
    Pic # 2, 3, 4, are different views of the frame and main upright shelf tabs and attachment plates for the wheels and casters.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	Welding Cart 1 002.jpg 
Views:	413 
Size:	78.0 KB 
ID:	699   Click image for larger version. 

Name:	Welding Cart 1 003.jpg 
Views:	370 
Size:	145.6 KB 
ID:	700   Click image for larger version. 

Name:	Welding Cart 1 004.jpg 
Views:	356 
Size:	144.5 KB 
ID:	701   Click image for larger version. 

Name:	Welding Cart 1 005.jpg 
Views:	362 
Size:	140.5 KB 
ID:	702  

  2. Default

    Nice project Ram48! What process are you using to weld it up?


    I need to make an adapter of some sorts for my Tig machine. I just bought the Tig runner system, it only has room for one bottle. Not that I use the helium bottle that much, but it would be nice to keep it with the Tig machine.

  3. #3

    Default

    Right now I am just using the Mig and I am at what I like to call my melt and pray stage of development.most welds are not pretty but hold and every once in a while I lay down a decent bead, and they are slowly becoming more common. I need a lot more helmet time. but once I get this project finished. I need to start playing with the Tig. I have not even fired it up yet.

  4. Default

    The Mig will come fast. Tig will be harder to pickup, but much more rewarding!

  5. #5

    Default

    Looking good, don't worry about pretty, just crank up the heat and learn to control it. It's all about helmet time, after awhile it becomes old hat, pretty comes later. You will find the 250Ex a great machine when you have the water cooler hooked to it. I can see you are well on your way to becoming a builder of neat things. Your last project looks real good.

  6. #6

    Default Cart update pics

    Here are some pictures of my progress on the welding cart.

    Pics #1 & #2 setting the horizontal shelf bracket between the uprights

    #3 & #4 close up of two of my better welds please critique, I want to learn

    #5 & #6 Bottom shelf being fit up for welding.

    #7 Braces added to bottom shelf

    #8 Cart skeleton is ready for final welding.

    This has been a good learning experience for me please let me know the good and bad you see in the cart. I will be adding the shelves, hangers for the cables and a way to secure the tanks. Any ideas on those things would be great
    Ray
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	Welding Cart 2 001.jpg 
Views:	349 
Size:	60.0 KB 
ID:	714   Click image for larger version. 

Name:	Welding Cart 2 002.jpg 
Views:	325 
Size:	73.7 KB 
ID:	715   Click image for larger version. 

Name:	Welding Cart 2 003.jpg 
Views:	363 
Size:	133.8 KB 
ID:	716   Click image for larger version. 

Name:	Welding Cart 2 004.jpg 
Views:	345 
Size:	46.2 KB 
ID:	717   Click image for larger version. 

Name:	Welding Cart 2 005.jpg 
Views:	346 
Size:	92.4 KB 
ID:	718  

    Click image for larger version. 

Name:	Welding Cart 2 006.jpg 
Views:	334 
Size:	80.8 KB 
ID:	719   Click image for larger version. 

Name:	Welding Cart 2 007.jpg 
Views:	345 
Size:	78.7 KB 
ID:	720   Click image for larger version. 

Name:	Welding Cart 2 008.jpg 
Views:	363 
Size:	136.0 KB 
ID:	721  

  7. Default

    Quote Originally Posted by Ram48 View Post
    #3 & #4 close up of two of my better welds please critique, I want to learn
    Ray I take it that you are right handed?
    You're putting too much metal / weld on. You either need to move faster, or turn down your wire speed a little. If your travel speed is acceptable or even a little slow for you, turn your voltage up. In other words the weld looks too cold.

  8. Default

    Here is a vertical up Mig weld I did, doesn't it look hotter than your?
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	Weld.jpg 
Views:	319 
Size:	137.3 KB 
ID:	722  

  9. #9

    Default settings for pic below

    Shield
    It is 14 Ga tube and it was a fillet weld Settings were 18v, 215 IPM with .030 wire and 75 / 25 mix.
    Thanks for the input.

  10. #10

    Default

    Move faster, making your weld profile flatter, look at shield arc's weld he has ripples, and a flatter weld, that's the kinda thing/look you should try for.

  11. #11

    Default Well its done

    Here are the completed shots of the cart project. Well except for the tig rod holders. thanks everyone for the welding tips and thoughts on the cart.
    it was a fun project and I learned a bit along the way. (I went from really suck at this to just bad at it) I will practice and keep at it and I hope it will come.
    The top and middle shelves are corian and the bottom shelf is mdf board. the plate that the tanks sit on is 1/4 steel plate. All are painted Hammertone black.

  12. Default

    That is an excellent job Ram! One of the best carts I've seen. You're off and running now.
    Won't be long until you have to get bigger bottles, you'll get tired of having to fill them so often.

  13. #13

    Default

    Nice cart Ram!
    Gerald

    Millermatic 251
    Spectrum 300 Plasma
    Everlast PowerTig 250EX
    Everlast PowerCool W300
    Harris / Victor OA
    Craftsman 13 Speed Drill Press
    ProTools Air/Hydraulic Bender
    48" Brake, 72" Brake, 52" Stomp Shear
    Mitler Bros. 36" High Throat Bead Roller
    Compressor, Notchers, Grinders, etc.

  14. #14

    Default

    Looks great, amazing how much engineering and thought has to go in to something like that, only those that have done that, will know that.

  15. #15

    Default changed it already

    This morning I went to the shop and looked at the cart, The wheels looked small to me and as I went to move it the two rear ones had taken a set to the floor and had a flat spot when rolled, they are semi solid so I guess thats what happens to them I went and picked up 8 inch solid rubber read wheels and 4 inch poly casters the first set was 6 and 3 inches the original set of wheels are on the flor next to the new ones.
    Next I need to come up with a better way to secure the tanks. this works ok But I can do better.
    It rolls a lot better now and the looks have improved too I think.

  16. #16

    Default Finishing touches to the cart

    Its not like the Aluminum show cart, That thing is by far the nicest I have seen.
    I added tig rod holders and a fire extinguisher and capped the sq tube frame.
    I had fun and learned a lot. Wish the welds were a bit better but As you all say it will take practice, practice and more practice.
    Ray

  17. #17

    Default

    looks dam fine to me, the only thing I could see missing was a water cooler for the Tig. but you have room for it. Nice build Ram,

  18. #18

    Default

    Quote Originally Posted by geezer View Post
    looks dam fine to me, the only thing I could see missing was a water cooler for the Tig. but you have room for it. Nice build Ram,
    That is exactly what the space next to the Plasma is for Geezer I thought ahead for once and determined the measurements for a cooler Before I designed the cart.

  19. #19

    Default

    Nice work!
    Big Willy in Rockford, Il. Power Pro 205, Lincoln 140 Mig, Oxy/Acetylene rig with a Cobra Torch, Full up Motorcycle shop.
    http://projectoldwing.com
    wruehl@hotmail.com
    Active Ironbutt Member.

Similar Threads

  1. Tig Welding Cart
    By Depdog in forum Other Custom Fabrications
    Replies: 5
    Last Post: 02-25-2014, 01:51 AM
  2. Welding Cart - Power Cart 250 - opinions?
    By ScottRussell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 12-05-2012, 01:19 PM
  3. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 03:30 PM
  4. This is project 3, from dgarnier, a Deer Condo
    By dgarnier in forum Hobyist Projects
    Replies: 16
    Last Post: 06-25-2011, 06:44 PM
  5. Welding cart
    By jtybt in forum General Welder Questions
    Replies: 1
    Last Post: 01-23-2010, 06:37 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •